(Na0.52K0.44Li0.04)Nb0.9-x Sbx Ta0.1O3 lead-free piezoelectric ceramics are prepared by a solid-state reaction method. With increasing Sb content, the transition temperature from orthorhombic to tetragonal polymorphic phase decreased. A composition (Na0.52K0.44Li0.04)Nb0.863Sb0.037Ta0.1O3 is found to possess excellent piezo- electric and electromechanical performances (d33 = 306pC/N, kp =48%, and kt=50%), and high Curie temperature (Tc = 320 ℃). These results indicate that (Na0.52K0.44Li0.04)Nb0.863Sb0.037 Ta0.1O3 is a promising lead-free piezoceramics replacement for lead zirconate titanate.  相似文献   
3.
Bi0.5 (Na0.72K0.28- x Lix )0.5 TiO3 (BNKLT- 100x) lead-free piezoelectric ceramics are synthesized by conventional solid state sintering techniques. The dielectric and piezoelectric properties of the BNKLT-100x ceramics as a function of Li content are systematically investigated. It is found that not only Li content but also the sintering temperature has a strong effect on the piezoelectric properties of BNKLT. The piezoelectric constant d33 Of BNKLT varies from 120 to 252pC/N in the Li content range from 0.03 to 0.16. In the sintering temperature range from 1080 to 1130℃, the d33 value of BNKLT-6 changes from 200pC/N to 252pC/N. The BNKLT-6 sample sintered at 1100℃ has the highest piezoelectric constant d33 of 252pC/N, with the electromechanical coupling factors kp of 0.32 and kt of 0.44.  相似文献   
4.
The effects of barium on electrical and dielectric properties of the SnO_2·Co_2O_3·Ta_2O_5 varistor system sintered at 1250℃ for 60min were investigated. It is found that barium significantly improves the nonlinear properties. The breakdown electrical field increases from 378.0 to 2834.5V/mm, relative dielectric constant (at 1kHz) falls from 1206 to 161 and the resistivity (at 1kHz) rises from 60.3 to 1146.5kΩ·cm with an increase of BaCO_3 concentration from 0mol% to 1.00mol%. The sample with 1.00mol% barium has the best nonlinear electrical property and the highest nonlinear coefficient (α=29.2). A modified defect barrier model is introduced to illustrate the grain-boundary barrier formation of barium-doped SnO_{2}-based varistors.  相似文献   
5.
研究了Sr对新型(Co, Nb)掺杂SnO2压敏材料微观结构和电学性质的影响.当SrCO 3的含量从零增加到1.50mol%时,(Co, Nb)掺杂SnO2压敏电阻的击穿电压从240V/mm猛增 到1482V/mm.样品的微观结构分析发现, 当SrCO3的含量从零增加到1.50 mol%时, SnO2的晶粒尺寸迅速减小.晶界势垒高度测量揭示,SnO2晶粒尺寸的迅速减小是击穿 关键词: 碳酸锶 二氧化锡 势垒 电学非线性  相似文献   
6.
(Sr,Co,Nb)掺杂SnO2压敏电阻的电学非线性   总被引:2,自引:2,他引:0       下载免费PDF全文
研究了Sr对新型(Co, Nb)掺杂SnO2压敏材料微观结构和电学性质的影响.当SrCO3的含量从零增加到1.50mol%时,(Co, Nb)掺杂SnO2压敏电阻的击穿电压从240V/mm猛增到1482V/mm.样品的微观结构分析发现, 当SrCO3的含量从零增加到1.50 mol%时, SnO2的晶粒尺寸迅速减小.晶界势垒高度测量揭示,SnO2晶粒尺寸的迅速减小是击穿电压急剧增高的主要原因.对Sr含量增加引起SnO2晶粒减小的根源进行了解释.掺杂1.50 mol% SrCO3的SnO2压敏电阻非线性系数为21.4,击穿电压高达1482V/mm.  相似文献   
7.
铌酸钾钠基无铅压电陶瓷的X射线衍射与相变分析   总被引:10,自引:0,他引:10       下载免费PDF全文
分析了斜方相、四方相铌酸钾钠基无铅压电陶瓷材料的结构和X射线衍射图谱的特点. 对于铌酸钾钠基压电材料斜方相结构, 从构成晶胞的一个单斜原胞进行分析, 计算出X射线衍射谱上每个衍射角附近的衍射峰数目和相对强度. 提出了2θ在20°—60°范围内根据(1 0 2)衍射峰(52°附近)和(1 2 1)衍射峰(57°附近)劈裂的数目区分斜方和四方相的新方法. 对于多晶陶瓷粉末, 可以更简便的由22°(或45°)附近前后峰的相对高低来判断斜方、四方相. 关键词: 铌酸钾钠 无铅压电陶瓷 X射线衍射 相变  相似文献   
8.
KNN Based Lead-Free Piezoceramics with Improved Thermal Stability   总被引:1,自引:0,他引:1       下载免费PDF全文
Lead-free piezoelectric ceramics (1 - x) (Na0.53K0.404 Li0.066)Nb0.92 Sb0.08 03 +xZrTiO3 are fabricated by conventional solid-state sintering method, and their dielectric and piezoelectric characteristics are investigated. With the addition of SrTiO3, the growth of the grain size is restrained, meanwhile the phase transition temperature of orthorhombic-tetragonal is shifted below room temperature. It is found that the ceramics with x = 0.010 exhibit excellent piezoelectric properties (d33 = 220 pC/N, kp = 41%, kt = 39%) and improved thermal stability around room temperature. The results indicate that these materials are promising lead-free piezoceramics for practical operations.  相似文献   
9.
The phase structures of lead-free (K0.48Na0.52)0.945Li0.055Sb0.05Nb0.95O3 piezoceramics are studied based on the measurements of ferroelectric and dielectric properties as well as the analyses of x-ray diffraction pattern and energy dispersive spectroscopy. The poled samples exhibit orthorhombic structure whereas the surface and interior for unpoled samples exhibit tetragonal and tetragonal-orthorhombic coexistent structures, respectively. These results are in agreement with the relative permittivity-temperature curves and demonstrate that phase transitions can be induced by Na volatilization and poling process. The remnant polarization Pr measured at 20°C increases continuously with the increase of electric field in the range of 2000-4000V/mm. This indicates that the polymorphic structure is more beneficial to the rotation or reorientation of dipoles than either the orthorhombic or the tetragonal structure. The randomly oriented domains may be the essential reason for the continuous rotation or reorientation and not good thermal stability.  相似文献   
10.
Lead-free (Na0.5K0.5)NbO3-xmol% ScTaO4 (x=0-1.5) ceramics are prepared using the conventional solid-state reaction method and their properties are investigated in detail. The results indicate that the piezoelectric properties and density are improved by the introduction of ScTaO4. Due to the high orthorhombic-tetragonal phase transition temperature TO-T (around 200°C), stable piezoelectric properties against temperature are obtained. In a wide temperature range of 15-160°C, kp of the (Na0.5K0.5)NbO3-0.5mol% ScTaO4 ceramic remains almost unchanged and d31 increases slightly from 59pC/N to 71pC/N. The deliquescent problem is effectively solved by the addition of ScTaO4. The piezoelectric properties of ScTaO4 modified (Na0.5K0.5)NbO3 ceramics show no obvious reduction and dielectric loss increases slightly after 120h of immersion. From the analysis, it is suggested that the density is an important factor that improves the humidity resistance of the specimens.  相似文献   