相似文献
 共查询到20条相似文献,搜索用时 578 毫秒
1.
利用X射线衍射和差示扫描量热分析研究了高温高压下Zr46.75Ti8.25Cu7.5Ni10Be27.5大块非晶合金的玻璃转变和晶化行为,结果发现压力降低了该大块非晶合金中的自由体积、热焓和晶化激活能. 关键词: 大块非晶合金 高压 差示扫描量热分析 玻璃转变  相似文献   

2.
利用X射线衍射技术、差示扫描量热分析技术和透射电子显微镜研究了非晶态Cu56Zr44合金的结构及其等温退火条件下的晶化过程.实验结果表明,非晶态Cu56Zr44合金在室温下的短程结构类似于硬球无规密堆积分布.在703K过冷液相区内等温退火时发现,当退火时间为3min时,晶化产物主要为Cu8Zr3相;当退火时间为6min时,Cu8Zr3关键词: 非晶态 56Zr44合金')" href="#">Cu56Zr44合金 结构 等温退火  相似文献   

3.
Amorphous Zr50Al15−xNi10Cu25Yx alloy powders were fabricated by mechanical alloying at low vacuum with commercial pure element powders. The effects on glass forming ability of Al partial substituted by Y in Zr50Al15Ni10Cu25 and thermal stability of Si3N4 powders addition were investigated. The as-milled powders were characterized by X-ray diffraction, scanning electron microscopy and differential scanning calorimeter. The results show that partial substitution of Al can improve the glass forming ability of Zr50Al15Ni10Cu25 alloy. Minor Si3N4 additions raise the crystallization activation energy of the amorphous phase and thus improve its thermal stability.  相似文献   

4.
A new amorphous Ti16.6Zr16.6Hf16.6Ni20Cu20A110 alloy has been developed using the novel equiatomic substitution technique. Melt spinning Ti16.6Zr16.6Hf16.6Ni20Cu20A110 forms an amorphous phase with a large supercooled liquid region, ΔT=70°C. After isothermal annealing within the supercooled liquid region for 3 h at 470°C, the amorphous alloy crystallizes to form a fine-scale distribution of 2–5 nm nanocrystals, and the supercooled liquid region increases to ΔT=108°C. Atomic-scale compositional analysis of this partially crystalline material using a three-dimensional atom probe (3DAP) is unable to detect any compositional difference between the nanocrystals and the remaining amorphous phase. After annealing for 1 hr at 620°C, the amorphous alloy crystallizes to form 20–50nm equiaxed grains of a hexagonal-type C14 Laves phase with lattice parameters a = 5.2Å and c = 9.0 Å. 3DAP analysis shows that this Laves phase has a composition very close to that of the initial amorphous phase, suggesting that the alloy crystallizes via a polymorphic rather than a primary crystallization mechanism, despite the complexity of the alloy composition.  相似文献   

5.
通过二次离子质谱仪(SIMS)研究了Mo在Zr57Nb5Cu15.4Ni12.6Al10非晶合金中的扩散,并计算出其扩散激活能Q和前置系数D0分别为1.95 eV和1.13×10-5m2s-1.根据Stokes-Einstern关系式研究了玻璃转变温度以下593—673 K之间Zr57Nb 关键词: 扩散 离子注入 二次离子质谱(SIMS) 黏滞特性  相似文献   

6.
We measured the electrical resistivity (4–300 K), superconducting critical temperature and thermal conductivity (0.5–7 K) of the amorphous metals Zr70Cu30 and La70Cu30. Heat treatments below crystallization temperature induced changes in these properties. In particular, in the first stage of the annealing of Zr70Cu30 there are systematic changes in the thermal conductivity and the critical temperature, while the electrical resistivity remains constant. We show that there is no simple correlation between the thermal conductivity processes in the low temperature and plateau regions. We also show that the thermal conductivity of as quenched La70Cu30 is typical of amorphous metals, contrary to information previously reported.  相似文献   

7.
利用透射电子显微镜对Ni67Zr33非晶合金晶化的研究发现了两个新的亚稳相T0与T10。其中T1相为体心正交(准四方〕晶体,点阵常数a≌b=0.89nm,c=3.14nm,空间群为Iba2或Ibam。温度升高,T1相转变为含有大量错排的A心正交Ni10Zr2相,用1/2(a+b)位移错排模型可以圆满地解释其电子衍射图中仅h+k为奇数的衍射斑沿c*方向拉长的现象,晶化稳定相为Ni10Zr,与Ni21Zr8(Ni5Zr2)相。 关键词:  相似文献   

8.
柳义  柳林  王俊  赵辉  荣利霞  董宝中 《物理学报》2003,52(9):2219-2222
应用同步辐射x射线小角散射法在原位对块体非晶合金Zr55Cu30Al 10Ni5在等温退火过程中的微结构变化进行研究.实验表明:在等温退火过程中电子 密度涨落反映了晶化之前的结构弛豫过程;在一定的退火温度下、随退火时间的增加,拓扑短程序弛豫与化学短程序弛豫之间存在一个电子密度均匀化的过程;导致这两种弛豫过程转变的退火时间与退火温度有关,温度越高,所需的退火时间越短. 关键词: 原位x射线小角散射 块体非晶合金 等温退火 结构弛豫  相似文献   

9.
刘俊明  吴状春  刘治国 《物理学报》1997,46(6):1146-1152
利用实时小角中子散射实验研究了非晶态Cu12.5Ni10Zr41Ti14Be22.5合金相分离的动力学标度性质.通过对相分离过程中实时小角中子散射谱进行详细的标度分析,揭示出散射函数S(q,t)(q为散射波矢,t为时间)在相分离的早期即达到动力学标度态,从而证明动力学标度假设也适用于描述深过冷液态的相分离过程 关键词:  相似文献   

10.
The crystallization of the amorphous Cu60Zr40 alloy has been studied by differential scanning calorimetry (DSC), scanning Auger microprobe (SAM) and transmission electron microscopy (TEM). The DSC trace showed that the sample exhibited a glass transition at 750 K and a strong exothermic effect beginning from 782 K. An enrichment of the element Zr and significant oxygen contamination in a zone near the surface to a depth of about 10 nm were revealed by SAM in the analysis of surface competition and depth profiles of the Cu60Zr40 sample. Also, the change of concentration ratio of Ca to Zr in amorphous matrix at the clean Cu60Zr40 surface as a function of annealing temperature was examined in detail, and it was found that the concentration of Zr at the surface is slightly higher than that in the bulk until 780K and that the concentration ratio of Cu to Zr in matrix has an abrupt increase in the temperature range of 780-800K. The observations by high resolution TEM revealed the appearance of cluster-like regions of approximately 1.5-2.0 nm in size just before crystallization and they distributed randomly throughout the sample. This phenomenon is analogous to the results obtained using field ion microscopy (FIM) by the present authors. The microstructural changes of the sample daring heating show the gradual crystallization of the amorphous matrix.  相似文献   

11.
同育全  申宝成  甘玉生  闫志杰 《物理学报》2005,54(10):4556-4561
通过在真空电弧熔炼炉内对合金铸锭进行反复熔炼处理,获得到了凝固组织不同的Zr65Al7.5Cu12.5Ni10Ag5合金铸锭.在相同的制备条件下,由凝固组织不同的合金铸锭通过吸铸法制备得到了薄片非晶合金.利用差示扫描量热法(DSC)对非晶合金的晶化动力学进行了分析.x射线衍射谱表明,在Zr65Al7.5Cu12.5Ni10Ag5非晶合金晶化过程中,二十面体准晶相(I相)作为初生相析出.Kissinger分析结果表明,合金铸锭的凝固组织细化,相对应的非晶合金发生晶化时,I相形成与分解的有效激活能都增大,说明非晶合金及析出的I相的热稳定性都提高.从结构的遗传性角度就合金铸锭凝固组织对相应非晶合金晶化过程中二十面体准晶相的形成动力学的影响进行了讨论. 关键词: 二十面体准晶相 晶化动力学 凝固组织  相似文献   

12.
X-ray diffraction experiments have been performed on amorphous sputtered Zr76Cu24 alloy in order to investigate the structural relaxation induced by thermal annealing below the crystallization temperature. Contrary to the low-temperature thermal properties which are very sensitive to heat treatments, only weak modifications affect the short-range structural order as defined by the total radial distribution function.  相似文献   

13.
孟庆格  李建国  周建坤 《中国物理》2006,15(7):1549-1557
Pr-based bulk metallic amorphous (BMA) rods (Pr60Ni30Al10) and Al-based amorphous ribbons (Al87Ni10Pr3) have been prepared by using copper mould casting and single roller melt-spun techniques, respectively. Thermal parameters deduced from differential scanning calorimeter (DSC) indicate that the glass-forming ability (GFA) of Pr60Ni30Al10 BMA rod is far higher than that of Al87Ni10Pr3 ribbon. A comparative study about the differences in structure between the two kinds of glass-forming alloys, superheated viscosity and crystallization are also made. Compared with the amorphous alloy Al87Ni10Pr3, the BMA alloy Pr60Ni30Al10 shows high thermal stability and large viscosity, small diffusivity at the same superheated temperatures. The results of x-Ray diffraction (XRD) and transmission electron microscope (TEM) show the pronounced difference in structure between the two amorphous alloys. Together with crystallization results, the main structure compositions of the amorphous samples are confirmed. It seems that the higher the GFA, the more topological type clusters in the Pr-Ni-Al amorphous alloys, the GFAs of the present glass-forming alloys are closely related to their structures.  相似文献   

14.
The logarithmic decrement and shear modulus of a bulk amorphous Zr52.5Ti5Cu17.9Ni14.6Al10 alloy were studied with an inverse torsion pendulum in the range from room temperature to the crystallization temperature and in the frequency range 5–40 Hz. The activation energy spectra of reversible and irreversible structural relaxation were estimated. The results obtained are discussed in the context of a two-energy-level model.  相似文献   

15.
黑祖昆  蒋为吉 《物理学报》1990,39(4):541-546
用透射电子显微镜对Ni51Zr49非晶合金的晶化过程进行了研究,发现晶化初期首先从非晶基体上析出的是具有C心单斜点阵的NiZr'相,a=0.3268nm,b=0.4101nm,c=0.5224nm,β=71.8°。与稳定相NiZr有很明确的取向关系:[100]NiZr'∥[100]NiZr [001]NiZr'∥[110]NiZr。它可以看成是NiZr相的亚稳态或超结构。随温度升高,逐渐转变成NiZr相。温度再高时,在非晶基体上还会析出少量Ni10Zr7相。晶化初期,无论是NiZr还是NiZr'相,都是以多次孪晶的形式析出。孪晶有这两种基本形式,一种是以NiZr或NiZr'的[021]方向为轴的180°孪晶,一种是以NiZr的[001]或NiZr'的[010]方向为轴的36°旋转孪晶,其它孪晶为这两种孪晶方式的重复与组合。随着温度的升高,孪晶逐渐减少。 关键词:  相似文献   

16.
研究了Zr65Cu17.5Ni10Al7.5合金定向凝固过程中组织形态的演变特征,探索了不同的凝固方向与重力场方向间的相互取向关系对凝固组织形态的影响.存在着一个临界抽拉速度Vfc,当抽拉速度大于该临界值时组织方向性变差.该合金本身的物理性质决定了它具有一个较小的临界值(Vfc=5mm/min).不同的凝固方向与重力场的相对取向关系改变了液-固界面前沿的浮力对流状态.当凝固方 关键词:  相似文献   

17.
采用高频熔炼后的真空单辊急冷技术制备了AgxCu50-xZr50金属玻璃,发现在x<12的范围内都可得到完全的非晶态。测量了x=2,4,6和10的AgxCu50-xZr50金属玻璃的玻璃转变温度和晶化温度,并采用Kissinger方法测定了晶化激活能Ea。发现在金属玻璃AgxCu50-xZr50关键词:  相似文献   

18.
The influence of uniaxial compression on the propagation of sound in Zr52.5Ti5Cu17.9Ni14.6Al10 and Pd40Cu30Ni10P20 bulk metallic glasses is investigated, and the third-order elastic moduli of these glasses are determined. __________ Translated from Fizika Tverdogo Tela, Vol. 47, No. 3, 2005, pp. 395–399. Original Russian Text Copyright ? 2005 by Kobelev, Kolyvanov, Khonik.  相似文献   

19.
Magnetic properties of amorphous and nanocrystalline Fe31Ni50Zr7B12, Fe31Ni40Co10Zr7B12 and Fe31Ni30Co20Zr7B12 alloys were studied by an unconventional “rf-Mössbauer” technique. Introduction of Co atoms into FeNiZrB alloy leads to a large increase of anisotropy field that suppresses the rf collapse effect. The rf induced crystallization effect observed in Co-containing alloys was attributed to the rf sidebands effect which induced in the alloys mechanical deformations via the magnetostriction. This effect is particularly strong in amorphous alloys and in nanocrystalline alloys containing significant fraction of amorphous matrix and is absent in Co-free alloy.  相似文献   

20.
Fe75Co6Zr9B10 amorphous alloy prepared by melt-spinning was annealed at various temperatures. The crystallization behavior and microstructure were investigated by differential thermal analysis (DTA), X-ray diffraction (XRD), transmission electron microscopy (TEM) and atomic force microscopy (AFM). The three exothermal peaks in the DTA curve of Fe75Co6Zr9B10 amorphous alloy correspond to the formations of α-Fe and α-Mn type phases, the growth of BCC-Fe volume fraction at the expense of α-Mn and residual amorphous phase and the precipitations of Fe3Zr, etc. intermetallic compounds, respectively. The second exothermic peak is not influenced by heating rate, but it shifts to a higher temperature region with increasing preannealing temperature of Fe75Co6Zr9B10 alloy. The α-Mn type phase is metastable and its lattice parameter determined by TEM is 0.8830 nm. AFM images show the development of surface morphology of alloy after annealing. The particle size increases with increasing annealing temperature.  相似文献   