首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 15 毫秒
1.
A series of well‐defined amphiphilic diblock copolymers consisting of hydrophobic polyisobutylene (PIB) and hydrophilic poly(2‐(diethylamino)ethyl methacrylate) (PDEAEMA) segments was synthesized via the combination of living carbocationic polymerization and reversible addition fragmentation chain transfer (RAFT) polymerization. Living carbocationic polymerization of isobutylene followed by end‐capping with 1,3‐butadiene was first performed at ?70 °C to give a well‐defined allyl‐Cl‐terminated PIB with a low polydispersity (Mw/Mn =1.29). This end‐functionalized PIB was further converted to a macromolecular chain transfer agent for mediating RAFT block copolymerization of 2‐(diethylamino)ethyl methacrylate at 60 °C in tetrahydrofuran to afford the target well‐defined PIB‐b‐PDEAEMA diblock copolymers with narrow molecular weight distributions (Mw/Mn ≤1.22). The self‐assembly behavior of these amphiphilic diblock copolymers in aqueous media was investigated by fluorescence spectroscopy and transmission electron microscope, and furthermore, their pH‐responsive behavior was studied by UV‐vis and dynamic light scattering. © 2014 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2014 , 52, 1478–1486  相似文献   

2.
Polyisobutylene‐b‐poly(N,N‐diethylacrylamide) (PIB‐b‐PDEAAm) well‐defined amphiphilic diblock copolymers were synthesized by sequential living carbocationic polymerization and reversible addition‐fragmentation chain transfer (RAFT) polymerization. The hydrophobic polyisobutylene segment was first built by living carbocationic polymerization of isobutylene at ?70 ° C followed by multistep transformations to give a well‐defined (Mw/Mn = 1.22) macromolecular chain transfer agent, PIB‐CTA. The hydrophilic poly(N,N‐diethylacrylamide) block was constructed by PIB‐CTA mediated RAFT polymerization of N,N‐diethylacrylamide at 60 ° C to afford the desired well‐defined PIB‐b‐PDEAAm diblock copolymers with narrow molecular weight distributions (Mw/Mn ≤1.26). Fluorescence spectroscopy, transmission electron microscope, and dynamic light scattering (DLS) were employed to investigate the self‐assembly behavior of PIB‐b‐PDEAAm amphiphilic diblock copolymers in aqueous media. These diblock copolymers also exhibited thermo‐responsive phase behavior, which was confirmed by UV‐Vis and DLS measurements. © 2015 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2015 , 53, 1143–1150  相似文献   

3.
Novel segmented polyurea elastomers containing soft polyisobutylene (PIB) segments were synthesized and characterized. The key ingredient, primary amine‐telechelic PIB oligomers (NH2‐PIB‐NH2) with number average molecular weights of 2500 and 6200 g/mol were synthesized. PIB‐based polyureas were prepared by using various aliphatic diisocyanates and diamine chain extenders with hard segment contents between 9.5 and 46.5% by weight. All copolymers displayed microphase morphologies as determined by dynamic mechanical analysis. Tensile strengths of nonchain‐extended and chain‐extended polyureas showed a linear dependence on the urea hard segment content. PIB‐based polyureas prepared with NH2‐PIB‐NH2 of Mn = 2500 g/mol, 4,4′‐methylendbis(cyclohexylisocyantate), and 1,6‐diaminohexane containing 45% hard segment exhibited 19.5 MPa tensile strength which rose to 23 MPa upon annealing at 150 °C for 12 h. With increasing hard segment content, elongation at break decreased from ~ 450% to a plateau of 110%. The hydrolytic and oxidative stability of PIB‐based polyureas were unprecedented. Although commercial “oxidatively resistant” thermoplastic polyurethanes degraded severely upon exposure to boiling water or concentrated nitric acid, the experimental polyureas survived without much degradation in properties. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 38–48, 2009  相似文献   

4.
In this study, the diffusion behavior of methyl ethyl ketone (MEK)/toluene mixtures, with MEK molar fractions (x1) in the liquid source lower than 0.2, in polyisobutylene (PIB) was investigated with vapor‐sorption Fourier transform infrared attenuated total reflectance (FTIR‐ATR) spectroscopy. FTIR‐ATR Fickian diffusion models for both binary and ternary systems were used to determine diffusion coefficients. Obtained diffusion coefficients for MEK from the binary diffusion model did not agree with those determined previously for the diffusion of MEK/toluene mixtures, with x1 > 0.2, in PIB. When the ternary diffusion model was used, the main‐term and cross‐term diffusion coefficients of MEK were comparable. © 2001 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 39: 908–914, 2001  相似文献   

5.
We present the synthesis of nonsymmetric α‐ω‐functionalized polyisobutylenes (PIBs) bearing different functional moieties on their chain ends. Thus, on one chain end either, a short tri‐ethylene oxide chain (TEO) or a phosphine oxide ligand is attached, whereas the other chain end is substituted by hydrogen bonding moieties (thymine/2,6‐diaminotriazine). The nonsymmetric PIBs were synthesized via living cationic polymerization using methyl‐styrene epoxide as initiator, followed by quenching reaction with 3‐bromopropyl‐benzene. Subsequent bromide/azide exchange and the use of the azide/alkyne click reaction allowed the synthesis of (a) (α)‐TEO‐(ω)‐thymine‐telechelic PIB ( 7a ), (b) (α)‐triethyleneoxide‐(ω)‐triazine telechelic PIB ( 7b ), and (c) (α)‐phosphinoxide‐(ω)‐thymine‐telechelic PIB ( 13 ) with molecular weights Mn ~ 4000 g mol?1 and low polydispersities (Mw/Mn = 1.3). The chemical identity of the final structures was proven by extensive 1H NMR investigations and matrix‐assisted laser desorption/ionization‐mass spectroscopy (MALDI). The presented method for the first time offers a simple and highly versatile approach toward supramolecular nonsymmetric α‐ω‐functionalized PIB. © 2011 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2011  相似文献   

6.
The controlled cationic polymerization of isobutylene (IB) initiated by H2O as initiator and TiCl4 as coinitiator was carried out in n‐Hexane/CH2Cl2 (60/40, v/v) mixture at −40 °C in the presence of N,N‐dimethylacetamide (DMA). Polyisobutylene (PIB) with nearly theoretical molecular weight (Mn = 1.0 × 104 g/mol), polydispersity (Mw/Mn) of 1.5 and high content (87.3%) of reactive end groups (tert‐Chlorine and α‐double bond) was obtained. The Friedel‐Crafts alkylation of triphenylamine (TPA) with the above reactive PIB was further conducted at different reactions, such as [TPA]/[PIB], solvent polarity, alkylation temperature, and time. The resultant PIBs with arylamino terminal group were characterized by 1H NMR, UV, and GPC with RI/UV dual detectors. The experimental results indicate that alkylation efficiency (Aeff) increased with increases in [TPA]/[PIB], reaction temperature, and reaction time and with a decrease in solvent polarity. The alkylation efficiency could reach 81.0% at 60/40(v/v) mixture of n‐Hex/CH2Cl2 with [TPA]/[PIB] of 4.49 at 50 °C for 54 h. Interestingly, the synthesis of PIB with arylamino terminal group could also be achieved in one pot by combination of the cationic polymerization of IB initiated by H2O/TiCl4/DMA system with the successive alkylation by further introduction of TPA. Mono‐, di‐ or tri‐alkylation occurred experimentally with different molar ratio of [TPA]/[PIB]. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 936–946, 2008  相似文献   

7.
The dynamic mechanical loss tangent (tan δ) peak of polyisobutylene (PIB) reveals an asymmetrical broad structure with a maximum on the high‐temperature side and a shoulder on the low‐temperature side. By comparing with the literature results, it is suggested that the shoulder and the maximum originate from local segmental motion and Rouse modes, respectively. Blending polystyrene (PS) with PIB has two effects on the relaxation behavior of PIB. One effect is that the maximum and the shoulder are both suppressed, but the maximum is suppressed to a higher extent. After PS forms the continuous phase, the maximum becomes lower than the shoulder, and even almost disappears when the weight ratio of PIB/PS is under 20/80. The other effect is that, before PS forms the continuous phase, the temperature position of the maximum (Ts) and that of the shoulder (Tα) remains constant, but after PS forms the continuous phase, both of them are reduced with decreasing particle size of the PIB phase, in a way similar to nano‐confinement effect on the depression of glass transition temperature. The depression amplitude of Ts is larger than that of Tα. The aforementioned two effects can be interpreted in terms of the limited expansion of free volume of the PIB phase exerted by the PS phase, which affects the maximum to a higher extent than the shoulder because Rouse modes are more sensitive to the free volume than local segments. © 2010 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys, 2010  相似文献   

8.
The syntheses of {‐poly(L ‐lactide) (PLLA)‐b‐polyisobutylene (PIB)‐}n multiblock copolymers were accomplished for the first time by chain extension of PLLA‐b‐PIB‐b‐PLLA triblock copolymers. Well‐defined PLLA‐b‐PIB‐b‐PLLA triblock copolymers with predictable Mns, low PDIs (1.10–1.18) and excellent blocking efficiencies were prepared by anionic ring‐opening polymerizations of L ‐lactide initiated with hydroxyallyl telechelic PIB (HO‐Allyl‐PIB‐Allyl‐OH) in toluene at 110 °C. The triblock copolymers were successfully chain extended with 4,4′‐methylenebis(phenylisocyanate) (MDI) to obtain the multiblock copolymers with good gravimetric yields of ~86 to 96%. The chain‐extended polymers were soluble in a range of common organic solvents. The block copolymers showed two glass transition temperatures in differential scanning calorimetric analysis for the PIB and PLLA blocks indicating microphase separation, which was supported by atomic force microscopy images. The as‐synthesized compression molded multiblock copolymers exhibited tensile strengths in the range of 8–24 MPa with elongations at break in the range of 2.5–400%. The static and dynamic mechanical properties showed a strong dependence on the relative PLLA content in the copolymer. The dynamic mechanical analysis also indicated microphase separation at higher PLLA compositions. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 3490–3505, 2009  相似文献   

9.
tert-Chloride-terminated polyisobutylenes (PIB) (1020 ≤ Mn ≤ 6700 g/mol) were dehydrochlorinated nonregiospecifically using basic alumina, or regiospecifically either via potassium tert-butoxide or in situ quenching of quasiliving PIB. Olefin-terminated PIBs were quantitatively ozonized at −78 °C using hexane/methylene chloride/methanol, 62/31/7 (v/v/v) cosolvents, and an ozone generator, employing pure oxygen as source gas. The primary ozonides were reduced using trimethyl phosphite to yield pure PIB methyl ketone from exo-olefin PIB, and a mixture of PIB methyl ketone and PIB aldehyde from mixed olefin-PIB. PIB methyl ketone was oxidized to carboxylate via the haloform reaction; titration revealed near-quantitative functionalization, but the reaction was slow. Tetrahalomethane oxidation was identified as a preferred alternative method, and was conducted using either CCl4 as the reaction solvent, THF as the solvent with CCl4 in reagent amounts, or hexane as the solvent with a phase-transfer catalyst and CCl4 in reagent amounts. The system using hexane, with tetra-n-butyl ammonium chloride as phase-transfer catalyst, showed complete conversion in ∼ 4 h. PIB carboxylic acid was recovered by acidification and isolation. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 3229–3240, 2008  相似文献   

10.
The relaxation behaviors of poly(dimethylsiloxane‐co‐diphenylsiloxane)s with different compositions were investigated using dynamic mechanical analysis (DMA) and differential scanning calorimetry (DSC). It is indicated that the content of Ph2SiO unit, which is closely associated with crystallinity of polysiloxane, has a remarkable influence on its relaxation behavior. Two‐phase (crystalline and amorphous phase) structure in the semicrystalline polysiloxane of the present system can be determined for discussing relaxation behavior. An increase in relaxation strength can be reasoned to a cooperative effect of decrease in fraction of crystalline phase and increase in friction between molecular chains. And enhancements in glass transition temperature (Tg) and effective activation energy for glass transition (Ea(eff)) were ascribed more to the stiffness imposed by Ph2SiO unit than decrease in fraction of crystalline phase. © 2008 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 46: 1652–1659, 2008  相似文献   

11.
The hydrolytic degradation of a series of poly‐L ‐lactide (PLLA)‐polyisobutylene (PIB) multiblock copolymers was studied in phosphate buffer solution (pH = 7.4) at 37 °C. The multiblock copolymers were synthesized by chain extension of PLLA‐b‐PIB‐b‐PLLA triblock copolymers, which were obtained by ring‐opening polymerization of L ‐lactide initiated by hydroxyallyl telechelic PIB. The degradation strongly depended on the PLLA segment length. At constant PIB segment length, the multiblock copolymer with the shortest PLLA segment length (DPn = 10), showed significant weight loss after 8 weeks, whereas weight loss for DPn = 36 was only observed after 24 weeks. The gel‐permeation chromatographic analysis showed a similar decrease in the number‐average molecular weight (Mn) with time further supporting the weight loss data. Dynamic mechanical analysis showed a decrease in ultimate stress and modulus with time. The crystallinity of multiblock copolymers changed significantly with degradation time as indicated from differential scanning calorimetric analysis. © 2010 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 48: 3767–3774, 2010  相似文献   

12.
The synthesis of novel arborescent (arb; randomly branched, “tree‐like,” and often called “hyperbranched”) block copolymers comprised of rubbery polyisobutylene (PIB) and glassy polystyrene (PSt) blocks (arb‐PIB‐b‐PSt) is described. The syntheses were accomplished by the use of arb‐PIB macroinitiators (prepared by the use of 4‐(2‐methoxyisopropyl) styrene inimer) in conjunction with titanium tetrachloride (TiCl4). The effect of reaction conditions on blocking of St from arb‐PIB was investigated. Purified block copolymers were characterized by 1H NMR spectroscopy and Size Exclusion Chromatography (SEC). arb‐PIB‐b‐PSt with 11.7–33.8 wt % PSt and Mn = 468,800–652,900 g/mol displayed thermoplastic elastomeric properties with 3.6–8.7 MPa tensile strength and 950–1830% elongation. Samples with 26.8–33.8 wt % PSt were further characterized by Atomic Force Microscopy (AFM), which showed phase‐separated mixed spherical/cylindrical/lamellar PSt phases irregularly distributed within the continuous PIB phase. Dynamic Mechanical Thermal Analysis (DMTA) and solvent swelling of arb‐PIB‐b‐PSt revealed unique characteristics, in comparison with a semicommercial PSt‐b‐PIB‐b‐PSt block copolymer. The number of aromatic branching points of the arb‐PIB macroinitiator, determined by selective destruction of the linking sites, agreed well with that calculated from equilibrium swelling data of arb‐PIB‐b‐PSt. This method for the quantitative determination of branching sites might be generally applicable for arborescent polymers. © 2005 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 43: 1811–1826, 2005  相似文献   

13.
The phase behavior of (PS‐PIB)2s‐PAA miktoarm star terpolymers with varying volume fractions of PAA was investigated directly by transmission electron microscopy, atomic force microscopy, and small‐angle X‐ray scattering, and indirectly by thermogravimetric analysis and degree of water sorption. The microdomains of (PS‐PIB)2s‐PAA demonstrate a unique and unexpected progression from highly ordered cylinders, to lower ordered spheres, to gyroid structures with increasing PAA content from 6.6 to 47 wt %. Interestingly, the phase behavior in the miktoarm star polymer system is significantly different from that reported previously for the linear counterpart of similar composition (PAA‐PS‐PIB‐PS‐PAA), where a steady progression from cylindrical to lamellar morphology was observed with increasing PAA content. At low PAA concentrations, the morphology is driven primarily by the relative solubility of the components, while at high PAA content the molecular architecture dominates. Thermal annealing demonstrated the thermodynamic stability of the morphologies, indicating the potential for design of novel microstructures for specific applications through precise control of architecture, composition, and interaction parameters of the components. © 2016 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2016 , 54, 916–925  相似文献   

14.
We discovered that polyisobutylene (PIB)‐based polyurethanes (PIB‐PUs) containing minute amounts (0.5%) of chemically bound organically modified montmorillonite (OmMMT) surprisingly produce films exhibiting improved properties. The OmMMT was prepared by reacting sodium montmorillonite (Na+MMT?) with quaternary ammonium salts of a tertiary amine carrying a ? NH2 functionality. The positively charged quaternary amine group becomes electrostatically attached to negatively charged MMT layers and defoliates it, whereas the free ? NH2 group reacts with diisocyanates and acts as an additional chain extender. Thus, when OmMMT is added to a mixture of ingredients assembled for the synthesis of PIB‐PUs, this modified clay becomes an integral part of the PU. Specifically, we found that the integration of 0.5% OmMMT to PIB‐based PUs produces films with significantly enhanced tensile strength, elongation, toughness, creep, and stress relaxation relative to that of PIB‐PUs. The findings were discussed and explained in terms of a proposed morphology for the nanocomposite. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2013 , 51, 4076–4087  相似文献   

15.
Two structurally closely related three‐arm star blocks were synthesized and characterized: tCum(PIB‐b‐PNBD)3 and tCum(PNBD‐b‐PIB)3 [where tCum (tricumyl) stands for the phenyl‐1,3,5‐tris(‐2‐propyl) fragment and PIB and PNBD are polyisobutylene and polynorbornadiene, respectively]. The syntheses were accomplished in two stages: (1) the preparation of the first (or inner) block fitted with appropriate chlorine termini capable of initiating the polymerization of the second (or outer) block with TiCl4 and (2) the mediation of the polymerization of the second block. Therefore, the synthesis of tCum(PIB‐b‐PNBD)3 was effected with tCum(PIB‐Clt)3 [where Clt is tert‐chlorine and number‐average molecular weight (Mn) = 102,000 g/mol] by the use of TiCl4 and 30/70 CH3Cl/CHCl3 solvent mixtures at ?35 °C. PNBD homopolymer contamination formed by chain transfer was removed by selective precipitation. According to gel permeation chromatography, the Mn's of the star blocks were 107,300–109,200 g/mol. NMR spectroscopy (750 MHz) was used to determine structures and molecular weights. Differential scanning calorimetry (DSC) indicated two glass‐transition temperatures (Tg's), one each for the PIB (?65 °C) and PNBD (232 °C) phases. Thermogravimetric analysis thermograms showed 5% weight losses at 293 °C in air and at 352 °C in N2. The synthesis of tCum(PNBD‐b‐PIB)3 was achieved by the initiation of isobutylene polymerization with tCum(PNBD‐Clsec)3 (where Clsec is sec‐chlorine and Mn = 2900 g/mol) by the use of TiCl4 in CH3Cl at ?60 °C. DSC for this star block (Mn = 14,200 g/mol) also showed two Tg's, that is, at ?67 and 228 °C for the PIB and PNBD segments, respectively. It is of interest that the Clsec terminus of PNBD, , readily initiated isobutylene polymerization. © 2003 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 41: 740–751, 2003  相似文献   

16.
Novel rubbery wound closures containing various proportions and molecular weights of polyisobutylene (PIB) and poly(2‐octyl cyanoacrylate) [P(OctCA)] for potential clinical use were designed, synthesized, characterized, and tested. Homo‐networks were prepared by crosslinking 3‐arm star‐shaped PIBs fitted with terminal cyanoacrylate groups, [Ø(PIB‐CA)3], and co‐networks by copolymerizing Ø(PIB‐CA)3 with OctCA using N‐dimethyl‐p‐toluidine (DMT). Neat Ø(PIB‐CA)3, and Ø(PIB‐CA)3/OctCA blends, upon contact with initiator, polymerize within seconds to optically transparent strong rubbery co‐networks, Ø(PIB‐CA)3co‐P(OctCA). Homo‐ and co‐network formation was demonstrated by sol/gel studies, and structures and properties were characterized by a battery of techniques. The Tg of P(OctCA) is 58 °C by DSC, and 75 °C by DMTA. Co‐networks comprising 25% Ø(PIB‐CA)3 (Mn = 2400 g/mol) and 75% P(OctCA) are stronger and more extensible than skin. Short and long term creep studies show co‐networks exhibit high dimensional stability and <6% creep strain at high loading. When deposited on porcine skin co‐networks yield hermetically‐adhering clear rubbery coatings. Strips of porcine skin coated with co‐networks could be stretched and twisted without compromising membrane integrity. The co‐network is nontoxic to L‐929 mouse fibroblasts. © 2015 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2015 , 53, 1640–1651  相似文献   

17.
In current tube models for entanglement, the tube representing the topological constraint is considered to move with time. This tube motion results in the constraint release (CR) as well as the dynamic tube dilation (DTD), and an importance of DTD has been argued for entangled star chains. Under these backgrounds, this article examines the validity of the DTD molecular picture for the star chains. For monodisperse star chains having noninverted type‐A (parallel) dipoles in respective arms, the normalized viscoelastic and dielectric relaxation functions μ(t) and Φ(t) were found to obey a relationship μ(t) ≅ [Φ(t)]2 if the tube actually dilates in the time scale of the star relaxation. For 6‐arm star cis‐polyisoprene (PI) chains (having those type‐A dipoles), dielectric and viscoelastic measurements were conducted to test this DTD relationship. Both viscoelastic and dielectric properties exhibited characteristic behavior expected from DTD models (assuming the arm retraction in the dilating tube), the exponential increase of the relaxation time and broadening of the relaxation mode distribution with increasing arm molecular weight Ma. However, in the range of Ma examined, Ma ≤ 8Me (Me = entanglement spacing), the above DTD relationship was not valid for a dominant part of the slow relaxation (and the models failed in this sense). Thus, for star chains at least in this range of Ma, the simple DTD picture assuming very rapid CR motion (rapid equilibration in the dilated tube) did not explain the slow relaxation behavior of star chains. This result in turn suggested the importance of the CR motion in this behavior. © 2000 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 38: 1024–1036, 2000  相似文献   

18.
Multiarm star‐branched polymers based on poly(styrene‐b‐isobutylene) (PS‐PIB) block copolymer arms were synthesized under controlled/living cationic polymerization conditions using the 2‐chloro‐2‐propylbenzene (CCl)/TiCl4/pyridine (Py) initiating system and divinylbenzene (DVB) as gel‐core‐forming comonomer. To optimize the timing of isobutylene (IB) addition to living PS⊕, the kinetics of styrene (St) polymerization at −80°C were measured in both 60 : 40 (v : v) methyl cyclohexane (MCHx) : MeCl and 60 : 40 hexane : MeCl cosolvents. For either cosolvent system, it was found that the polymerizations followed first‐order kinetics with respect to the monomer and the number of actively growing chains remained invariant. The rate of polymerization was slower in MCHx : MeCl (kapp = 2.5 × 10−3 s−1) compared with hexane : MeCl (kapp = 5.6 × 10−3 s−1) ([CCl]o = [TiCl4]/15 = 3.64 × 10−3M; [Py] = 4 × 10−3M; [St]o = 0.35M). Intermolecular alkylation reactions were observed at [St]o = 0.93M but could be suppressed by avoiding very high St conversion and by setting [St]o ≤ 0.35M. For St polymerization, kapp = 1.1 × 10−3 s−1 ([CCl]o = [TiCl4]/15 = 1.82 × 10−3M; [Py] = 4 × 10−3M; [St]o = 0.35M); this was significantly higher than that observed for IB polymerization (kapp = 3.0 × 10−4 s−1; [CCl]o = [Py] = [TiCl4]/15 = 1.86 × 10−3M; [IB]o = 1.0M). Blocking efficiencies were higher in hexane : MeCl compared with MCHx : MeCl cosolvent system. Star formation was faster with PS‐PIB arms compared with PIB homopolymer arms under similar conditions. Using [DVB] = 5.6 × 10−2M = 10 times chain end concentration, 92% of PS‐PIB arms (Mn,PS = 2600 and Mn,PIB = 13,400 g/mol) were linked within 1 h at −80°C with negligible star–star coupling. It was difficult to achieve complete linking of all the arms prior to the onset of star–star coupling. Apparently, the presence of the St block allows the PS‐PIB block copolymer arms to be incorporated into growing star polymers by an additional mechanism, namely, electrophilic aromatic substitution (EAS), which leads to increased rates of star formation and greater tendency toward star–star coupling. © 1999 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 37: 1629–1641, 1999  相似文献   

19.
Allyl‐telechelic polyisobutylene (A‐PIB‐A) produced by the bis‐benzocyclobutane dichloride (bBCB‐diCl) initiator contains the bis‐benzocyclobutane (bBCB) fragment at the center of the macromolecule (A‐PIB‐bBCB‐PIB‐A). Thermolysis of A‐PIB‐bBCB‐PIB‐A quantitatively converts the central bBCB fragment to a substituted conjugated tetraene (A‐PIB‐tetraene‐PIB‐A). The structure of A‐PIB‐tetraene‐PIB‐A was anticipated from small molecule models and identified/quantitated by 1H NMR spectroscopy. This is the first time a reactive functional group was introduced at the statistical center of a (telechelic) PIB. Subsequently, the A‐PIB‐tetraene‐PIB‐A was peroxidized to an epoxy derivative. Reaction of the A‐PIB‐tetraene‐PIB‐A with HSCH2CH2OH produced HOCH2‐telechelic PIB containing a central  CH2OH function, and hydrosilation with HSi(Me2)‐O‐Si(Me2)H produced SiH‐telechelic PIB with a central  SiH function. Reactions with maleic anhydride, tetracyanoethylene, butyl lithium, and potassium permanganate have also been examined. In sum, A‐PIB‐bBCB‐PIB‐A and A‐PIB‐tetraene‐PIB‐A are useful intermediates for the synthesis of novel PIB‐based materials for various end uses under investigation. © 2018 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2018 , 56, 1140–1145  相似文献   

20.
The interaction between poly(acrylic acid) polymers (PAA) of low‐ (2000 g/mol) and high‐ (450,000 g/mol) molecular weight (Mw) hydrophobically modified with pyrene (PAAMePy) and β‐ and γ‐cyclodextrins (β‐CD, γ‐CD) was investigated with fluorescent techniques. The interaction with β‐CD promotes little variation in the spectral and photophysical behavior of the polymer, whereas significant changes are observed upon addition of γ‐CD. The degree of inclusion (between the pyrene groups of the polymer and the cyclodextrins) is followed through the observation of the changes in the absorption, excitation (collected in the monomer and excimer emission regions) and emission (IE/IM ratio) spectra and from time‐resolved data. Within the studied range of γ‐CD concentration, the fluorescence decays of the long chain (high Mw) PAAMePy polymers were found tri‐exponential in the monomer and excimer emission regions in agreement with previous studies. In the case of the low Mw PAAMePy polymers, tri‐exponential decays were observed at the monomer and excimer emission wavelengths. However, when a γ‐CD concentration of 0.01 and 0.03 M is reached for, respectively, the low‐ and high‐labeled pyrene short chain (low Mw) polymers, the fluorescence decays in the excimer region become biexponential (two excimers) with no rising component, thus showing that all pyrene groups are encapsulated (and preassociated) into the γ‐CD cavity. In the case of the high Mw polymers, the addition of γ‐CD has been found to change the level of polymer interaction from pure intramolecular (water in the absence of cyclodextrin) to a coexistence of intra‐ with intermolecular interactions. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 1402–1415, 2008  相似文献   