1.
Starting from calcium sulfate (gypsum) as fermentation by‐product of lactic acid production process, high performance composites have been produced by melt‐blending polylactide (PLA, L/D isomer ratio of 96:4) and β‐anhydrite II (AII) filler, that is, calcium sulfate hemihydrate previously dehydrated at 500 °C. Characterized by attractive mechanical and thermal properties due to good filler dispersion throughout the polyester matrix, these composites are interesting for potential use as biodegradable rigid packaging. Physical characterization of selected composites filled with 20 and 40 wt % AII has been performed and compared to processed unfilled PLA with similar amorphous structure. State of dispersion of the filler particles and interphase characteristic features have been investigated using light microscopy (LM) and scanning electron microscopy (SEM). Addition of AII did not decrease PLA thermal stability as revealed by thermogravimetry analyses (TGA) and allowed reaching a slight increase of PLA crystallizability during melt crystallization and upon heating from the glassy, amorphous state (DSC). It was found by thermomechanical measurements (DMTA) that the AII filler increased pronouncedly storage modulus (E′) of the composites in comparison with PLA in a broad temperature range. The X‐ray investigations showed stable/unchanged crystallographic structure of AII during processing with molten PLA and in the composite system. The notable thermal and mechanical properties of PLA–AII composites are accounted for by the good filler dispersion throughout the polyester matrix confirmed by morphological studies, system stability, and favorable interactions between components. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 45: 2770–2780, 2007  相似文献   

2.
In this article, the composites based on long glass fibre reinforced polypropylene/intumescent flame retardant (LGFPP/IFR) were prepared by melt blending. The influence of thermal oxidative ageing on the LGFPP/IFR composites with different thermal oxidative ageing time at 140 °C was studied by means of oven heating. The thermal stability and flammability of the composites were respectively investigated by thermal gravimetric analysis (TG), limiting oxygen index (LOI), UL-94 test, cone calorimeter test (CCT), scanning electronic microscopy (SEM), mechanical properties test and energy-dispersive X-ray analysis (EDAX). A trend of increase first and then decrease in LOI values was shown in 0–50 days ageing, with the same trend as thermal stability obtained from TG in nitrogen condition. The CCT results indicated that the LGFPP/IFR composites after ageing achieved a higher heat release rate, which means a higher fire risk. The mechanical properties showed a global decrease in just 10 days ageing. Morphologies obtained from SEM showed that both the rupture of PP matrix and fibre interface debonding led to the decrease in mechanical properties. The EDAX proved that IFR particles could emerge and gather on the surface of sample in ageing procedure, which had great effects on the thermal stability and flame retardancy of the composites.  相似文献   

3.
Biocomposites comprising a combination of natural fibres and bio-based polymers are good alternatives to those produced from synthetic components in terms of sustainability and environmental issues. However, it is well known that water or aqueous chemical solutions affect natural polymers/fibres more than the respective synthetic components. In this study the effects of water, salt water, acidic and alkali solutions ageing on water uptake, mechanical properties and flammability of natural fibre-reinforced polypropylene (PP) and poly(lactic acid) (PLA) composites were compared. Jute, sisal and wool fibre- reinforced PP and PLA composites were prepared using a novel, patented nonwoven technology followed by the hot press method. The prepared composites were aged in water and chemical solutions for up to 3 week periods. Water absorption, flexural properties and the thermal and flammability performances of the composites were investigated before and after ageing each process. The effect of post-ageing drying on the retention of mechanical and flammability properties has also been studied. A linear relationship between irreversible flexural modulus reduction and water adsorption/desorption was observed. The aqueous chemical solutions caused further but minor effects in terms of moisture sorption and flexural modulus changes. PLA composites were affected more than the respective PP composites, because of their hydrolytic sensitivity. From thermal analytical results, these changes in PP composites could be attributed to ageing effects on fibres, whereas in PLA composite changes related to both those of fibres present and of the polymer. Ageing however, had no adverse effect on the flammability of the composites.  相似文献   

4.
Starting from gypsum, a by-product of lactic acid fabrication process, novel “green” composites have been produced by melt-blending polylactide (PLA) and this filler after a previous specific dehydration to obtain anhydrite II (AII). Such a material is potentially interesting in biodegradable/rigid packaging and in technical applications requiring rigidity, heat resistance and dimensional stability. In order to obtain PLA-AII composites characterized by specific end-use flame retardant properties, the addition of selected organo-modified layered silicates (OMLS) was considered. Co-addition of AII and OMLS leads to PLA (nano)composites characterized by good (nano)filler dispersion, thermal stability and adequate mechanical resistance. The flame retardant properties as shown by cone calorimetry showed significant increase in the ignition time compared to neat PLA and a substantial decrease, i.e., ca. 40%, of the maximum rate of heat release, whereas the UL94 HB test was successfully passed revealing non-dripping effect and extensive char formation. The study represents a new approach in formulating novel PLA grades with improved characteristic features.  相似文献   

5.
Summary: Starting from gypsum as by-product of lactic acid fabrication process, novel high performance composites have been produced by melt-blending PLA and this filler after a previous specific dehydration performed at 500 °C for min. 1h. Due to PLA sensitivity towards hydrolysis, the utilization of β-anhydrite II (AII) as filler is a prerequisite. Characterized by attractive mechanical and thermal properties due to good filler dispersion throughout the polyester matrix, these composites are interesting in biodegradable rigid packaging or technical applications. Interestingly, tensile strength of PLA – AII composites proved remarkably high, e.g. higher than 35 MPa at 50 wt-% filler content. However a decrease of impact properties has been recorded. To increase the toughness of these composites while preserving high stiffness an impact modifier based on ethylene copolymer has been mixed with both the polymer matrix and AII by melt-compounding. The effectiveness of the impact modifier was confirmed in both neat PLA and AII-based composites. Addition of 5-10 wt-% impact modifier into highly filled composites (30 to 40 wt-% filler) leads to an attractively threefold increase of impact strength with respect to the compositions without modifier, remarkable thermo-mechanical performances and good filler dispersion.  相似文献   

6.
30 wt% aligned untreated long hemp fibre/PLA (AUL) and aligned alkali treated long hemp fibre/PLA (AAL) composites were produced by film stacking and subjected to accelerated ageing. Accelerated ageing was carried out using UV irradiation and water spray at 50 °C for four different time intervals (250, 500, 750 and 1000 h). After accelerated ageing, tensile strength (TS), flexural strength, Young's modulus (YM), flexural modulus and mode I fracture toughness (KIc) were found to decrease and impact strength (IS) was found to increase for both AUL and AAL composites. AUL composites had greatest overall reduction in mechanical properties than that for AAL composites upon exposure to accelerated ageing environment. FTIR analysis and crystallinity contents of the accelerated aged composites support the results of the deterioration of mechanical properties upon exposure to accelerated ageing environment.  相似文献   

7.
Poly(lactic acid)(PLA) composites with 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide(DOPO) and DOPOcontaining polyhedral oligomeric silsesquioxane(DOPO-POSS) were prepared via melting extrusion and injection molding. The crystallization, mechanical, and flame-retardant properties of PLA/DOPO and PLA/DOPO-POSS were investigated by differential scanning calorimetry(DSC), X-ray diffraction(XRD), tensile testing, thermogravimetric analysis(TGA), limiting oxygen index(LOI),and cone calorimeter test. The DSC results showed that the DOPO added could act as a plasticizer as reflected by lower glass transition temperature and inhibited crystallization of part of the PLA; the DOPO-POSS acted like a filler in the PLA matrix and slightly improved the crystallinity of the PLA matrix. The XRD and DSC analyses indicated that the PLA composites by cold molding injection were amorphous, and the PLA composites following a heat treatment in an oven at 120 °C for 30 min achieved crystallinity. All the PLA and its composites after heat treatment had improved mechanical properties. The thermogravimetric analysis(TGA) tests showed that the PLA,DOPO and DOPO-POSS decomposed separately in the PLA/DOPO and PLA/DOPO-POSS, respectively. The cone calorimeter tests offered clear evidence that addition of the DOPO-POSS resulted in an evident reduction of 25% for the peak of heat release rate(p-HRR).It was also confirmed that the crystalline flame-retardant PLA composites after heat treatment had better flame retardant properties than the amorphous PLA composites prepared by the cold molding.  相似文献   

8.
Hybrid sisal fibers (HSFs) were made by mixing untreated sisal fibers with alkali-treated sisal fibers (ASFs), and the HSFs were blended with polylactic acid (PLA) matrix. Then the diatomite particles were added into the PLA/HSFs composite to make PLA/HSFs/diatomite composite. The effect of these two fillers on mechanical and thermal properties was investigated. The results showed that the reinforcing effect of HSFs was better than ASFs. Mechanical and thermal properties (especially the impact strength and crystallinity) of PLA/HSFs were higher than that of PLA/ASFs. The addition of diatomite further improved the mechanical and thermal properties of PLA composites.  相似文献   

9.
Polylactide (PLA)/starch blend/clay and PLA/clay composites are prepared by melt blending. Structural and thermal characterizations are performed by differential scanning calorimetry, X-ray diffraction analysis, and thermogravimetric analysis. The fire properties are assessed on a dual cone calorimeter. Combustion residue and char formation is characterized by optical microscopy and attenuated total reflection infrared spectroscopy. Although the clay is not fully intercalated/exfoliated, the composites exhibit a higher thermal stability and much reduced peak heat release rate, and the PLA/starch blend composite retains its mechanical properties. For the PLA/starch blend composite, smoke release is also considerably reduced. Catalyzed, oxidative decomposition is shown to occur early in the thermal decomposition of the composites, prior to increased thermal stability. The inclusion of clay promotes char formation and increases the quantity of carbonaceous char in the combustion residue. There is minimal migration of the clay to the surface prior to ignition and char is formed mainly after ignition and during burning. During the later stages of burning some of the char formed is converted to CO2.  相似文献   

10.
Large amounts of stable β-anhydrite II (AII), a specific type of dehydrated gypsum and a by-product of lactic acid production process, can be melt-blended with bio-sourced and biodegradable polylactide (PLA) to produce economically interesting novel composites with high tensile strength and thermal stability.To enhance their toughness, while preserving an optimal stiffness, selected low molecular weight plasticizers (bis(2-ethylhexyl) adipate and glyceryl triacetate) and polymeric adipates with different molecular weights have been mixed with a specific PLA (l/d isomer ratio of 96/4) and 40 wt% of AII using an internal kneader. Addition of up to 10 wt% plasticizer into these highly filled compositions can trigger a fourfold increase of the impact strength with respect to the compositions without any modifier, cold crystallization properties and a significant decrease of their glass transition temperature. Moreover, these ternary compositions (PLA-AII-plasticizer) are clearly characterized by easier processing, notable thermo-mechanical performances and good filler dispersion. This study represents a new approach in formulating novel melt-processable polyester grades with improved characteristic features using PLA as biodegradable polymer matrix.  相似文献   

11.
We have prepared a series of polylactide/exfoliated graphite (PLA/EG) nanocomposites by melt‐compounding and investigated their morphology, structures, thermal stability, mechanical, and electrical properties. For PLA/EG nanocomposites, EG was prepared by the acid treatment and following rapid thermal expansion of micron‐sized crystalline natural graphite (NG), and it was characterized to be composed of disordered graphite nanoplatelets. It was revealed that graphite nanoplatelets of PLA/EG nanocomposites were dispersed homogeneously in the PLA matrix without forming the crystalline aggregates, unlike PLA/NG composites. Thermal degradation temperatures of PLA/EG nanocomposites increased substantially with the increment of EG content up to ~3 wt %, whereas those of PLA/NG composites remained constant regardless of the NG content. For instance, thermal degradation temperature of PLA/EG nanocomposite with only 0.5 wt % EG was improved by ~10 K over PLA homopolymer. Young's moduli of PLA/EG nanocomposites increased noticeably with the increment of EG content up to ~3 wt %, compared with PLA/NG composites. The percolation threshold for electrical conduction of PLA/EG nanocomposites was found to be at 3–5 wt % EG, which is far lower graphite content than that (10–15 wt % NG) of PLA/NG composites. © 2010 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 48: 850–858, 2010  相似文献   

12.
To increase the thermal and mechanical properties of poly(l-lactic acid) (PLA), a nontoxic biomesogen PFBH derived from ferulic acid (FA), 4-hydroxybenzoic acid (HBA) and 1,6-hexanediol (HD) was introduced into the PLA backbones by solution polymerization of PLA, PFBH and chain linker hexamethylene diisocyanate (HDI). The content of PFBH was varied from 0 to 30 mol% so that the effects of the biomesogen content on the thermal and physical properties, morphological textures and enzymatic degradation were examined, respectively. The synthesized materials were characterized by means of differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), wide angle X-ray diffraction (WAXD), polarizing light microscopy (PLM) and mechanical property measurements. It was found that introducing biomesogenic units could increase the thermal stability and reinforce the elastic properties, while reduced the melting temperature, the degree of crystallinity and the enzymatic degradation rate. The nontoxicity and biocompatibility of degradation would make the products promising candidates for medical applications in the area of tissue engineering.  相似文献   

13.
In order to modify the brittleness and flame retardant properties of poly(lactic acid) (PLA), a series of flame retardant toughened PLA composites were prepared using poly(ethylene glycol) 6000 (PEG6000) as a toughening and charring agent together with ammonium polyphosphate (APP) as an acid source and blowing agent. The fire and thermal behavior of PLA/PEG/APP composites was evaluated by limiting oxygen index (LOI), UL‐94, cone calorimeter, and thermogravimetric analysis (TGA). The results showed that the PLA/PEG/APP system had good charring ability and could improve the flame retardancy of PLA. When the content of APP in the composites was more than 5 wt%, all samples could reach UL‐94 V‐0 rating. The results of mechanical property tests demonstrated that the brittleness of PLA was also improved after blended with PEG6000. All the PLA/PEG/APP composites with an APP content of less than 10 wt% showed an obvious neck and fracture behavior, that is, the tensile behavior of PLA was changed from brittle to ductile. Copyright © 2010 John Wiley & Sons, Ltd.  相似文献   

14.
Poly(lactic acid) (PLA)/poly(butylene succinate) (PBS) blends were prepared using a carboxylic acid salt as nucleating agent (NA). The effect of NA on the crystallization kinetics of PLA and PLA/PBS blend was investigated using a differential scanning calorimeter, a polarized optical microscope and a wideangle X-ray diffractometer. The crystallization rate of PLA component in PLA/PBS blends is increased effectively by NA through fast nucleation and growth rate of PLA α'-form crystal, which is confirmed by isothermal crystallization behavior of PLA/PBA/NA composites. The isothermal crystallization results also show that the incorporation of NA induces heterogeneous nucleation mechanism in PLA component. The increased number of crystal nuclei hinders the increase of average grain size of PLA component in composites but contributes to a higher crystallinity of both PLA and PBS components in PLA/PBS blends. Finally, the mechanical properties and dynamic mechanical properties of PLA/PBS/NA composites are improved because of the increased crystallinity, which are superior to that of PLA/PBS blend.  相似文献   

15.
Poly(lactic acid) (PLA) composites consisting of PLA, rice starch (RS) (0–50 wt%) and epoxidised natural rubber (ENR50) were compounded by a twin-screw extruder and compression moulded into dumbbell specimens. Tensile tests were performed to characterize the mechanical properties of the PLA/RS composites. Morphological studies were done on the tensile fractured surface of the specimens by using scanning electron microscopy (SEM). Twenty weight percent of RS achieved a good balance of strength and stiffness. Beyond 20 wt% loading of RS, the tensile strength and elongation at break of PLA decreased drastically. This may be attributed to the agglomeration of RS, which could then act as stress concentrator. The incorporation of ENR50 increased the tensile strength and elongation at break of the PLA/RS composites remarkably, owing to the elastomeric behaviour and compatibilisation effects of ENR50. Interestingly, the morphology of PLA/RS composites transformed to a more ductile one with the addition of ENR. The kinetics of water absorption of the PLA/RS composites conforms to Fick's law. The Mm and D values are dependent on the RS and ENR concentrations. The tensile properties of the PLA/RS composites deteriorated after water absorption. The retention-ability and recoverability of the PLA/RS composites are relatively low, attributed to the hydrolysis of PLA, degradation of the PLA–RS interface and leaching of the RS particles. In addition, the tensile properties of PLA/RS composites decreased drastically upon exposure to enzymatic degradation. Extensive pinhole and surface erosion on the PLA/RS composites indicate high degree of hydrolysis. Whilst the addition of ENR leads to some improvements in tensile properties, nevertheless, it enhanced the biodegradability of the PLA/RS composites when exposed to water and -amylase enzymatic treatments.  相似文献   

16.
以竹粉(bamboo flour,BF)为生物质填料,乙酰柠檬酸丁酯(acetyl tributyl citrate,ATBC)为增韧剂,通过与聚乳酸(polylactic acid,PLA)熔融共混制备了BF/PLA增韧复合材料,并采用红外光谱、热重分析、转矩流变仪、扫描电镜及力学性能测试等考察了ATBC添加对BF/PLA复合材料结构与性能的影响。结果表明,ATBC可改善BF/PLA复合材料的加工流变性,降低复合材料玻璃化转变温度、冷结晶温度及熔融温度,但对复合材料的热稳定性没有影响。FTIR分析显示,ATBC的加入可使BF/PLA复合材料C—O红外吸收峰位增大,表明ATBC与PLA之间存在一定相互作用。当ATBC用量为15%时,BF/PLA复合材料断裂伸长率由增韧前的8.1%增加到35.6%,提高了339.5%。SEM图片显示,此时复合材料断面粗糙,表现出韧性断裂形貌。该研究结果可为进一步探索增韧竹纤维/聚乳酸复合材料制备及应用,提供试验数据和理论参考。  相似文献   

17.
To develop environmental‐friendly and flame‐retarded polymer composites, bio‐based polylactic acid (PLA) was loaded with thermally stable polyhedral octaphenyl silsesquioxane (OPS). Pure PLA and PLA/OPS composites with the OPS of 1, 3, 5, and 10 wt% were prepared by extrusion and injection molding, respectively. The scanning electron microscopy (SEM), polarized optical microscope (POM), differential scanning calorimetry (DSC), X‐ray diffraction (XRD), and thermal gravimetric analysis (TGA) were used to analyze the dispersion of the OPS in the PLA matrix and the effects of OPS on the crystallization and thermal stability properties of PLA/OPS composites, respectively. Limited oxygen index (LOI) and cone calorimeter (CONE) measurements were used to study flame retardancy of PLA and PLA/OPS composites. In order to study the flame‐retardant mechanism, the char residues were investigated by SEM, Fourier transform infrared spectra (FTIR), and X‐ray photoelectron spectroscopy (XPS). TGA‐FTIR was used to analyze the gaseous products of their thermal decomposition. The results show that the OPS particles were submicron in the PLA and could increase the crystallization rate of PLA and form small‐sized secondary α‐form crystalline compared with the pure PLA spherulite. The PLA and OPS decomposed individually in the PLA/OPS composites by TGA. According to the LOI tests, the PLA with the OPS loading exhibited very small reduction of LOI. However, the CONE tests indicated that the OPS could improve the flame retardancy of the PLA by means of low peak heat release rate and average heat release rate. It was obtained that the degree and type of the PLA crystalline for the pure PLA and PLA/OPS affect their flame retardancy. In the max thermal decomposition stage of PLA and PLA/OPS, their gaseous products were similar; at high temperatures, the PLA/OPS produced simple and clear gaseous products of PLA with solid SiO2 in the gas phase.  相似文献   

18.
Poly(lactic acid) (PLA) composites containing 5 wt% synthetic (type 4A) and natural (chabazite) zeolites were prepared using extrusion/injection molding. Morphological, structural, and thermal properties of composites were investigated by scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR), and differential scanning calorimetry (DSC). DSC results revealed that the glass transition and melting temperatures were not significantly changed; however, the incorporation of both type 4A and chabazite zeolites enhanced the nucleation of PLA crystallites as well as increased the percent crystallinity. Thermal degradation properties of PLA and PLA/zeolite composites were studied by non-isothermal thermogravimetric analysis (TGA) in nitrogen atmosphere. TGA results showed that at temperatures above 300 °C, PLA/type 4A synthetic zeolite composites were thermally decomposed more easily than the PLA and PLA/chabazite natural zeolite composites. The apparent activation energies of thermal degradation of PLA and PLA/zeolites composites estimated using both the Flynn-Wall-Ozawa and Kissinger methods followed the same order: PLA/type 4A < PLA/chabazite < PLA.  相似文献   

19.
A number of experimental techniques are employed to characterize physical and thermal properties of poly(lactic acid), PLA. To characterize PLA in terms of molecular mass and molecular mass distribution, size exclusion chromatography was used. The value of the specific refractive index increment was measured by differential refractometry. The thermal properties of semicrystalline PLA were measured by standard and temperature-modulated differential scanning calorimetry. The thermal stability of PLA was monitored by measuring the changes of mass using thermogravimetric analysis. The mechanical properties of amorphous PLA were measured by dynamic mechanical analysis and the results were discussed and compared with DSC in the glass transition region.  相似文献   

20.
A combination of solution casting and melt extrusion technique was used to fabricate Boron nitride (BN)-filled Polylactic acid (PLA)/polybutylene adipate terephthalate (PBAT) blend composites. The BN particles were surface treated with a silane coupling agent and functionalization was confirmed via spectroscopic analysis. Field emission scanning electron microscopy confirmed that the BN surface treatment improved the particle adhesion with the polymer matrices and acted as a compatibilizer for the polymers. Moreover, changes in the particle orientation in the blend composite yielded improved thermal conductivity in different directions. The inclusion of the treated BN particles enhanced the in-plane (~1.1 W m−1K−1) and through-plane (~0.8 W m−1K−1) thermal conductivity of the composites as compared to the neat PLA. In addition, the storage modulus of the composite become more than 3 GPa that is twice that of the PLA/PBAT blend with a reasonable tensile property. In general, compared with the PLA/PBAT blend, the blend composites exhibited superior thermal and mechanical properties.  相似文献   