1.
Amorphous gallium nitride (a-GaN) thin films were deposited on glass substrate by electron beam evaporation technique at room temperature and high vacuum using N 2 as carrier gas. The structural properties of the films was studied by X-ray diffraction (XRD) and scanning electron microscope (SEM). It was clear from XRD spectra and SEM study that the GaN thin films were amorphous. The absorbance, transmittance and reflectance spectra of these films were measured in the wavelength range of 300–2200 nm. The absorption coefficient spectral analysis in the sharp absorption region revealed a direct band gap of E g = 3:1 eV. The data analysis allowed the determination of the dispersive optical parameters by calculating the refractive index. The oscillator energy E 0 and the dispersion energy E d, which is a measure of the average strength of inter-band optical transition or the oscillator strength, were determined. Electrical conductivity of a-GaN was measured in a different range of temperatures. Then, activation energy of a-GaN thin films was calculated which equalled E a = 0:434 eV.  相似文献   

2.
The optical characterization of poly (ethylene oxide)/zinc oxide thin films has been done by analyzing the absorption spectra in the spectral wavelength region 380–800 nm using a ultraviolet-spectrophotometer at room temperature. Thin film polymer composites made of poly (ethylene oxide) (PEO) containing zinc oxide (ZnO) filler concentrations (0%, 2%, 6%, 10%, and 14%) by weight were used in this study. The optical results obtained were analyzed in terms of the absorption formula for non-crystalline materials. The optical energy gap and other basic optical constants such as dielectric constants and optical conductivity were investigated and showed a clear dependence on the ZnO filler concentration. It was found that the optical energy gap for the composite films is less than that for the neat PEO, and that it decreases as the ZnO concentration increases. Enhancement of the optical conductivity was observed with increase in the ZnO concentration. Dispersion of refractive index was analyzed using the Wemple–DiDomenico single oscillator model. The refractive index (n), extinction coefficient (k), and dispersion parameters (Eo, Ed) were calculated for the investigated films.  相似文献   

3.
Nanocrystalline cadmium selenide (nc-CdSe) thin films have been prepared by thermal evaporation using the inert gas condensation (IGC) technique. Transmission electron microscopy (TEM) studies show that the CdSe nanocrystals (NCs) are spherical in shape. Constant photocurrent method (CPM) is used to determine the value of absorption coefficient in low absorption region of as-deposited, annealed and light soaked nc-CdSe thin films. Values of optical band gap (Eg) have been determined by using Tauc's relation for as-deposited, annealed and light soaked nc-CdSe thin films from the α values evaluated from reflection and transmission measurements. We have used a derivative procedure to sub-gap absorption spectra in order to get information on the energetic distribution of the occupied density of states below Fermi level. Constants such as optical gap Eg, Urbach edge Eu have been obtained from CPM spectra in as-deposited, annealed and light soaked nc-CdSe thin films. Concentration of defect states has also been calculated in as-deposited, annealed and light soaked nc-CdSe thin films.  相似文献   

4.
A method has been proposed for determining the optical properties of a thin film layer on absorbing substrates. The film optical parameters such as thickness, refractive index, absorption coefficient, extinction coefficient and the optical energy gap of an absorbing film are retrieved from the interference fringes of the reflection spectrum at normal incidence. The envelopes of the maxima of the spectrum EM and of the minima Em are introduced in analytical forms to find the reflectance amplitudes at the interfaces and approximate values of the thin film refractive index. Then, the interference orders and film thickness are calculated to get accurate values of the needed optical parameters. There are no complex fitting procedures or assumed theoretical refractive index dispersion relations. The method is applied to calculate the optical properties of an epitaxial gallium nitride thin film on a silicon (1 1 1) substrate. Good agreement between our results and the published data are obtained.  相似文献   

5.
Thin films of Zn40Se60 were prepared by the vacuum thermal evaporation technique. The influence of annealed temperature on the structural and optical properties was investigated using the X-ray diffraction (XRD), scanning electron microscopy (SEM) and optical transmission. The XRD studies show that the as-deposited film is amorphous in nature, but the crystallinity improved with increasing the annealing temperature. Furthermore the particle size and crystallinity increased whereas the dislocation and strains decreased with increasing the annealing temperature. SEM studies showed that the annealing temperature induced changes in the morphology of the as-deposited sample. Various optical constant have been calculated for as-deposited and annealed films. The mechanism of the optical absorption follows the rule of direct transition. It was found that, the optical energy gap (Eg) decreased with increasing the annealing temperature. These results can be interpreted by the Davis and Motte model. On the other hand the maximum value of the refractive index (n) is shifted toward the long wavelength by increasing the annealing temperature.  相似文献   

6.
The influence of the thickness of the a-Si : H film on its optical properties was studied using spectrophotometric measurements of the film transmittance and reflectance in the wavelength range 200–3000 nm. Both the refractive index and the absorption coefficient were found to increase as the film thickness increased and the absorption edge shifted to lower energies. Both the optical energy gap, Eg, and Urbach parameter values, E0, decreased with increasing thickness. This decrease in Eg and E0 was slow for thicknesses above 400 nm.  相似文献   

7.
The present study focuses on the effects of gamma irradiation on structural and optical properties of polycrystalline Ga10Se85Sn5 thin films with a thickness of ~300?nm deposited by the thermal evaporation technique on cleaned glass substrates. X-ray diffraction patterns of the investigated thin films show that crystallite growth occurs in the orthorhombic phase structure. The surface study carried out by using the scanning electron microscope (SEM) confirms that the grain size increases with gamma irradiation. The optical parameters were estimated from optical transmission spectra data measured from a UV–vis-spectrophotometer in the wavelength range of 200–1100?nm. The refractive index dispersion data of the investigated thin films follow the single oscillator model. The estimated values of static refractive index n0, oscillator strength Ed, zero frequency dielectric constant ε0, optical conductivity σoptical and the dissipation factor increases after irradiation, while the single oscillator energy Eo decreases after irradiation. It was found that the value of the optical band gap of the investigated thin films decreases and the corresponding absorption coefficient increases continuously with an increase in the dose of gamma irradiation. This post irradiation changes in the values of optical band gap and absorption coefficient were interpreted in terms of the bond distribution model.  相似文献   

8.
We present the methodological framework of the Swanepoel method for the spectrophotometric determination of optical properties in thin films using transmittance data. As an illustrative case study, we determined the refractive index, thickness, absorption index, and extinction coefficient of a nanostructured 3 mol% Y2O3-doped ZrO2 (yttria stabilized zirconia, 3YSZ) thin film prepared by the sol-gel method and deposited by dipping onto a soda-lime glass substrate. In addition, using the absorption index obtained with the Swanepoel method, we calculated the optical band gap of the film. The refractive index was found to increase, then decrease, and finally stabilize with increasing wavelength of the radiation, while the absorption index and extinction coefficient decreased monotonically to zero. These trends are explained in terms of the location of the absorption bands. We also deduced that this 3YSZ thin film has a direct optical band gap of 4.6 eV. All these results compared well with those given in the literature for similar thin films. This suggests that the Swanepoel method has an important role to play in the optical characterization of ceramic thin films.  相似文献   

9.
We have prepared SrTiO3/BaTiO3 thin films with multilayered structures deposited on indium tin oxide (ITO) coated glass by a sol-gel deposition and heating at 300-650 °C. The optical properties were obtained by UV-vis spectroscopy. The films show a high transmittance (approximately 85%) in the visible region. The optical band gap of the films is tunable in the 3.64-4.19 eV range by varying the annealing temperature. An abrupt decrease towards the bulk band gap value is observed at annealing temperatures above 600 °C. The multilayered film annealed at 650 ° C exhibited the maximum refractive index of 2.09-1.91 in the 450-750 nm wavelength range. The XRD and AFM results indicate that the films annealed above 600 ° C are substantially more crystalline than the films prepared at lower temperatures which were used to change their optical band gap and complex refractive index to an extent that depended on the annealing temperature.  相似文献   

10.
We report the structural and optical properties of high-energy ion-beam irradiated Co-doped magnesium titanate thin films. (Mg0.95Co0.05)TiO3 (MCT) thin films were deposited on quartz substrates using radio frequency magnetron sputtering. Subsequently, the films were annealed for crystallinity and were irradiated with 100?MeV Ag ions by varying the ion fluence. The X-ray diffraction patterns of the films before and after the irradiation were refined using the Rietveld refinement and the variations in the lattice parameters were correlated with the ion fluence. Although, annealing of thin films results in an enhancement in refractive index and optical bandgap, the ion fluence induces significant changes in the refractive index and optical bandgap. Atomic force microscopy is employed to study the surface morphology of the films. The impact of ion fluence on structural and optical properties of MCT thin films has been investigated.  相似文献   

11.
Chemical bath deposition of ZnS thin films from NH3/SC(NH2)2/ZnSO4 solutions has been studied. The effect of various process parameters on the growth and the film quality are presented. The influence on the growth rate of solution composition and the structural, optical properties of the ZnS thin films deposited by this method have been studied. The XRF analysis confirmed that volume of oxygen of the as-deposited film is very high. The XRD analysis of as-deposited films shows that the films are cubic ZnS structure. The XRD analysis of annealed films shows the annealed films are cubic ZnS and ZnO mixture structure. Those results confirmed that the as-deposited films have amorphous Zn(OH)2. SEM studies of the ZnS thin films grown on various growth phases show that ZnS film formed in the none-film phase is discontinuous. ZnS film formed in quasi-linear phase shows a compact and a granular structure with the grain size about 100 nm. There are adsorbed particles on films formed in the saturation phase. Transmission measurement shows that an optical transmittance is about 90% when the wavelength over 500 nm. The band gap (Eg) value of the deposited film is about 3.51 eV.  相似文献   

12.
CdSe thin films were deposited on glass substrates using Successive Ionic Layer Adsorption and Reaction (SILAR) method at room temperature and ambient pressure. The relationship between refractive index and energy bandgap was investigated. The film thickness effect on the structural, morphological, optical and electrical properties of CdSe thin films was investigated. The X-ray diffraction (XRD) and scanning electron microscopy (SEM) studies showed that all the films exhibit polycrystalline nature with hexagonal structure and are covered well with glass substrates. The crystalline and surface properties of the films improved with increasing film thickness. The optical absorption studies revealed that the films are found to be a direct allowed transition. The energy bandgap values were changed from 1.93 to 1.87 eV depending on the film thickness. The electron effective mass (me?/mo), refractive index (n), optical static and high frequency dielectric constant (εo, ε) values were calculated by using the energy bandgap values as a function of the film thickness. The resistivity of the films changed between 106 and 102 Ω-cm with increasing film thickness at room temperature.  相似文献   

13.
Cr doped CdO thin films were deposited on glass substrates by reactive DC magnetron sputtering with varying film thickness from 250 to 400 nm. XRD studies reveal that the films exhibit cubic structure with preferred orientation along the (2 0 0) plane. The optical transmittance of the films decreases from 92 to 72%, whereas the optical energy band gap of the films decreased from 2.88 to 2.78 eV with increasing film thickness. The Wemple–DiDomenico single oscillator model has been used to evaluate the optical dispersion parameters such as dispersion energy (Ed), oscillator energy (Eo), static refractive index (no) and high frequency dielectric constant (ε). The nonlinear optical parameters such as optical susceptibility (χ(1)), third order nonlinear optical susceptibility (χ(3)) and nonlinear refractive index (n2) of the films were also determined.  相似文献   

14.
We report results obtained from optical absorption studies carried out on amorphous silicon thin films deposited by plasma-enhanced chemical vapour deposition (PECVD) from silane plasma. The influence of the film thickness was studied on the two series of samples deposited from undiluted silane and under moderate hydrogen dilution of silane. Spectral refractive indices and absorption coefficients were determined from transmittance spectra. The spectral absorption coefficients were used to determine the Tauc optical band-gap energies Eg, the B factors of the Tauc plots, the iso-energy values E04 (energy at which the absorption coefficient is equal to 104 cm−1). The results were correlated with volume fractions of the amorphous phase and voids and with the film thickness.  相似文献   

15.
ZnO thin films were deposited by thermal evaporation of a ZnO powder. The as-deposited films are dark brown, rich zinc and present a low transmittance. Then, these films were annealed in air atmosphere at different temperatures between 100 and 400 °C. Their microstructure and composition were studied using XRD and RBS measurements respectively. By increasing the temperature, it was found that film oxidation starts at 250 °C. XRD peaks related to ZnO appear and peaks related to Zn decrease. At 300 °C, zinc was totally oxidised and the films became totally transparent. The electrical conductivity measurement that were carried out in function of the annealing temperature showed the transition from highly conductive Zn thin film to a lower conductive ZnO thin film. The optical gap (Eg) was deduced from the UV-vis transmittance, and its variation was linked to the formation of ZnO.  相似文献   

16.
Bismuth Zinc niobate (Bi1.5Zn1.0Nb1.5O7) thin films were deposited by pulsed laser deposition (PLD) method on fused silica substrates at different oxygen pressures. The structural, microwave dielectric and optical properties of these thin films were systematically studied for both the as-deposited and the annealed films at 600°C. The as-deposited films were all amorphous in nature but crystallized on annealing at 600°C in air. The surface morphology as studied by atomic force microscopy (AFM) reveals ultra-fine grains in the case of as-deposited thin films and cluster grain morphology on annealing. The as-deposited films exhibit refractive index in the range of 2.36–2.53 (at a wavelength of 750 nm) with an optical absorption edge value of 3.30–3.52 eV and a maximum dielectric constant of 11 at 12.15 GHz. On annealing the films at 600°C they crystallize to the cubic pyrochlore structure accompanied by an increase in band gap, refractive index and microwave dielectric constant.  相似文献   

17.
Transparent metal oxide thin films of samarium oxide (Sm2O3) were prepared on pre-cleaned fused optically flat quartz substrates by radio-frequency (RF) sputtering technique. The as-deposited thin films were annealed at different temperatures (873, 973 and 1073 K) for 4 h in air under normal atmospheric pressure. The topological morphology of the film surface was characterized by using atomic force microscopy (AFM). The optical properties of the as-prepared and annealed thin films were studied using their reflectance and transmittance spectra at nearly normal incident light. The estimated direct optical band gap energy (\(E_{\mathrm {g}}^{\mathrm {d}}\)) values were found to increase by increasing the annealing temperatures. The dispersion curves of the refractive index of Sm2O3 thin films were found to obey the single oscillator model.  相似文献   

18.
Electron beam gun technique was used to prepare Ta2O5 thin films onto infrasil substrates of thicknesses 333 and 666 nm. The structure characterization was investigated using X-ray diffraction patterns. Transmittance measurements in the wavelength range (240-2000 nm) were used to calculate the refractive index n and the absorption index k depending on Swanepole's method. The dispersion curve of the refractive index shows an anomalous dispersion in the absorption region and a normal one in the transparent region. The analysis of the optical absorption data revealed that the optical band gap Eg was indirect transition. It was found that the refractive index dispersion data obeyed the single oscillator of the Wemple-DiDomenico model, from which the dispersion parameters (Eo and Ed) and the high frequency dielectric constant were determined. The electric free carrier susceptibility and the carrier concentration to the effective mass ratio were estimated according to the model of Spitzer and Fan. Graphical representation of the relaxation time as a function of photon energy was also presented.  相似文献   

19.
Electron beam evaporation technique was used to prepare TiO2 and Ti2O3 thin films onto glass substrates of thicknesses 50, 500 and 1000 nm for each sample. The structural investigations revealed that the as-deposited films are amorphous in nature. Transmittance measurements in the wavelength range (350-2000 nm) were used to calculate the refractive index n and the absorption index k using Swanepoel's method. The optical constants such as optical band gap , optical conductivity σopt, complex dielectric constant, relaxation time τ and dissipation factor tan δ were determined. The analysis of the optical absorption data revealed that the optical band gap Eg was indirect transitions. The optical dispersion parameters Eo and Ed were determined according to Wemple and Didomenico method.  相似文献   

20.
Zinc selenide nanocrystalline thin films are grown onto amorphous glass substrate from an aqueous alkaline medium, using chemical bath deposition (CBD) method. The ZnSe thin films are annealed in air for 4 h at various temperatures and characterized by structural, morphological, optical and electrical properties. The as-deposited ZnSe film grew with nanocrystalline cubic phase alongwith some amorphous phase present in it. After annealing metastable nanocrystalline cubic phase was transformed into stable polycrystalline hexagonal phase with partial conversion of ZnSe into ZnO. The optical band gap, Eg, of as-deposited film is 2.85 eV and electrical resistivity of the order of 106-107 Ω cm. Depending upon annealing temperature, decrease up to 0.15 eV and 102 Ω cm were observed in the optical band gap, Eg, and electrical resistivity, respectively.  相似文献   