排序方式: 共有63条查询结果,搜索用时 15 毫秒
61.
采用反应磁控溅射方法,在(0001)蓝宝石单晶衬底上,制备了纳米多晶Gd2O3掺杂CeO2(GDC)氧离子导体电解质薄膜,采用X射线衍射仪(XRD)、原子力显微镜(AFM)对薄膜物相、结构、粗糙度、表面形貌等生长特性进行了表征,利用交流阻抗谱仪测试了GDC薄膜不同温度下的电学性能;实验结果表明,GDC薄膜为面心立方结构,在所研究的衬底温度范围内,均呈强(111)织构生长;薄膜表面形貌随衬底温度发生阶段性变化:衬底温度由室温升高到300℃时,
关键词:
2O3掺杂CeO2电解质薄膜')" href="#">Gd2O3掺杂CeO2电解质薄膜
反应磁控溅射
生长特性
电学性能 相似文献
62.
The energetic atom deposition of thin Au/Au(100) film has been studied by molecular dynamics simulation using the Au-Au interatomic interaction potential with embedded atom method. By investigating the variation of coverage curves and Bragg diffraction intensities during the film growth, the transition of Stranski-Kranstanov growth mode to Frank-van der Merwe growth mode was observed with the increase of the incident energy of deposition atoms. The role of energetic atoms in the film growth is discussed by analyzing the transport properties of deposited atoms and the evolution of incident energy and substrate temperatures. 相似文献
63.
高浓度Er/Yb共掺ZnO薄膜的结构及室温光致发光特性 总被引:3,自引:0,他引:3
采用射频磁控溅射方法制备了Er/Yb共掺ZnO薄膜,研究了退火处理对高浓度Er/Yb共掺ZnO薄膜的结构演化和光致发光(PL)特性的影响。X射线衍射分析结果表明:Er/Yb掺杂导致ZnO薄膜的晶粒细化及择优取向性消失,ZnO晶粒随退火温度的增加而逐渐长大。900℃退火时,出现Er3 、Yb3 偏析,退火温度高于1000℃时,薄膜与基体间发生了界面反应,1200℃时,ZnO完全转变为Zn2SiO4相。光致发光测量结果表明:高于900℃退火处理后,Er/Yb共掺ZnO薄膜在1540 nm附近具有明显的光致发光,发光强度在退火温度为1050℃时达到最大值;光致发光光谱呈现典型的晶体基质中Er3 离子发光光谱所具有的明锐多峰结构特征。此外,探讨了薄膜结构演化及其对光致发光光谱的影响。 相似文献