马争争  李建青  田召明  邱洋  袁松柳 《中国物理 B》2012,21(10):107503-107503
The 0.6(Bi1-xLax)FeO 3-0.4SrTiO 3(x = 0,0.1) multiferroic ceramics are prepared by a modified Pechini method to study the effect of substitution of SrTiO3 and La in BiFeO3.The X-ray diffraction patterns confirm the single phase characteristics of all the compositions each with a rhombohedral structure.The magnetic properties of the ceramics are significantly improved by a solid solution with SrTiO3 and substitution of La.The values of the dielectric constant ε r and loss tangent tan δ of all the samples decrease with increasing frequency and become constant at room temperature.The La-doped 0.6BiFeO3-0.4SrTiO3 ceramics exhibit improved dielectric and ferroelectric properties,with higher dielectric constant enhanced remnant polarization(Pr) and lower leakage current at room temperature.Compared with a anti-ferromagnetic BiFeO3 compound,the 0.6(Bi0.9La0.1)FeO3-0.4SrTiO3 sample shows the optimal ferromagnetism with remnant magnetization M r ~ 0.135 emμ/g and ferroelectricity with Pr ~ 5.94 μC/cm 2 at room temperature.  相似文献   
2.
The 0.6(Bi1-xLax)FeO 3-0.4SrTiO 3(x = 0,0.1) multiferroic ceramics are prepared by a modified Pechini method to study the effect of substitution of SrTiO3 and La in BiFeO3.The X-ray diffraction patterns confirm the single phase characteristics of all the compositions each with a rhombohedral structure.The magnetic properties of the ceramics are significantly improved by a solid solution with SrTiO3 and substitution of La.The values of the dielectric constant ε r and loss tangent tan δ of all the samples decrease with increasing frequency and become constant at room temperature.The La-doped 0.6BiFeO3-0.4SrTiO3 ceramics exhibit improved dielectric and ferroelectric properties,with higher dielectric constant enhanced remnant polarization(Pr) and lower leakage current at room temperature.Compared with a anti-ferromagnetic BiFeO3 compound,the 0.6(Bi0.9La0.1)FeO3-0.4SrTiO3 sample shows the optimal ferromagnetism with remnant magnetization M r ~ 0.135 emμ/g and ferroelectricity with Pr ~ 5.94 μC/cm 2 at room temperature.  相似文献   
3.
溶胶凝胶法制备了Na0.5Bi0.5Ti1-xMnxO3(x=0,0.02,0.04)陶瓷样品,X射线衍射(XRD)分析表明陶瓷样品均形成了单一的钙钛矿(ABO3)型结构且没有杂质相的形成.随着Mn含量的增加,XRD峰向高角度方向移动,表明Mn离子进入Na0.5Bi0.5TiO3晶格.掺杂样品均表现出室温铁磁性和铁电性.磁测量表明样品中存在复杂的磁相互作用,包括铁磁,反铁磁和顺磁相互作用.以上结果表明,通过Mn的掺杂可以使铁电材料Na0.5Bi0.5TiO3转变为多铁材料.  相似文献   
1
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号