This study investigated and discovered a new miscible ternary blend system comprising three amorphous polymers: poly(vinyl acetate) (PVAc), poly(vinyl p‐phenol) (PVPh), and poly(methyl methacrylate) (PMMA) using thermal analysis and optical and scanning electron microscopies. The ternary compositions are largely miscible except for a small region of borderline ternary miscibility near the side, where the binary blends of PVAc/PMMA are originally of a borderline miscibility with broad Tg. In addition to the discovering miscibility in a new ternary blend, another objective of this study was to investigate whether the introduction of a third polymer component (PVPh) with hydrogen bonding capacity might disrupt or enhance the metastable miscibility between PVAc and PMMA. The PVPh component does not seem to exert any “bridging effect” to bring the mixture of PVAc and PMMA to a better state of miscibility; neither does the Δχ effect seem to disrupt the borderline miscible PVAc/PMMA blend into a phase‐separated system by introducing PVPh. Apparently, the ternary is able to remain in as a miscible state as the binary systems owing to the fact that PVPh is capable of maintaining roughly equal H‐bonding interactions with either PVAc or PMMA in the ternary mixtures to maintain balanced interactions among the ternary mixtures. © 2006 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 44: 1147–1160, 2006  相似文献   

2.
Blends of amorphous poly(DL‐lactide) (DL‐PLA) and crystalline poly(L‐lactide) (PLLA) with poly(methyl methacrylate) (PMMA) were prepared by both solution/precipitation and solution‐casting film methods. The miscibility, crystallization behavior, and component interaction of these blends were examined by differential scanning calorimetry. Only one glass‐transition temperature (Tg) was found in the DL‐PLA/PMMA solution/precipitation blends, indicating miscibility in this system. Two isolated Tg's appeared in the DL‐PLA/PMMA solution‐casting film blends, suggesting two segregated phases in the blend system, but evidence showed that two components were partially miscible. In the PLLA/PMMA blend, the crystallization of PLLA was greatly restricted by amorphous PMMA. Once the thermal history of the blend was destroyed, PLLA and PMMA were miscible. The Tg composition relationship for both DL‐PLA/PMMA and PLLA/PMMA miscible systems obeyed the Gordon–Taylor equation. Experiment results indicated that there is no more favorable trend of DL‐PLA to form miscible blends with PMMA than PLLA when PLLA is in the amorphous state. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 41: 23–30, 2003  相似文献   

3.
In this work, we report evidences of cocrystallization in ternary blends made of crystalline ferroelectric poly(vinylidene fluoride‐trifluorethylene) [P(VDF‐TrFE)] copolymers. Complete cocrystallization has been unequivocally demonstrated by the observation of just one Curie and one Melting temperature in their calorimetric thermograms. These temperatures were intermediary among the respective temperatures of the individual constituents, that is, P(VDF‐TrFE)72/28, P(VDF‐TrFE)63/37, and P(VDF‐TrFE)50/50. Dielectric and X ray diffraction data were used to complement the investigation. The binary blends made of 63/37 and 72/28 copolymers were found to be miscible in the entire range of composition, with the behavior of their Curie temperatures being well fitted by an equation very similar to that proposed by Gordon‐Taylor to describe the behavior of the glass transition temperatures in true binary blends. In the ternary crystalline system, we have found evidences that the complete miscibility of the binary blend made of 63/37 and 72/28 copolymers actually drives the P(VDF‐TrFE)50/50 copolymer to accommodate their chains in its binary crystalline structure. © 2010 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 48: 621–626, 2010  相似文献   

4.
Diglycidyl ether of bisfenol-A (DGEBA)/poly(vinyl acetate) (PVAc)/poly(4-vinyl phenol) brominated (PVPhBr) ternary blends cured with 4,4’-diaminodiphenylmethane (DDM) were investigated by differential scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMTA) and scanning electron microscopy (SEM). Homogeneous (DGEBA+DDM)/PVPhBr networks with a unique T g are generated. Ternary blends (DGEBA+DDM)/PVAc/PVPhBr are initially miscible and phase separate upon curing arising two T gs that correspond to a PVAc-rich phase and to epoxy network phase. Increasing the PVPhBr content the T gof the PVAc phase move to higher temperatures as a consequence of the PVAc-PVPhBr interactions. Different morphologies are generated as a function of the blend composition.  相似文献   

5.
Miscibility behavior of poly(3-hydroxybutyrate) [PHB]/poly(vinylidene chloride-co-acrylonitrile) [P(VDC-AN)] blends have been investigated by differential scanning calorimetry and optical microscopy. Each blend showed a single Tg, and a large melting point depression of PHB. All the blends containing more than 40% PHB showed linear spherulitic growth behavior and the growth rate decreased with P(VDC-AN) content. The interaction parameter χ12, obtained from melting point depression analysis, gave the value of −0.267 for the PHB/P(VDC-AN) blends. All results presented in this article lead to the conclusion that PHB/P(VDC-AN) blends are completely miscible in all proportions from a thermodynamic viewpoint. The miscibility in these blends is ascribed to the specific molecular interaction involving the carbonyl groups of PHB. © 1997 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 35: 2645–2652, 1997  相似文献   

6.
Even though poly(ethylene oxide) (PEO) is immiscible with both poly(l ‐lactide) (PLLA) and poly(vinyl alcohol) (PVA), this article shows a working route to obtain miscible blends based on these polymers. The miscibility of these polymers has been analyzed using the solubility parameter approach to choose the proper ratios of the constituents of the blend. Then, PVA has been grafted with l ‐lactide (LLA) through ring‐opening polymerization to obtain a poly(vinyl alcohol)‐graft‐poly(l ‐lactide) (PVA‐g‐PLLA) brush copolymer with 82 mol % LLA according to 1H and 13C NMR spectroscopies. PEO has been blended with the PVA‐g‐PLLA brush copolymer and the miscibility of the system has been analyzed by DSC, FTIR, OM, and SEM. The particular architecture of the blends results in DSC traces lacking clearly distinguishable glass transitions that have been explained considering self‐concentration effects (Lodge and McLeish) and the associated concentration fluctuations. Fortunately, the FTIR analysis is conclusive regarding the miscibility and the specific interactions in these systems. Melting point depression analysis suggests that interactions of intermediate strength and PLOM and SEM reveal homogeneous morphologies for the PEO/PVA‐g‐PLLA blends. © 2016 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2016 , 54, 1217–1226  相似文献   

7.
Blends of isotactic (natural) poly(3‐hydroxybutyrate) (PHB) and poly(methyl methacrylate) (PMMA) are partially miscible, and PHB in excess of 20 wt % segregates as a partially crystalline pure phase. Copolymers containing atactic PHB chains grafted onto a PMMA backbone are used to compatibilize phase‐separated PHB/PMMA blends. Two poly(methyl methacrylate‐g‐hydroxybutyrate) [P(MMA‐g‐HB)] copolymers with different grafting densities and the same length of the grafted chain have been investigated. The copolymer with higher grafting density, containing 67 mol % hydroxybutyrate units, has a beneficial effect on the mechanical properties of PHB/PMMA blends with 30–50% PHB content, which show a remarkable increase in ductility. The main effect of copolymer addition is the inhibition of PHB crystallization. No compatibilizing effect on PHB/PMMA blends with PHB contents higher than 50% is observed with various amounts of P(MMA‐g‐HB) copolymer. In these blends, the graft copolymer is not able to prevent PHB crystallization, and the ternary PHB/PMMA/P(MMA‐g‐HB) blends remain crystalline and brittle. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 1390–1399, 2002  相似文献   

8.
The miscibility of blends of phenolphthalein poly(ether ether sulfone) (PES-C) and poly(ethylene oxide) (PEO) was established on the basis of the thermal analysis results. Differential scanning calorimetry (DSC) studies showed that the PES-C/PEO blends prepared by casting from N,N-dimethylformamide (DMF) possessed a single, composition-dependent glass transition temperature (Tg), and thus that PES-C and PEO are miscible in the amorphous state at all compositions at lower temperature. At higher temperature, the blends underwent phase separation, and the PES-C/PEO blend system was found to display a lower critical solution temperature (LCST) behavior. The phase separation process in the blends has also been investigated by using DSC. Annealed at high temperatures, the PES-C/PEO blends exhibited significant changes of thermal properties, such as the enthalpy of crystallization and fusion, temperatures of crystallization and melting, depending on blend composition when phase separation occurred. These changes reflect different characteristics of phase structure in the blends, and were taken as probes to determine phase boundary. From both the thermal analysis and optical microscopy, the phase diagram of the blend system was established. © 1997 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 35 : 1383–1392, 1997  相似文献   

9.
Linear and four‐armed poly(l ‐lactide)‐block‐poly(d ‐lactide) (PLLA‐b‐PDLA) block copolymers are synthesized by ring‐opening polymerization of d ‐lactide on the end hydroxyl of linear and four‐armed PLLA prepolymers. DSC results indicate that the melting temperature and melting enthalpies of poly (lactide) stereocomplex in the copolymers are obviously lower than corresponding linear and four‐armed PLLA/PDLA blends. Compared with the four‐armed PLLA‐b‐PDLA copolymer, the similar linear PLLA‐b‐PDLA shows higher melting temperature (212.3 °C) and larger melting enthalpy (70.6 J g?1). After these copolymers blend with additional neat PLAs, DSC, and WAXD results show that the stereocomplex formation between free PLA molecular chain and enantiomeric PLA block is the major stereocomplex formation. In the linear copolymer/linear PLA blends, the stereocomplex crystallites (sc) as well as homochiral crystallites (hc) form in the copolymer/PLA cast films. However, in the four‐armed copolymer/linear PLA blends, both sc and hc develop in the four‐armed PLLA‐b‐PDLA/PDLA specimen, which means that the stereocomplexation mainly forms between free PDLA molecule and the inside PLLA block, and the outside PDLA block could form some microcrystallites. Although the melting enthalpies of stereocomplexes in the blends are smaller than that of neat copolymers, only two‐thirds of the molecular chains participate in the stereocomplex formation, and the crystallization efficiency strengthens. © 2014 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2014 , 52, 1560–1567  相似文献   

10.
The miscibility and thermal properties of poly(N‐phenyl‐2‐hydroxytrimethylene amine)/poly(N‐vinyl pyrrolidone) (PHA/PVP) blends were examined by using differential scanning calorimetry (DSC), high‐resolution solid‐state nuclear magnetic resonance (NMR) techniques, and thermogravimetric analysis (TGA). It was found that PHA is miscible with PVP, as shown by the existence of a single composition‐dependent glass transition temperature (Tg) in the whole composition range. The DSC results, together with the 13C crosspolarization (CP)/magic angle spinning (MAS)/high‐power dipolar decoupling (DD) spectra of the blends, revealed that there exist rather strong intermolecular interactions between PHA and PVP. The increase in hydrogen bonding and in Tg of the blends was found to broaden the line width of CH—OH carbon resonance of PHA. The measurement of the relaxation time showed that the PHA/PVP blends are homogeneous at least on the scale of 1–2 nm. The proton spin‐lattice relaxation in both the laboratory frame and the rotating frame were studied as a function of the blend composition, and it was found that blending did not appreciably affect the spectral densities of motion (sub‐Tg relaxation) in the mid‐MHz and mid‐KHz frequency ranges. Thermogravimetric analysis showed that PHA has rather good thermal stability, and the thermal stability of the blend can be further improved with increasing PVP content. © 1999 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 37: 237–245, 1999  相似文献   

11.
Polymer blends of poly(vinylphenol) (PVPh) and poly(styrene‐co‐vinylphenol) with poly(p‐acetoxystyrene) (PAS) were prepared by solution casting from tetrahydrofuran solution. The thermal properties and hydrogen bonding of the blends were investigated by differential scanning calorimetry (DSC) and Fourier transform infrared spectroscopy. Although hydrogen bonding existed between the PVPh and PAS segments, the experimental results indicated that PVPh is immiscible with PAS as shown by the existence of two glass‐transition temperatures over the entire composition range by DSC. This phenomenon is attributed to the strong self‐association of PVPh, intramolecular screening, and functional group accessibility effects of the PVPh/PAS blend system. However, the incorporation of an inert diluent moiety such as styrene into the PVPh chain renders the modified polymer to be miscible with PAS. Copolymers containing between 16 and 51 mol % vinylphenol were fully miscible with PAS according to DSC studies. These observed results were caused by the reduction of the strong self‐association of PVPh and the increase of the interassociation between PVPh and PAS segments with the incorporation of styrene on the PVPh chain. According to the Painter‐Coleman association model, the interassociation equilibrium constant of PVPh/PAS blends was determined by a model compound and polymer blend. Good correlation between these two methods was obtained after considering the intramolecular screening and functional group accessibility effect in the polymer blend. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 1661–1672, 2002  相似文献   

12.
A miscible homopolymer–copolymer pair viz., poly(ethyl methacrylate) (PEMA)–poly(styrene‐co‐butyl acrylate) (SBA) is reported. The miscibility has been studied using differential scanning calorimetry. While 1 : 1 (w/w) blends with SBA containing 23 and 34 wt % styrene (ST) become miscible only above 225 and 185 °C respectively indicating existence of UCST, those with SBA containing 63 wt % ST is miscible at the lowest mixing temperature (i.e., Tg's) but become immiscible when heated at ca 250 °C indicating the existence of LCST. Miscibility for blends with SBA of still higher ST content could not be determined by this method because of the closeness of the Tg's of the components. The miscibility window at 230 °C refers to the two copolymer compositions of which one with the lower ST content is near the UCST, while the other with the higher ST content is near the LCST. Using these compositions and the mean field theory binary interaction parameters between the monomer residues have been calculated. The values are χST‐BA = 0.087 and χEMA‐BA = 0.013 at 230 °C. © 2000 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 38: 369–375, 2000  相似文献   

13.
The phase behavior of a partially miscible blend of poly(ethylene oxide) (PEO) and cellulose acetate butyrate (CAB) and the crystalline microstructure of PEO in the blend were studied with differential scanning calorimetry (DSC), optical microscopy, and synchrotron small‐angle X‐ray scattering (SAXS) methods. PEO/CAB showed a lower critical solution temperature (LCST) of 168 °C at the critical composition of PEO of 60 wt %. All blend compositions showed a single glass‐transition temperature (Tg) when they were prepared at temperatures lower than the LCST. However, with increasing CAB content, Tg of the blend changed abruptly at 70 wt % CAB; that is, a cusp existed. Below 70 wt % CAB, the change in Tg with blend composition was predicted by the Brau–Kovacs equation, whereas this change was predicted by the Fox equation at higher CAB contents. A gradual but small depression of the melting point of PEO in the blend with an increasing amount of CAB suggested that the PEO/CAB blends exhibited a weak intermolecular interaction. From DSC and SAXS experiments, it was found that amorphous CAB was incorporated into the interlamellar region of PEO for blends with less than 20 wt % CAB, whereas it was segregated to exist in the interfibrillar region in PEO for other blends with larger amounts of CAB. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 1673–1681, 2002  相似文献   

14.
Thermal processing at various temperatures has been used to fabricate poly(vinylidene fluoride‐co‐trifluoroethylene) [P(VDF‐co‐TrFE)] films with varied crystalline properties in an attempt to improve their piezoelectric properties. Although the dielectric constant of the films annealed at higher temperature is smaller than that of cooled and quenched ones, it has been shown that the annealed films possess larger crystallinity and stacked lamellar crystal grain size. The ferroelectric domains deriving from crystal region in all the samples are effectively improved by hot polarization. As a result, the remnant polarizations (Pr) and coercive electric field (Ec) of the corresponding films are improved at a low frequency due to the response of dipoles in crystal phase, and the largest piezoelectric constant in the longitudinal thickness mode (d33=?25 pC/N) is obtained in an annealed copolymer film. The results illustrate improving the crystal structure of P(VDF‐co‐TrFE) is an effective way to realize high electromechanical properties, which provides broadly applied scenery for this kind of copolymer in piezoelectric components. © 2012 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys, 2012  相似文献   

15.
In a first step of this contribution, the observed glass transition temperature‐composition behavior of miscible blends of poly(styrene‐coN,N‐dimethylacrylamide) (SAD17) containing 17 mol % of N,N‐dimethylacrylamide and poly(styrene‐co‐acrylic acid) (SAA18, SAA27, and SAA32) containing increasing acrylic acid content, are analyzed according to theoretical approaches. Both Kwei and Brostow equations describe well the experimental data though better fits were obtained with the Brostow's approach. The specific interactions involved in these systems are a combination of intra and interassociation hydrogen bonding. The positive deviation from the linear mixing rule of Tg‐composition observed within the SAA18+SAD17 blend system, indicates that interassociation interactions are prevailing. More pronounced intra‐association interactions within the SAA32+SAD17 blend system led to a large negative deviation while a fine balance is established between these two types of interactions within the SAA27+SAD17 blend. A thermodynamic analysis was carried out according to the Painter‐Coleman association model. The miscibility and phase behavior of SAD17+SAA18 and SAD17+SAA27 blends are well predicted. However, this model predicts a partial miscibility of SAD17+SAA32 system. Finally, the fitting parameter free method developed by Coleman to predict the Tg‐composition behavior is applied. This method predicts fairly well the evolution trend of experimental Tgs of the SAA18+SAD17 and SAA27+SAD17 blend systems. However, the compositional dependence of SAA32+SAD17 blend Tg was not predictable by this method. © 2009 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 47:2074–2082, 2009  相似文献   

16.
In this study, we successfully report an intimate ternary blend system of polycarbonate (PC)/poly(methyl methacrylate) (PMMA)/poly(vinyl acetate) (PVAc) obtained by the simultaneous coalescence of the three guest polymers from their common γ‐cyclodextrin (γ‐CD) inclusion compound (IC). The thermal transitions and the homogeneity of the coalesced ternary blend were studied by differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA). The observation of a single, common glass transition strongly suggests the presence of a homogeneous amorphous phase in the coalesced ternary polymer blend. This was further substantiated by solid‐state 13C NMR observation of the T(1H)s for each of the blend components. For comparison, ternary blends of PC/PMMA/PVAc were also prepared by traditional coprecipitation and solution casting methods. TGA data showed a thermal stability for the coalesced ternary blend that was improved over the coprecipitated blend, which was phase‐segregated. The presence of possible interactions between the three polymer components was investigated by infrared spectroscopy (FTIR). The analysis indicates that the ternary blend of these polymers achieved by coalescence from their common γ‐CD–IC results in a homogeneous polymer blend, possibly with improved properties, whereas coprecipitation and solution cast methods produced phase separated polymer blends. It was also found that control of the component polymer molar ratios plays a key role in the miscibility of their coalesced ternary blends. Coalescence of two or more normally immiscible polymers from their common CD–ICs appears to be a general method for obtaining well‐mixed, intimate blends. © 2004 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 42: 4182–4194, 2004  相似文献   

17.
High molecular weight bisphenol A or hydroquinone‐based poly(arylene ether phosphine oxide/sulfone) homopolymer or statistical copolymers were synthesized and characterized by thermal analysis, gel permeation chromatography, and intrinsic viscosity. Miscibility studies of blends of these copolymers with a (bisphenol A)‐epichlorohydrin based poly(hydroxy ether), termed phenoxy resin, were conducted by infrared spectroscopy, dynamic mechanical analysis, and differential scanning calorimetry. All of the data are consistent with strong hydrogen bonding between the phosphonyl groups of the copolymers and the pendent hydroxyl groups of the phenoxy resin as the miscibility‐inducing mechanism. Complete miscibility at all blend compositions was achieved with as little as 20 mol % of phosphine oxide units in the bisphenol A poly(arylene ether phosphine oxide/sulfone) copolymer. Single glass transition temperatures (Tg) from about 100 to 200°C were achieved. Replacement of bisphenol A by hydroquinone in the copolymer synthesis did not significantly affect blend miscibilities. Examination of the data within the framework of four existing blend Tg composition equations revealed Tg elevation attributable to phosphonyl/hydroxyl hydrogen bonding interactions. Because of the structural similarities of phenoxy, epoxy, and vinylester resins, the new poly(arylene ether phosphine oxide/sulfone) copolymers should find many applications as impact‐improving and interphase materials in thermoplastics and thermoset composite blend compositions. © 1999 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 37: 1849–1862, 1999  相似文献   

18.
Various phase behavior of blends of poly(vinyl ether)s with polyesters of two types (highly crystalline and less crystalline with different main‐chains) were examined using differential scanning calorimetry (DSC) and optical microscopy (OM). Effects of varying the main‐chain polarity of the constituent polyesters on the phase behavior of the blends were analyzed. Miscibility in PVME/polyester blends was found only in polyesters with backbone CH2/CO ratio = 3.5 to 7.0). Tg‐composition relationships for blends of PVME with highly crystalline polyesters (PBA, PHS) were found to differ significantly from those for PVME blends with less‐crystalline polyesters (PTA, PEAz). Crystallinity of highly crystalline polyester constituents in blends caused significant asymmetry in the Tg‐composition relationships, and induced positive deviation of blends' Tg above linearity; on the other hand, blends of PVME with less crystalline polyesters exhibit typical Fox or Gordon‐Taylor types of relationships. The χ parameters for the miscible blends were found to range from ?0.17 to ?0.33, reflecting generally weak interactions. Phase behavior was analyzed and compared among blends of PVME with rapidly crystallizing vs. less‐crystallizing polyesters, respectively. Effects of polyesters' crystallinity and structures on phase behavior of PVME/polyester blends are discussed. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 45: 2899–2911, 2007  相似文献   

19.
Positron annihilation lifetime spectroscopy and differential scanning calorimetry (DSC) measurements were performed for blends of polyacrylamide (PAM) and poly(ethylene glycol) (PEG) and blends of poly(dimethylacrylamide) (PDMAM) and PEG. The samples were prepared by codissolution in a concentration range of 0–100 wt % PEG. The thermal behavior, characterized by DSC measurements, showed similar variations of the glass‐transition temperatures (Tg's) with the PEG concentration for the two systems. Pure PAM and PDMAM presented Tg's of 188 and 111 °C, respectively. A relatively small and nearly linearly decreasing Tg was observed for the two systems in the range of 20–80 wt % PEG. PEG crystals were present in all blend compositions, and no melting point depression was observed. The thermal results pointed to the partial miscibility of the blends. The degree of crystallinity of PEG increased with increasing PEG concentration for the PDMAM/PEG systems. The ortho‐positronium lifetime (τ3) increased with increasing PEG concentration for both blends. However, the parameter of the ortho‐positronium formation probability (I3) decreased with the PEG concentration. The product τI3, which was proportional to the total free volume fraction, was approximately constant with the PEG concentration for PDMAM blends and increased with the PEG concentration for PAM systems. This result may be interpreted as a consequence of a more heterogeneous structure in PAM blends. Scanning electron microscopy micrographs of blends with 40 and 80 wt % PEG provided evidence of the regions associated with PEG crystallites. © 2003 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 41: 1493–1500, 2003  相似文献   

20.
The miscibility of poly(hydroxyether terephthalate ester) (PHETE) with poly(4‐vinyl pyridine) (P4VP) was established on the basis of thermal analysis. Differential scanning calorimetry showed that each blend displayed a single glass‐transition temperature (Tg), which is intermediate between those of the pure polymers and varies with the composition of blend. The Tg‐composition relationship can be well described with Kwei equation with k = 1 and q = ?30.8 (K), suggesting the presence of the intermolecular specific interactions in the blend system. To investigate the intermolecular specific interactions in the blends, the model compounds such as 1,3‐diphenoxy‐2‐propanol, 4‐methyl pyridine, and ethyl benzoate were used to determine the equilibrium constants, according to Coleman and Painter model, to account for the association equilibriums of several structural moieties, using liquid Fourier transform infrared difference spectroscopy. In terms of the difference in the association equilibrium constant, it is proposed that there are the competitive specific interactions in the blends, which were confirmed by means of Fourier transform infrared spectroscopy of the blends. It is observed that upon adding P4VP to the system, the ester carbonyls of PHETE that were H‐bonded with the hydroxyl groups were released because of the formation of the stronger interchain association via the hydrogen bonding between the hydroxyls of PHETE and tertiary nitrogen atoms of P4VP. © 2006 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 44: 1618–1626, 2006  相似文献   