排序方式: 共有63条查询结果,搜索用时 31 毫秒
1.
Diode-end-pumped continuous-wave(CW) Tm:YAP and Tm:YLF slab lasers are demonstrated. The a-cut Tm:YAP and Tm:YLF slabs with doping concentrations of 4 at.-% and 3.5 at.-%,respectively,are pumped by fast-axis collimated laser diodes at room temperature. The maximum CW output powers of 72 and 50.2 W are obtained from Tm:YAP and Tm:YLF,respectively,while the pump power is 220 W,corresponding to the slope efficiencies of 37.9% and 26.6%,respectively. 相似文献
2.
大尺寸光通讯磁光薄膜衬底钆镓石榴石(Gd3Ga5O12)单晶的生长研究 总被引:3,自引:1,他引:2
随着光纤通讯产业的迅猛发展,市场对3英寸光通讯磁光薄膜衬底钆镓石榴石(分子式为Gd3Ga5O12,简称GGG)的需求量急剧增加。本文从磁光薄膜(YIG以及类YIG)对其外延基底单晶GGG物化性能的要求出发,综述了在利用传统的提拉法生长大尺寸、符合磁光薄膜衬底要求的Gd3Ga5O12单晶的过程中,出现的诸如Ga2O3组分挥发,界面翻转,螺旋生长和晶体的开裂等问题,针对各个问题讨论了它们的形成机制并提出了它们的解决方法。最后,还根据目前磁光膜的发展情况,预见了纯GGG和掺质GGG单晶的研究和发展趋势。 相似文献
3.
采用温度梯度法生长了熔体掺杂Ce浓度为1at%的YAlO3晶体,对于其吸收光谱、荧光光谱和x射线激发发射谱进行了表征分析.根据吸收光谱提出了一个色心模型,从而成功的解释了为什么刚生长出的晶体为粉红色,而分别经氢气和空气在1400℃退火后均能变为无色的现象和退火以后吸收光谱发生的显著变化.温度梯度法生长的Ce:YAP在330nm处存在着一定程度的自吸收和自激发.光致激发发射谱的发射主峰在368nm,而x射线激发发射谱的主发射峰红移至391nm,这表明在x射线激发下,晶体对发射光的自吸收将会减少.另外在x射线激发发射谱上,经H2退火和空气退火后的样品其发射强度比未退火的晶体要强. 相似文献
4.
研究了γ-辐照前后纯Y2SiO5和Eu3+掺杂的Y2SiO5晶体吸收光谱的变化,辐照后,未退火和氢气退火的纯Y2SiO5晶体在260~270 nm和320 nm波段产生了附加吸收峰,分别是由F心和O-心的吸收引起的;经过空气退火的纯YSO晶体中,由于消除了氧空位,因此辐照后没有出现色心吸收峰。在Eu3+∶Y2SiO5晶体中,不但有相同的F心和O-心吸收峰,而且还有Eu2+离子在300 nm和390 nm的吸收峰。随着辐照剂量的增加,色心附加吸收峰增强。空气退火能减少Eu3+∶Y2SiO5晶体中的色心,而氢气退火能增加色心。 相似文献
5.
Judd--Ofelt analysis of spectra and experimental evaluation of laser performance of Tm3+ doped Lu2SiO5 crystal 下载免费PDF全文
This paper reports that the Tm^3+:Lu2SiO5 (Tm:LSO) crystal is grown by Czochralski technique. The roomtemperature absorption spectra of Tm:LSO crystal are measured on a b-cut sample with 4 at.% thulium. According to the obtained Judd-Ofelt intensity parameters Ω2=9.3155×10^-20 cm^2, Ω4=8.4103×10^-20 cm^2, Ω6=1.5908×10^-20 cm^2, the fluorescence lifetime is calculated to be 2.03 ms for ^3F4 → ^3H6 transition, and the integrated emission cross section is 5.81×10^-18 cm^2. Room-temperature laser action near 2μm under diode pumping is experimentally evaluated in Tm:LSO. An optical-optical conversion efficiency of 9.1% and a slope efficiency of 16.2% are obtained with continuouswave maximum output power of 0.67 W. The emission wavelengths of Tm:LSO laser are centred around 2.06μm with spectral bandwidth of -13.6 nm. 相似文献
6.
<正>We report the luminescence properties and decay profiles of Ce:YAlO_3,Mn:YAlO_3,and Ce,Mn:YAlO_3 crystals grown by Czochralski method.The spectroscopic properties show that both Mn~(2+) ions and Mn~(4+) ions exist in Mn:YAlO_3 and Ce,Mn:YAlO_3 crystals.The Mn~(2+) ions have a broad emission band of 60 nm in Mn-doped YAlO_3 crystal at 530 nm.The luminescence spectra also indicate that there is significant energy transfer between Ce~(3+) and Mn~(4+) in Ce,Mn:YAlO_3 crystal.Because of the energy transfer,the first decay component in Ce,Mn:YAlO_3 decreases from 24.5 to 10.8 ns,which is much faster than that of Ce:YAlO_3. 相似文献
7.
<正>YAG:Ce crystal with a diameter of 110 mm is successfully grown by the temperature gradient technique (TGT).The effects of annealing on the luminescence efficiency of YAG:Ce crystal are investigated,and the optimal annealing temperature and atmosphere are obtained.The mechanism of variation behavior of the luminescence efficiency of YAG:Ce under different annealing conditions is discussed and some details on the luminescence associated with color centers are analyzed. 相似文献
8.
Yb:YAP晶体的光谱性能研究 总被引:1,自引:0,他引:1
应用中频感应加热提拉法生长出掺杂浓度为10;原子分数的Yb:YAP晶体,研究了室温下Yb:YAP晶体的吸收和发射光谱特性以及荧光寿命.Yb:YAP晶体在959nm处有最强吸收,吸收截面约为1.51 × 10-20 cm2,在1040nm处的发射截面为0.6 ×10-cm2,激光上能级荧光寿命为1.2 ms,此处自吸收较小,是实现激光输出的候选波长.研究了氧气退火对Yb:YAP晶体的光谱性能的影响.Yb:YAP晶体轴向效应明显,b轴将是作为激光输出的首选方向.比较了Yb:YAP晶体和Yb:YAG晶体的光谱性能参数. 相似文献
9.
10.
温梯法生长76mm Ce:YAG闪烁晶体的研究 总被引:1,自引:1,他引:0
首次采用温度梯度法(TGT)成功生长了直径为76mm高光学质量的Ce:YAG高温闪烁晶体,采用ICP-AES测试了Ce离子在Ce:YAG晶体中的分凝系数约为0.082.在室温下,测试了原生态Ce:YAG晶体的吸收光谱和X射线激发发射光谱(XEL).吸收光谱显示了Ce3+离子的3个特征吸收带,对应的中心波长分别为223nm,340nm及460nm;XEL发射谱表明Ce:YAG的发射峰为550nm,能与硅光二极管有效地耦合. 相似文献