To achieve a high-quality high-κ/Ge interfaces for high hole mobility Ge p-MOSFET applications,a simple chemical cleaning and surface passivation scheme is introduced,and Ge p-MOSFETs with effective channel hole mobility up to665 cm2/V·s are demonstrated on a Ge(111) substrate.Moreover,a physical model is proposed to explain the dipole layer formation at the metal–oxide–semiconductor(MOS) interface by analyzing the electrical characteristics of HCl- and(NH4)2S-passivated samples. 相似文献
2.
Effect of the Si-doped In0.49Ga0.51P barrier layer on the device performance of In0.4Ga0.6As MOSFETs grown on semi-insulating GaAs substrates 下载免费PDF全文
In0.4Ga0.6As channel metal-oxide-semiconductor field-effect transistors (MOSFETs) with and without an Si-doped In0.49Ga0.51P barrier layer grown on semi-insulating GaAs substrates have been investigated for the first time. Compared with the In0.4Ga0.6As MOSFETs without an In0.49Ga0.51P barrier layer, In0.4Ga0.6As MOSFETs with an In0.49Ga0.51P barrier layer show higher drive current, higher transconductance, lower gate leakage current, lower subthreshold swing, and higher effective channel mobility. These In0.4Ga0.6As MOSFETs (gate length 2 μm) with an In0.49Ga0.51P barrier layer exhibit a high drive current of 117 mA/mm, a high transconductance of 71.9 mS/mm, and a maximum effective channel mobility of 1266 cm2/(V·s). 相似文献
3.
Effect of ultrathin GeO_x interfacial layer formed by thermal oxidation on Al_2O_3 capped Ge 下载免费PDF全文
We propose a modified thermal oxidation method in which an Al2O3 capping layer is used as an oxygen blocking layer (OBL) to form an ultrathin GeOx interracial layer, and obtain a superior Al2O3/GeOx/Ge gate stack. The GeOx interfacial layer is formed in oxidation reaction by oxygen passing through the Al2O3 OBL, in which theAl2O3 layer could restrain the oxygen diffusion and suppress the GeO desorption during thermal treatment. The thickness of the GeOx interfacial layer would dramatically decrease as the thickness of Al2O3 OBL increases, which is beneficial to achieving an ultrathin GeOx interfacial layer to satisfy the demand for small equivalent oxide thickness (EOT). In addition, the thickness of the GeOx interfacial layer has little influence on the passivation effect of the Al2O3/Ge interface. Ge (100) p-channel metal- oxide-semiconductor field-effect transistors (pMOSFETs) using the Al2O3/GeOx/Ge gate stacks exhibit excellent electrical characteristics; that is, a drain current on-off (Ionloft) ratio of above 1 104, a subthreshold slope of - 120 mV/dec, and a peak hole mobility of 265 cm2/V.s are achieved. 相似文献
4.
To achieve a high-quality high-κ/Ge interfaces for high hole mobility Ge p-MOSFET applications, a simple chemical cleaning and surface passivation scheme is introduced, and Ge p-MOSFETs with effective channel hole mobility up to 665 cm2/V.s are demonstrated on a Ge (111) substrate. Moreover, a physical model is proposed to explain the dipole layer formation at the metal-oxide-semiconductor (MOS) interface by analyzing the electrical characteristics of HCl- and (NH4)2S-passivated samples. 相似文献