Polyethersulfone (PES) membrane, one of the most important polymeric materials because of its good chemical resistance, thermal stability, mechanical, and film‐forming properties, has already been used in hemodialysis, tissue engineering, and artificial organs. In order to improve the blood compatibility of PES membrane, many amphiphilic block copolymers have been synthesized and used as additives for surface modification. The object of this study is to develop a hydrophilic PES membrane by blending a comblike amphiphilic block copolymer poly (vinyl pyrrolidone)‐block‐poly [acrylate‐graft‐poly (methyl methacrylate)]‐block‐poly‐(vinyl pyrrolidone) [PVP‐b‐P (AE‐g‐PMMA)‐b‐PVP] synthesized by RAFT polymerization. The cytocompatibility performance of PVP‐b‐P (AE‐g‐PMMA)‐b‐PVP modified PES membrane was evaluated, which showed better cytocompatibility compared with that of pristine PES membrane. Endothelial cells cultured on the modified membranes present improved growth in terms of scanning electron microscope observation, MTT assay, and confocal laser scanning microscope observation. These results indicate that the modified membrane has great potential application in blood‐contact fields such as hemodialysis and bio‐artificial liver supports. Copyright © 2015 John Wiley & Sons, Ltd.  相似文献   

2.
从分子结构设计出发,采用自由基聚合、醚化、酯化、原子转移自由基聚合(ATRP)、可逆加成断裂链转移自由基聚合(RAFT)等方法合成了一系列具有不同分子结构(包括接枝、嵌段、交替、超支化等)和链形态(包括直链、梳状、哑铃状、链球状等)的两亲性共聚物,并对这些聚合物进行了谱学表征和性能测试.将这些两亲性共聚物与聚合物膜材料(包括聚偏氟乙烯、聚氯乙烯、聚砜、聚醚砜、聚醚砜酮等)进行溶液共混,通过相转化法制备共混膜,在成膜热力学和动力学分析的基础上,对共混膜的结构和性能进行调控.研究发现,两亲性共聚物在成膜过程中自发地向膜表面迁移富集,并进行自组装,在膜表面形成两亲性共聚物包膜,显著改善了聚合物多孔膜的亲水性和抗污染性能.此外,两亲性共聚物中的功能基团还可赋予共混膜某些功能特性,如生物相容性、环境响应性(pH、温度敏感性)、酶活性等.  相似文献   

3.
A styrene-maleic anhydride (SMA) alternating copolymer with ultrahigh molecular weight (Mw > 106) synthesized in super critical carbon dioxide (SC CO2) medium was used as hydrophilic polymeric additive in the preparation of polyethersulfone (PES) membranes. The PES/SMA blend membranes were prepared by immersion precipitation process. X-ray photoelectronic spectroscopy (XPS) measurements confirmed that the hydrolyzed SMA preferentially segregated to membrane–coagulant interface during membrane formation. For the PES/SMA blend membranes, no big change was observed in the cross-sectional structure and the mechanical properties were well maintained after SMA addition except that a thicker top layer was formed. The surface morphology analysis by atomic force microscopy (AFM) showed that the membrane surface roughness increased with the added SMA amount. The results of water contact angle, water absorbance measurements and static protein adsorption experiments revealed that the surface enrichment of SMA endowed PES/SMA blend membranes with significantly improved surface hydrophilicity and protein-adsorption resistance.  相似文献   

4.
A series of comb-like poly(phenylene oxide)s (PPO) graft copolymers with controlled grafting density and length of grafts were synthesized by atom transfer radical polymerization (ATRP). The α-bromo-poly(2,6-dimethyl-1,4-phenylene oxide)s (BPPO) were used as macroinitiators to polymerize vinyl monomers and the graft copolymers carrying polystyrene (PS), poly(p-acetoxystyrene) (PAS), and poly(methyl methacrylate) (PMMA) as side chains were synthesized and characterized by NMR, FTIR, GPC, DSC and TGA. The composition-dependent glass-transition temperatures (Tg) of PPO-g-PS exhibited good correlation with theoretical curve in Couchman equations except for the cases of low PS content (<40 mol%) copolymers in which a positive deviation was observed due to enhanced molecular interactions. The increase in monomer/initiator ratio led to the increase of degree of polymerization and the decrease of polydispersity. Despite the immiscibility nature between PPO and PMMA, the PPO-g-PMMA exhibited enhanced compatibilization as apparent single Tg in a wide temperature window throughout various compositions revealing an efficient segmental mixing on a molecular scale due to grafting structure.  相似文献   

5.
The surface of polyethersulfone (PES) membrane was modified by blending triblock copolymers of methoxyl poly(ethylene glycol)-polyurethane-methoxyl poly(ethylene glycol) (mPEG-PU-mPEG), which were synthesized through solution polymerization with mPEG Mns of 500 and 2000, respectively. The PES and PES/mPEG-PU-mPEG blended membranes were prepared through spin coating coupled with liquid-liquid phase separation. FTIR and (1)H NMR analysis confirmed that the triblock copolymers were successfully synthesized. The functional groups and morphologies of the membranes were studied by ATR-FTIR and SEM, respectively. It was found that the triblock copolymers were blended into PES membranes successfully, and the morphologies of the blended membranes were somewhat different from PES membrane. The water contact angles and platelet adhesion were decreased after blending mPEG-PU-mPEG into PES membranes. Meanwhile, the activated partial thromboplastin time (APTT) for the blended membranes increased. The anti-protein-fouling property and permeation property of the blended membranes improved obviously. SEM observation and 3-(4, 5-Dimethylthiazol-2-yl)-2, 5-diphenyl tetrazolium bromide (MTT) assay proved the surfaces of the blended membranes promoted human hepatocytes adhesion and proliferation better than PES membrane.  相似文献   

6.
Polymer blending is used to modify or improve the dimensional and thermal stability of any two different polymers or copolymers. In this study, both sulfonated polybenzimidazole homopolymer (MS-p-PBI 100) and sulfonated poly(aryl ether benzimidazole) copolymers (MS-p-PBI 50, 60, 70, 80, 90) were successfully synthesized from commercially available monomers. The chemical structure and thermal stability of these polymers was characterized by 1H NMR, FT-IR and TGA techniques. Blend membranes (BMs) were prepared from the salt forms of sulfonated poly(ether sulfone) (PES 70) and MS-p-PBI 100 using dimethylacetamide (DMAc). These blend membranes exhibited good stability in boiling water. The blending of 1 wt.% of MS-p-PBI 100 and 99 wt.% of PES 70 to produce the blend membrane BM 1 reduced membrane swelling, thus leading to good dimensional stability and comparable proton conductivity. Hence, BM 1 was chosen for the fabrication of a membrane electrode assembly (MEA) for proton exchange membrane fuel cell (PEMFC) and direct methanol fuel cell (DMFC) applications. This paper reports on PEMFC and DMFC performance under specific conditions.  相似文献   

7.
Chitosan-N-poly(ethylene glycol) brush copolymers with different degree of substitution (DS) were synthesized via reductive amination of chitosan by methoxy poly(ethylene glycol) (MPEG) aldehyde. Chitosan-N-MPEG copolymers were high-molecular-weight products with desirable DS; solubility and solution viscosity of those copolymers depended on the method of the synthesis of MPEG aldehyde and on DS. Synthesis of MPEG aldehyde by the use of TEMPO radical/BAIB was not suitable because of partial oxidation of methoxy groups of MPEG resulting in bifunctional PEG derivatives leading to cross-linking. Adsorption studies of chitosan-N-MPEG graft copolymers on silica surface show that these polymers adsorb in highly hydrated layers.  相似文献   

8.
To endow hydrophobic poly(vinylidene fluoride) (PVDF) membranes with reliable hydrophilicity and protein resistance, an amphiphilic hyperbranched-star polymer (HPE-g-MPEG) with about 12 hydrophilic arms in each molecule was synthesized by grafting methoxy poly(ethylene glycol) (MPEG) to the hyperbranched polyester (HPE) molecule using terephthaloyl chloride (TPC) as the coupling agent and blended with PVDF to fabricate porous membranes via phase inversion process. The chemical composition changes of the membrane surface were confirmed by X-ray photoelectron spectroscopy (XPS), and the membrane morphologies were measured by scanning electron microscopy (SEM). Water contact angle, static protein adsorption, and filtration experiments were used to evaluate the hydrophilicity and anti-fouling properties of the membranes. It was found that MPEG segments of HPE-g-MPEG enriched at the membrane surface substantially, while the water contact angle decreased as low as 49 degrees for the membrane with a HPE-g-MPEG/PVDF ratio of 3/10. More importantly, the water contact angle of the blend membrane changed little after being leached continuously in water at 60 degrees C for 30 days, indicating a quite stable presence of HPE-g-MPEG in the blend membranes. Furthermore, the blend membranes showed lower static protein adsorption, higher water and protein solution fluxes, and better water flux recovery after cleaning than the pure PVDF membrane.  相似文献   

9.
The single-step synthesis of proton conducting poly(vinylidene fluoride) (PVDF) graft copolymer electrolytes is demonstrated. The graft copolymers of PVDF backbone with poly(sulfopropyl methacrylate) (PVDF-g-PSPMA) and poly(styrene sulfonic acid) (PVDF-g-PSSA) were synthesized using PVDF as a macroinitiator for atom transfer radical polymerization (ATRP). 1H NMR and FT-IR spectroscopy show that the “grafting from” method using ATRP was successful and the maximum grafting degrees were 35 and 25 wt% for PVDF-g-PSPMA and PVDF-g-PSSA, respectively. The IEC values were 0.63 and 0.45 meq/g, the water uptakes were 46.8 and 33.4 wt% and the proton conductivities were 0.015 and 0.007 S/cm at room temperature, for PVDF-g-PSPMA and PVDF-g-PSSA, respectively. Both membranes exhibited excellent thermal stability up to around 350 °C, verified by thermal gravimetric analysis (TGA).  相似文献   

10.
Abstract

Hydrophilicity-controlled poly(arylene ether sulfone) copolymers with phenolphthalein-based carboxylic acid groups (PES-COOH-X) were synthesized via direct copolymerization by adjusting the feed molar ratio. The chemical structures of the obtained copolymers were confirmed by 1H nuclear magnetic resonance (NMR) spectroscopy. The copolymers showed good solubility in common aprotic solvents and exhibited excellent mechanical properties. The water contact angles of the obtained copolymers could be reduced by approximately 52% from 92.1° to 44.2° with increasing content of phenolphthalein-derived monomer, 2-[bis(4-hydroxyphenyl)methyl] benzoic acid (PPH-COOH), in the feed molar ratio. A series of PES-COOH-X membranes was prepared via a conventional immersion precipitation phase inversion method. The effects of the monomer feed molar ratio on the morphology, hydrophilicity, pure water flux, and water uptake of the prepared membranes were investigated. The results showed that the pure water flux of the PES-COOH-X membranes was significantly enhanced by almost a factor of two as compared to the pristine PES membrane. From the water contact angle data, it was identified that the hydrophilicity of the membranes was increased rapidly with increasing PPH-COOH content in the membranes. These hydrophilicity-controlled poly(arylene ether sulfone) copolymers may be considered as good candidates for separation membrane materials.  相似文献   

11.
Two enantiomeric amphiphilic graft copolymers consisting of water soluble poly(2‐hydroxyethyl methacrylate) (HEMA) and biodegradable oligo(L ‐lactide) (OLLA) or oligo(D ‐lactide) (ODLA) were synthesized by free radical copolymerization. HEMA‐OL(D)LA macromonomers were synthesized by ring opening polymerization of L ‐ or D ‐lactide. Both HEMA‐OLA macromonomers and graft copolymers were characterized by NMR spectroscopy and gel permeation chromatography. Graft copolymers and their stereocomplexes were analyzed by wide angle X‐ray diffraction and differential scanning calorimetry (DSC). Due to the formation of stereocomplex crosslinks between poly(HEMA) main chains, amphiphilic, biodegradable hydrogels prepared by blending of two enantiomeric poly(HEMA‐g‐OLLA) and poly(HEMA‐g‐ODLA) degraded more slowly in phosphate buffered saline than individual optically pure poly‐(HEMA‐g‐OL(D)LA).  相似文献   

12.
Three well-defined diblock copolymers of poly(methyl methacrylate-b-methacrylic acid)(P(MMA-b-MAA))were synthesized using atom transfer radical polymerization method and varying poly(methacrylic acid)(PMAA)chain lengths. These copolymers were blended with PVC to fabricate porous membranes via phase inversion process.Membrane morphologies were observed by scanning electron microscopy(SEM),and chemical composition changes of the membrane surfaces were measured by X-ray photoelectron spectroscopy(XPS).Static and dynamic protein adsorption experiments were used to evaluate antifouling properties of the blend membranes.It was found that,the blend membranes containing longer PMAA arm length showed lower static protein adsorption,higher water permeation flux and better protein solution flux recovery.  相似文献   

13.
Polymer blends of sulfonated poly(ether ether ketone) (SPEEK) and poly(ether sulfone) (PES) in N-methyl-2-pyrrolidinone (NMP) were prepared by solution casting. The investigation on water uptake, methanol uptake, permeability and proton conductivity has been conducted. The spin-lattice relaxation time in the rotating frame of PES/SPEEK blend was obtained from the results of cross-polarization magic angle spinning (CP/MAS) solid state 13C NMR. SPEEK blended with PES resulted in increasing , indicating the molecular motion of polymer chain was reduced. The glass transition temperature of the PES/SPEEK blend membranes were predicted by the Kwei equation. PES plays an important role in the decreasing water uptake, methanol uptake and methanol permeability while enhancing the thermal stability of the blend membrane, which shows the feasibility for direct methanol fuel cell.  相似文献   

14.
ABSTRACT

A-B Type block copolymer of N-vinylpyrrolidone (NVP) and 4-vinylpyridine (VPy) [poly(NVP-b-VPy) and graft copolymers of VPy onto copolymers of NVP with 4-vinylbenzyl N,N-diethyldithiocarbamate (VBDC) [poly(NVP-g-VPy) were synthesized by the iniferter method. the compatibility between NVP and VPy units in the copolymers was evaluated from the glass transition temperature of these copolymers. Hydroquinone was then oxidized by the synthesized NVP-VPy copolymers-Cu(II) complex catalysts. the influence of the distribution of each monomer unit in copolymers on the catalytic activity was studied by comparing the activity of these copolymers. the catalytic activity of these copolymers increased in the order: NVP-VPy blend polymer, poly(NVP-b-VPy), poly(NVP-g-VPy), random copolymer [poly(NVP-ran-VPy)]. This order parallels the compatibility between NVP units and VPy units in these copolymers.  相似文献   

15.
Amphiphilic graft copolymers are excellent additives for the development of antifouling membranes by nonsolvent induced phase separation. We report a convenient approach to the synthesis of novel graft copolymers with hydrophobic polyacrylonitrile (PAN) backbones and hydrophilic poly(2-hydroxyethyl methacrylate) (PHEMA) side chains. Atom transfer radical polymerization (ATRP) of 2-hydroxyethyl methacrylate was carried out with poly(acrylonitrile-co-p-chloromethyl styrene) (PAN-co-PCMS) as a macroinitiator in the presence of CuCl/2,2’-bipyridine at 50 °C in dimethyl sulfoxide. Kinetics of the graft polymerization was also evaluated. The synthesis of poly(acrylonitrile-co-p-chloromethyl styrene-g-2-hydroxyethyl methacrylate) (PAN-co-(PCMS-g-PHEMA)) can be relatively controlled when CMS (the ATRP sites) unit in the macroinitiator is around 5 mol%. Both the macroinitiators and graft copolymers were characterized by FTIR, NMR and GPC. The surface morphology and wettability of the copolymer films were studied by AFM and water contact angle measurement, respectively. We demonstrate that phase segregation between the PAN-co-PCMS backbones and the PHEMA side chains takes place and the surface hydrophilicity of the graft copolymers increases with the length of the PHEMA side chains. Because these amphiphilic graft copolymers can be synthesized in mass, they will be useful as latent additives for the fabrication of advanced PAN separation membranes.  相似文献   

16.
DMFC用PES/SPEEK共混阻醇质子交换膜   总被引:1,自引:0,他引:1  
将磺化聚醚醚酮(SPEEK, 磺化度DS为68.3%)和聚醚砜(PES)两种聚合物共混制得PES/SPEEK共混膜. DSC研究表明两种聚合物之间具有较好的相容性, 因而共混膜均匀致密, 未发生大尺度相分离. PES的混入能有效降低膜的溶胀度及甲醇透过系数. 纯SPEEK 膜40 ℃时在1 mol•L−1甲醇水溶液中溶胀度达到160%, 45 ℃时就完全溶解, 而含30%(w)PES的共混膜在80 ℃时的溶胀度仅有15%. 室温下含20%−30%(w)PES的共混膜的甲醇透过系数为1×10−7 cm2•s−1左右, 比Nafion 115膜的透过系数小一个数量级. 尽管80 ℃下30%(w)PES/SPEEK共混膜的电导率与Nafion 115膜相当, 但由于共混膜的厚度比Nafion 115膜小1/3左右, 膜电阻较小, 因而其电池性能比Nafion 115膜的好.  相似文献   

17.
In this study, styrene–maleic anhydride (SMA) copolymer was modified by ring opening reaction of its anhydride groups with diethanolamine (DEA). The modified SMA copolymer was blended in different concentrations (2.5, 4 and 5.5 %) with Polyethersulfone (PES) to improve the hydrophilicity of PES membranes and the corresponding blend membrane was prepared through phase inversion. The influence of SMA copolymer on morphology, mechanical properties, water flux, rejection and anti-fouling properties of blend membrane were investigated. The modified SMA and their composition were confirmed by FT-IR and 1HNMR techniques. The asymmetric structure of membrane was revealed by SEM. The water flux and contact angle results show that the hydrophilicity of membrane surface was increased by addition of SMA copolymer. The better anti-fouling properties of the PES/modified SMA blend membranes in comparison with the PES membrane also confirmed that the hydrophilicity of blend membrane enhances.  相似文献   

18.
Graft copolymers comprising poly(vinylidene fluoride‐co‐chlorotrifluoroethylene) backbone and poly(styrene sulfonic acid) side chains, i.e. P(VDF‐co‐CTFE)‐g‐PSSA were synthesized using atom transfer radical polymerization (ATRP) for composite nanofiltration (NF) membranes. Direct initiation of the secondary chlorinated site of CTFE units facilitates grafting of PSSA, as revealed by FT‐IR spectroscopy. The successful “grafting from” method and the microphase‐separated structure of the graft copolymer were confirmed by transmission electron microscopy (TEM). Wide angle X‐ray scattering (WAXS) also showed the decrease in the crystallinity of P(VDF‐co‐CTFE) upon graft copolymerization. Composite NF membranes were prepared from P(VDF‐co‐CTFE)‐g‐PSSA as a top layer coated onto P(VDF‐co‐CTFE) ultrafiltration support membrane. Both the rejections and the flux of composite membranes increased with increasing PSSA concentration due to the increase in SO3H groups and membrane hydrophilicity, as supported by contact angle measurement. The rejections of NF membranes containing 47 wt% of PSSA were 83% for Na2SO4 and 28% for NaCl, and the solution flux were 18 and 32 L/m2 hr, respectively, at 0.3 MPa pressure. Copyright © 2008 John Wiley & Sons, Ltd.  相似文献   

19.
Hydrophilic modification of ultrafiltration membranes was achieved through blending of Pluronic F127 with poly(ether sulfone) (PES). The chemical composition and morphology changes of the membrane surface were confirmed by water contact angle, X-ray photoelectron spectroscopy, scanning electron microscopy, and protein adsorption measurements. The decreased static water contact angle with an increase in the Pluronic F127 content indicated an increase of surface hydrophilicity. XPS analysis revealed enrichment of PEO segments of Pluronic F127 at the membrane surface. The apparent protein adsorption amount decreased significantly from 56.2 to 0 microg/cm(2) when the Pluronic F127 content varied from 0% to 10.5%, which indicated that the blend membrane had an excellent ability to resist protein adsorption. The ultrafiltration experiments revealed that the Pluronic F127 content had little influence on the protein rejection ratio and pure water flux. Most importantly, at a high Pluronic F127 content membrane fouling, especially irreversible fouling, has been remarkably reduced. The flux recoveries of blend membranes reached as high as 90% after periodic cleaning in three cycles.  相似文献   

20.
Graft copolymers of natural rubber and poly(dimethyl(acryloyloxymethyl)phosphonate) (NR-g-PDMAMP), and natural rubber and poly(dimethyl(methacryloyloxyethyl)phosphonate) (NR-g-PDMMEP), were prepared in latex medium via a “grafting from” methodology based on the photopolymerization of dimethyl(acryloyloxymethyl)phosphonate (DMAMP) and dimethyl(methacryloyloxyethyl) phosphonate (DMMEP), respectively, used as phosphorus-containing monomers. The grafting polymerization was initiated from N,N-diethyldithiocarbamate groups previously bound in side position of the rubber chains. The effects of monomer concentration on monomer conversion and grafting rate were investigated, showing that conversion and grafting rate increased with increasing monomer concentration and reaction time. Highest conversions and grafting rates were obtained with a molar ratio [DMAMP]/[initiating units] = 7 for a reaction time of 180 min. Calculation of the graft average length () from 1H NMR spectra of the synthesized graft copolymers showed values were in the range of 9-73. Visualizations of NR-g-PDMAMP and NR-g-PDMMEP latices by Transmission Electron Microscopy (TEM) showed that they exhibit core-shell morphologies. Degradation of NR-g-PDMAMP and NR-g-PDMMEP occurred in two steps: decomposition of dimethylphosphonate-functionalized grafts took place prior to the second step corresponding to the decomposition of NR backbone, but the degradation temperature of this last step was higher than that of pure NR.  相似文献   