ZnO film is attractive for high frequency surface acoustic wave device application when it is coupled with diamond. In order to get good performance and reduce insertion loss of the device, it demands the ZnO film possessing high electrical resistivity and piezoelectric coefficient d33. Doping ZnO film with some elements may be a desirable method. In this paper, the ZnO films undoped and doped with Cu, Ni, Co and Fe, respectively (doping concentration is 2.0 at.%) are prepared by magnetron sputtering. The effect of different dopants on the microstructure, piezoelectric coefficient d33, and electrical resistivity of the film are investigated. The results indicate that Cu dopant can enhance the c-axis orientation and piezoelectric coefficient d33, the Cu and Ni dopant can increase electrical resistivity of the ZnO film up to 109 Ω cm. It is promising to fabricate the ZnO films doped with Cu for SAW device applications.  相似文献   

2.
High quality Co-doped ZnO thin films are grown on single crystalline Al2O3(0001) and ZnO(0001) substrates by oxygen plasma assisted molecular beam epitaxy at a relatively lower substrate temperature of 450℃. The epitaxial conditions are examined with in-situ reflection high energy electron diffraction (RHEED) and ex-situ high resolution x-ray diffraction (HRXRD). The epitaxial thin films are single crystal at film thickness smaller than 500nm and nominal concentration of Co dopant up to 20%. It is indicated that the Co cation is incorporated into the ZnO matrix as Co^2+ substituting Zn^2+ ions. Atomic force microscopy shows smooth surfaces with rms roughness of 1.9 nm. Room-temperature magnetization measurements reveal that the Co-doped ZnO thin films are ferromagnetic with Curie temperatures Tc above room temperature.  相似文献   

3.
As-grown undoped zinc oxide (ZnO) films have been annealed in zinc-rich, oxygen-rich and vacuum ambient, and the electron concentration varied greatly after the annealing process. It decreased nearly two orders of magnitude after the sample was annealed in oxygen, while increased nearly three times after annealed in metallic zinc ambient, and increased slightly after annealed in vacuum. It was found that the variation trend of the electron concentration is always the same with the expected variation of oxygen vacancy (VO) under the three investigated conditions, it is thus speculated that VO may be the dominant donor source in ZnO. By supplying more oxygen during the growth process to suppress VO, ZnO films with lower electron concentration were obtained, which verifies the above speculation.  相似文献   

4.
The Cu-doped ZnO films were prepared by direct current reactive magnetron sputtering using a zinc target with various Cu-chips attached. The influences of Cu-doping on the microstructure, photoluminescence, and Raman scattering of ZnO films were systematically investigated. The results indicate that ZnO films doped with moderate Cu dopant (2.0-4.4 at.%) can obtain wurtzite structure with strong c-axis orientation. The near band edge (NBE) emission of ZnO film can be enhanced by Cu dopant with a concentration of 2.0 at.% and quench quickly with further increase of doping concentration. Two additional modes at about 230 and 575 cm−1, which could be induced by Cu dopant, can be observed in Raman spectra of the Cu-doped ZnO films.  相似文献   

5.
The optical properties of undoped zinc oxide (ZnO) thin films of various thicknesses were compared with those of Ga-doped (GZO) thin films. Transparent, high-quality undoped ZnO and GZO films were deposited successfully using radio-frequency (RF) sputtering at room temperature. The films were polycrystalline with a hexagonal structure and a strongly preferred orientation along the c-axis. The films had an average optical transmission >85% in the visible part of the electromagnetic spectrum. The undoped ZnO thin films were more transparent than the GZO thin films. In the photoluminescence (PL) spectrum, ZnO film has higher quality than GZO as a result of decrease in the green emission intensity.  相似文献   

6.
The current study investigates the performance of dye-sensitized solar cells (DSSCs) based on Al-doped and undoped ZnO nanorod arrays synthesized by a simple hydrothermal method. Current density-voltage (J-V) characterizations indicate that Al-doping in ZnO crystal structure can significantly improve current densities and the energy conversion efficiency (η) of ZnO nanorod-based DSSCs. The maximum η, 1.34%, was achieved in DSSC when Al-doped ZnO nanorod arrays were grown in 0.04 M zinc acetate dihydrate solution with 5 mM aluminum nitrate nonahydrate. This result represents a large increase of η in Al-doped ZnO nanorod-based DSSCs as compared to undoped (0.05%). The improved DSSC photovoltaic performance can be attributed to two main factors: (1) increased light harvesting efficiency due to a large amount of N719 adsorbed on the large surface area of Al-doped ZnO nanorod arrays, and (2) increased electrical conductivity due to A13+ ion doped into the ZnO lattice at the divalent Zn2+ site, allowing electrons to move easily into the Al-doped ZnO conduction band.  相似文献   

7.
The effects of annealing on the chemical states of N dopant, electrical, and optical properties of N-doped ZnO film grown by molecular beam epitaxy (MBE) are investigated. Both the as-grown ZnO:N film and the film annealed in N2 are of n-type conductivity, whereas the conductivity converts into p-type conductivity for the film annealed in O2. We suggest that the transformation of conductivity is ascribed to the change in ratio of the N molecular number on O site (N2)O to the N atom number on O site (NO) in ZnO:N films under the various annealed atmosphere. For the ZnO:N film annealed in N2, the percentage content of (N2)O is larger than that of NO, i.e.the ratio >1, resulting in the n-type conductivity. However, in the case of the ZnO:N film annealed in O2, the percentage content of (N2)O is fewer than that of NO, i.e., the ratio <1, giving rise to the p-type conductivity. There is an obvious difference between low-temperature (80K) PL spectra of ZnO:N film annealed in N2 and that of ZnO:N film annealed in O2. An emission band located at 3.358eV is observed in the spectra of the ZnO:N film after annealed in N2, this emission band is due to donor-bound exciton (D0X). After annealed in O2, the PL of the donor-bound exciton disappeared, an emission band located at 3.348eV is observed, this emission band is assigned to acceptor-bound exciton (A0X).  相似文献   

8.
We report synthesis of a transparent magnetic semiconductor by incorporating Ni in zinc oxide (ZnO) matrix. ZnO and nickel-doped zinc oxide (ZnO:Ni) thin films (∼60 nm) are prepared by fast atom beam (FAB) sputtering. Both undoped and doped films show the presence of ZnO phase only. The Ni concentration (in at%) as determined by energy dispersive X-ray (EDX) technique is ∼12±2%. Magnetisation measurement using a SQUID magnetometer shows that the Ni-doped films are ferromagnetic, having coercivity (Hc) values 192, 310 and 100 Oe and saturation magnetization (Ms) values of 6.22, 5.32 and 4.73 emu/g at 5, 15 and 300 K, respectively. The Ni-doped film is transparent (>80%) across visible wavelength range. Resistivity of the ZnO:Ni film is ∼2.5×10−3 Ω cm, which is almost two orders of magnitude lower than the resistivity (∼4.5×10−1 Ω cm) of its undoped counterpart. Impurity d-band splitting is considered to be the cause of increase in conductivity. Interaction between free charges generated by doping and localized d spins of Ni is discussed as the reason for ferromagnetism in the ZnO:Ni film.  相似文献   

9.
The undoped and Al-doped ZnO nanostructures were fabricated on the ITO substrates pre-coated with ZnO seed layers using the hydrothermal method. The undoped well-aligned ZnO nanorods were synthesized. When introducing the Al dopant, ZnO shows various morphologies. The morphology of ZnO changes from aligned nanorods, tilted nanorods, nanotubes/nanorods to the nanosheets when the Al doping concentrations increase. The ZnO nanostructures were characterized by X-ray diffraction, field emission scanning electron microscopy, X-ray photoelectron spectroscopy, photoluminescence and Raman technology. The Al doping concentrations play an important role on the morphology and optical properties of ZnO nanostructures. The possible growth mechanism of the ZnO nanostructures was discussed.  相似文献   

10.
Li-N dual-doped p-type ZnO (ZnO:(Li, N)) thin films are prepared by pulsed laser deposition. The optical properties are studied using temperature-dependent photoluminescence. The Lizn-No complex acceptor with an energy 1evel of 138 me V is identified from the free-to-neutral-acceptor (e, A0 ) emission. The Haynes factor is about 0.087 for the Lizn-No complex acceptor, with the acceptor bound-exciton binding energy of 12meV. Another deeper acceptor state located at 248 meV, also identified from the (e, A0) emission, is attributed to zinc vacancy acceptor. The two acceptor states might both contribute to the observed p-type conductivity in ZnO:(Li,N).  相似文献   

11.
Undoped, Ga-, In-, Zr-, and Sn-doped ZnO transparent semiconductor thin films were deposited on alkali-free glasses by sol–gel method. 2-methoxyethanol (2-ME) and diethanolamine (DEA) were chosen as a solvent and a stabilizer, respectively. The doping concentration was maintained at 2 at.% in the impurity doping precursor solutions. The effects of different dopants on the structural, optical, and electrical properties of ZnO thin films were investigated. XRD results show that all annealed ZnO-based thin films had a hexagonal (wurtzite) structure. ZnO thin films doped with impurity elements obviously improved the surface flatness and enhanced the optical transmittance. All impurity doped ZnO thin films showed high transparency in the visible range (>91%). The Ga- and In- doped ZnO thin films exhibited higher Hall mobility and lower resistivity than did the undoped ZnO thin film.  相似文献   

12.
The microstructure, and the electrical and optical properties of undoped zinc oxide (ZnO) and cadmium-doped ZnO (CZO) films deposited by a sol–gel method have been investigated. The films have a polycrystalline structure with hexagonal wurtzite ZnO. Scanning electron microscopy (SEM) images indicated that the films have a wrinkle network with uniform size distributions. The elemental analyses of the CZO films were carried out by energy dispersive X-ray analysis. The fundamental absorption edge changed with doping. The optical band gap of the films decreased with Cd dopant. The optical constants of the films such as refractive index, extinction coefficient and dielectric constants changed with Cd dopant. A two-probe method was used to investigate the electrical properties, and the effect of Cd content on the electrical properties was investigated. The electrical conductivity of the films was improved by incorporation of Cd in the ZnO film.  相似文献   

13.
Cu- and Ag-doped ZnO films were deposited by direct current co-reactive magnetron sputtering technique. The microstructure, the chemical states of the oxygen, zinc, copper and silver and the optical properties in doped ZnO films were investigated by X-ray diffraction spectroscopy (XRD), X-ray photoelectron spectroscopy (XPS) and UV-Visible spectroscopy. XRD analysis revealed that both of Cu- and Ag-doped ZnO films consist of single phase ZnO with zincite structure while the doping elements had an evident effect on the (0 0 2) preferential orientation. The XPS spectra showed that the chemical states of oxygen were different in Cu- and Ag-doped ZnO thin films, which may lead to the shift of the band gap as can be observed in the transmittance and absorption spectra. Meanwhile, the widths of band tails of ZnO films became larger after Cu and Ag doping.  相似文献   

14.
Nitrogen-doped ZnO (ZnO:N) films are prepared by thermal oxidation of sputtered Zn3N2 layers on A1203 substrates. The correlation between the structural and optical properties of ZnO:N films and annealing temperatures is investigated. X-ray diffraction result demonstrates that the as-sputtered Zn3N2 films are transformed into ZnO:N films after annealing above 600℃. X-ray photoelectron spectroscopy reveals that nitrogen has two chemical states in the ZnO:N films: the No acceptor and the double donor (N2)o. Due to the No acceptor, the hole concentration in the film annealed at 700℃ is predicted to be highest, which is also confirmed by Hall effect measurement. In addition, the temperature dependent photoluminescence spectra allow to calculate the nitrogen acceptor binding energy.  相似文献   

15.
Zinc oxide (ZnO) and aluminium-doped zinc oxide (ZnO:Al) thin films were prepared by RF diode sputtering at varying deposition conditions. The effects of negative bias voltage and RF power on structural and optical properties were investigated. X-ray diffraction measurements (XRD) confirmed that both un-doped and Al-doped ZnO films are polycrystalline and have hexagonal wurtzite structure. The preferential 〈0 0 1〉 orientation and surface roughness evaluated by AFM measurements showed dependence on applied bias voltage and RF power. The sputtered ZnO and ZnO:Al films had high optical transmittance (>90%) in the wavelength range of 400-800 nm, which was not influenced by bias voltage and RF power. ZnO:Al were conductive and highly transparent. Optical band gap of un-doped and Al-doped ZnO thin films depended on negative bias and RF power and in both cases showed tendency to narrowing.  相似文献   

16.
Mn/Ga noncompensated codoped ZnO films were prepared on c-cut sapphire substrates via pulsed laser deposition. The structural, magnetic, transport, and optical properties of the films were then investigated. Addition of the Ga donor increases the electron concentration and enhances the magnetization in these films because of the net negative charge of the special noncompensated codoping, which can adjust the carrier concentration as well as the magnetic moment. Moreover, the Fermi level moves into the conduction band because of the increase in electron concentration, which results in an increase in the optical band gap value, from 3.28 eV for the undoped ZnO film to 3.61 eV for the (Mn,Ga)-codoped ZnO film.  相似文献   

17.
Undoped and tin (Sn) doped ZnO films have been deposited by sol gel spin coating method. The Sn/Zn nominal volume ratio was 1, 3 and 5% in the solution. The effect of Sn incorporation on structural and electro-optical properties of ZnO films was investigated. All the films have polycrystalline structure, with a preferential growth along the ZnO (002) plane. The crystallite size was calculated using a well-known Scherrer's formula and found to be in the range of 26-16 nm. X-ray diffraction patterns of the films showed that Sn incorporation leads to substantial changes in the structural characteristics of ZnO films. The SEM measurements showed that the surface morphology of the films was affected from the Sn incorporation. The highest average optical transmittance value in the visible region was belonging to the undoped ZnO film. The optical band gap and Urbach energy values of these films were determined. The absorption edge shifted to the lower energy depending on the Sn dopant. The shift of absorption edge is associated with shrinkage effect. The electrical conductivity of the ZnO film enhanced with the Sn dopant. From the temperature dependence of conductivity measurements, the activation energy of ZnO film increased with Sn incorporation.  相似文献   

18.
梁爽  梅增霞  杜小龙 《中国物理 B》2012,21(6):67306-067306
Ga-doped ZnO(GZO) films are prepared on amorphous glass substrates at room temperature by radio frequency magnetron sputtering.The results reveal that the gallium doping efficiency,which will have an important influence on the electrical and optical properties of the film,can be governed greatly by the deposition pressure and film thickness.The position shifts of the ZnO(002) peaks in X-ray diffraction(XRD) measurements and the varied Hall mobility and carrier concentration confirms this result.The low Hall mobility is attributed to the grain boundary barrier scattering.The estimated height of barrier decreases with the increase of carrier concentration,and the trapping state density is nearly constant.According to defect formation energies and relevant chemical reactions,the photoluminescence(PL) peaks at 2.46 eV and 3.07 eV are attributed to oxygen vacancies and zinc vacancies,respectively.The substitution of more Ga atoms for Zn vacancies with the increase in film thickness is also confirmed by the PL spectrum.The obvious blueshift of the optical bandgap with an increase of carrier concentration is explained well by the Burstein-Moss(BM) effect.The bandgap difference between 3.18 eV and 3.37 eV,about 0.2 eV,is attributed to the metal-semiconductor transition.  相似文献   

19.
丁斌峰  周生强 《中国物理 B》2011,20(12):127701-127701
Due to the fault of the first author, this article entitled “The coexistence of ferroelectricity and ferromagnetism in Mn-doped BaTiO3 thin films”, published in “Chinese Physics B”, 2011,Vol.20, Issue 12, Article No. 127701, has been found to copy from the article entitled“Decisive role of oxygen vacancy in ferroelectric versus ferromagnetic Mn-doped BaTiO3 thin films”, published in “Journal of Applied Physics”, 2011,Vol.109, Issue 8, article No. 084105. So the above article in “Chinese Physics B” has been withdrawn from the publication.<  相似文献   

20.
邓宁  庞华  吴畏 《中国物理 B》2014,(10):493-496
In this study the effects of doping atoms(Al, Cu, and N) with different electro-negativities and ionic radii on resistive switching of HfO2-based resistive random access memory(RRAM) are systematically investigated. The results show that forming voltages and set voltages of Al/Cu-doped devices are reduced. Among all devices, Cu-doped device shows the narrowest device-to-device distributions of set voltage and low resistance. The effects of different dopants on switching behavior are explained with deferent types of CFs formed in HfO2 depending on dopants: oxygen vacancy(Vo) filaments for Al-doped HfO2 devices, hybrid filaments composed of oxygen vacancies and Cu atoms for Cu-doped HfO2 devices,and nitrogen/oxygen vacancy filaments for N-doped HfO2 devices. The results suggest that a metal dopant with a larger electro-negativity than host metal atom offers the best comprehensive performance.  相似文献   