Femtosecond laser ablation characteristics of nickel-based superalloy C263
Authors:N G Semaltianos  W Perrie  P French  M Sharp  G Dearden  S Logothetidis and K G Watkins
Institution:(1) Department of Engineering, University of Liverpool, Brownlow Hill, Liverpool, L69 3GH, UK;(2) Department of Physics, Aristotle University of Thessaloniki, Thessaloniki, 54124, Greece
Abstract:Femtosecond laser (180 fs, 775 nm, 1 kHz) ablation characteristics of the nickel-based superalloy C263 are investigated. The single pulse ablation threshold is measured to be 0.26±0.03 J/cm2 and the incubation parameter ξ=0.72±0.03 by also measuring the dependence of ablation threshold on the number of laser pulses. The ablation rate exhibits two logarithmic dependencies on fluence corresponding to ablation determined by the optical penetration depth at fluences below ∼5 J/cm2 (for single pulse) and by the electron thermal diffusion length above that fluence. The central surface morphology of ablated craters (dimples) with laser fluence and number of laser pulses shows the development of several kinds of periodic structures (ripples) with different periodicities as well as the formation of resolidified material and holes at the centre of the ablated crater at high fluences. The debris produced during ablation consists of crystalline C263 oxidized nanoparticles with diameters of ∼2–20 nm (for F=9.6 J/cm2). The mechanisms involved in femtosecond laser microprocessing of the superalloy C263 as well as in the synthesis of C263 nanoparticles are elucidated and discussed in terms of the properties of the material.
Keywords:PACS" target="_blank">PACS  79  20  Ds  81  05  Bx  68  37  Hk  68  37  Ps  81  07  -b
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号