1.
Photoirradiation surface molecularly imprinted polymers for the separation of 6‐O‐α‐d ‐maltosyl‐β‐cyclodextrin were synthesized using functionalized silica as a matrix, 4‐(phenyldiazenyl)phenol as a light‐sensitive monomer, and 6‐O‐α‐d ‐maltosyl‐β‐cyclodextrin as a template. Fourier transform infrared spectroscopy results indicated that 4‐(phenyldiazenyl)phenol was grafted onto the surface of functionalized silica. The obtained imprinted polymers exhibited specific recognition toward 6‐O‐α‐d ‐maltosyl‐β‐cyclodextrin. Equilibrium binding experiments showed that the photoirradiation surface molecularly imprinted polymers obtained the maximum adsorption amount of 6‐O‐α‐d ‐maltosyl‐β‐cyclodextrin at 20.5 mg/g. In binding kinetic experiments, the adsorption reached saturation within 2 h with binding capacity of 72.8%. The experimental results showed that the adsorption capacity and selectivity of imprinted polymers were effective for the separation of 6‐O‐α‐d ‐maltosyl‐β‐cyclodextrin, indicating that imprinted polymers could be used to isolate 6‐O‐α‐d ‐maltosyl‐β‐cyclodextrin from a conversion mixture containing β‐cyclodextrin and maltose. The results showed that the imprinted polymers prepared by this method were very promising for the selective separation of 6‐O‐α‐d ‐maltosyl‐β‐cyclodextrin.  相似文献   

2.
Novel skipped‐π polymers in which the π‐components are connected with 2‐substituted trimethylene tethering units exhibit bathochromically shifted, broadened ultraviolet absorption with a unique lower‐energy absorption band and a largely red‐shifted fluorescent emission. These results suggest that through‐space π–π interactions owing to a stair‐like stacking substructure in these polymers extend the π‐conjugation of the components in the ground and excited states. As the photophysical properties of the polymers observed both in a solution and in a dried film are similar to those of the J‐aggregates of π‐molecules, these polymers may be considered as pseudo J‐stacking (or J‐like‐stacking) polymers. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2013 , 51, 3412–3419  相似文献   

3.
Two series of polyimides based on laterally attached p‐terphenyl and biphenyl groups were synthesized. The solubility and thermal properties were studied using DSC, thermogravimetric analysis, and the solubility test. These polymers exhibited good thermal stability and excellent solubility. The high solubility for both polymer series was attributed to the non‐coplanarity of diamine monomers and the use of fluorinated dianhydride, whereas the slightly better solubility for polymers based on p‐terphenyl was attributed to further weakening of interchain interaction of the polymers. Both polymer series exhibited glass‐transition temperatures (Tg's) in the range of 244–272 °C. The Tg's of polymers containing laterally attached p‐terphenyls were higher than those of their counterparts containing biphenyls by 5–17 °C. This was attributed to the formation of an interdigitated structure that hinders the segmental movement of polymer chains. © 2001 John Wiley & Sons, Inc. J Polym Sci Part A: Polym Chem 39: 2998–3007, 2001  相似文献   

4.
4‐Tolyldiphenylamine (TDPA) and N,N′‐diphenyl‐N,N′‐bis(4‐methylphenyl)‐1,1′‐biphenyl‐4,4′‐diamine (TPD), were reacted with benzaldehyde (BA) using p‐toluenesulfonic acid as a catalyst to yield linear polymers. The polymers were reacted with 2,3‐dichloro‐5,6‐dicyano‐1,4‐benzoquinone (DDQ) in tetrahydrofuran (THF) at room temperature. 1H‐NMR showed that all the methine protons in the residue of BA were completely removed at the mole ratio of repeating unit : DDQ, 2 : 1. The resulting polymers showed good solubility in chloroform or THF. The reacted TDPA‐BA and TPD‐BA polymers gave new UV absorption peaks at 697.0 and 722.5 nm and showed reversible redox potentials about 0.994 and 1.021 V, respectively. Direct current (d.c.) conductivity of the reacted polymers was in the range of 10?11 S/cm, which is more than two orders higher than the unreacted polymers. The polymer showed pentad split electron spin resonance (ESR) signal, whose concentration was one in 670 or 230 repeating unit for TDPA‐BA and TPD‐BA polymers, respectively. Copyright © 2001 John Wiley & Sons, Ltd.  相似文献   

5.
Novel conjugated polymers composed of benzo[1,2‐b:4,5‐b′]dithiophene and thieno[3,4‐b]pyrazine or dithieno[3′,2′:3,4;2″,3″:5,6]benzo[1,2‐d]imidazole units are synthesized by Stille polycondensation. The resulting polymers display a longer wavelength absorption and well‐defined redox activities. The effective intramolecular charge‐transfer and energy levels of all polymers are elucidated by computational calculations. Bulk‐heterojunction solar cells based on these polymers as p‐type semiconductors and [6,6]‐phenyl‐C61‐butyric acid methyl ester (PC61BM) as an n‐type semiconductor are fabricated, and their photovoltaic performances are for the first time evaluated. © 2015 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2015 , 53, 1067–1075  相似文献   

6.
A series of new low band gap π‐conjugated polymers containing N‐alkyldithieno[3,2‐b:2′,3′‐d]pyrrole, benzo[c][1,2,5]thiadiazole, and alkylthiophenes are reported. The polymerization condition was standardized and the use of CuO to obtain high‐molecular‐weight polymer was also realized. The molecular weight of the polymers was found to be in the range of 45,000–53,000. All the polymers were found to be soluble in most of the common organic solvents, such as chloroform, dichloromethane, THF, and chlorobenzene with excellent film forming properties. The λmax of the polymers was found to be in the range of 687–663 nm with band gap in the range of 1.35–1.43 eV. The oxidation potential of the polymers from cyclic voltammetry was determined to be 0.5–0.75 V. The HOMO levels of the above synthesized polymers were found to be between 5.24 and 5.54 eV. All the polymers exhibited a PL emission in between 755 and 773 nm. The polymers were found to be thermally stable above 277 °C with only a 5% weight loss. From the thermal stability values, it is expected that the current set of polymers are stable enough for the application in electronic devices. To realize the potential use of the polymers, EL devices were fabricated and found to show red emission with comparatively low threshold voltage. A brightness of 54 cd m−2 for the device with polymer PC could be reached. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 6514–6525, 2009  相似文献   

7.
A new dicarboxylic acid monomer, 1,1‐bis[4‐(4‐carboxyphenoxy)phenyl]‐4‐tert‐butylcyclohexane, bearing a pendent tert‐butylcyclohexylidene group was prepared in three steps from 4‐tert‐butylcyclohexanone. The monomer was reacted with various diamines to produce a series of new polyamides with triphenyl phosphite and pyridine as condensing agents. These polyamides were produced with inherent viscosities of 0.74 to 1.02 dL g−1. All the polymers were characterized by X‐ray diffraction that revealed this amorphous nature. These polymers exhibited excellent solubility in a variety of solvents. Almost all the polymers could be dissolved in N‐methyl‐2‐pyrrolidinone, N,N‐dimethylacetamide (DMAc), N,N‐dimethylformamide, dimethyl sulfoxide, pyridine, and even in tetrahydrofuran and cyclohexanone. These polymers showed glass‐transition temperatures between 223 and 256 °C and decomposition temperatures at 10% weight loss ranging from 468 to 491 °C and 469 to 498 °C in nitrogen and air atmospheres, respectively. Transparent, tough, and flexible films of these polymers were cast from the DMAc solutions. These polymer films had tensile strengths ranging from 76 to 99 MPa, elongations at break from 7 to 19%, and initial moduli from 2.1 to 2.7 GPa. © 2000 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 38: 797–803, 2000  相似文献   

8.
A series of poly[ω‐(4′‐methoxy‐biphenyl‐4‐oxy)alkyl‐1‐glycidylether]s were synthesized by chemically modifying the corresponding poly(ω‐bromoalkyl‐1‐glycidylether)s with the sodium salt of 4‐hydroxy‐4′‐methoxybiphenyl. New high‐molecular‐weight side‐chain liquid‐crystalline polymers were obtained with excellent yields and almost quantitative degrees of modification. They were all insoluble in THF and other common solvents. Characterization by 13C NMR confirmed that all the polymers had the expected structure. The liquid crystalline behavior of the polymers was analyzed by DSC and polarized optical microscopy, and mesophase assignments were confirmed by X‐ray diffraction studies. Polymers that had alkyl spacers with n = 2 and 4 were smectic C, those that had spacers with n = 6 and 8 were nematic cybotactic, and those that had longer spacers (n = 10 and 12) were smectic C again. © 2005 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 43: 5998–6006, 2005  相似文献   

9.
Summary: Host‐guest complexes of α‐cyclodextrin (α‐CD) and methylated β‐cyclodextrin (Me‐β‐CD) with diacrylates and dimethacrylates of butan‐1,4‐diol and hexan‐1,6‐diol at varying stoichiometries were studied. The complexes were analyzed by means of 1H NMR, two‐dimensional ROESY spectroscopy and Job's curves, which clearly revealed the discriminating influence of the two hosts towards complex formation. The corresponding polymers were obtained using a redox initiator system in water. Thermal analysis and IR measurements of the polymers provided evidence for the existence of a polyrotaxane architecture.

Proposed structure of the cross‐linked polymers obtained by the redox polymerization of the Me‐β‐CD complexed monomers.  相似文献   


10.
A series of novel mesogen‐jacketed liquid‐crystal polymers, poly[2,5‐bis(4′‐alkoxyphenyl)‐styrene] (P‐n, n = 1–11), were prepared via free‐radical polymerization of newly synthesized monomers, 2,5‐bis(4′‐alkoxyphenyl)styrene (M‐n, n = 1–11). The influence of the alkoxy tail length on the liquid‐crystalline behaviors of the monomers and the polymers was investigated with differential scanning calorimetry (DSC), thermogravimetry, polarized optical microscopy (POM), and wide‐angle X‐ray diffraction (WAXD). The monomers with n = 1–4, 9, and 11 were monotropic nematic liquid crystals. All other monomers exhibited enantiotropic nematic properties. Their melting points (Tm's) decreased first as n increased to 6, after which Tm increased slightly at longer spacer lengths. The isotropic–nematic transition temperatures decreased regularly with increasing n values in an odd–even way. The glass‐transition temperatures (Tg's) of the polymers first decreased as the tail lengths increased and then leveled off when n ≥ 7. All polymers were thermally stable and entered the mesophase at a temperature above Tg. Upon further heating, no mesophase‐to‐isotropic melt transition was observed before the polymers decomposed. WAXD studies indicated that an irreversible order–order transition for the polymers with short tails (n ≤ 5) and a reversible order–order transition for those with elongated tails (n ≥ 6) occurred at a temperature much higher than Tg. However, such a transition could not be identified by POM and could be detected by DSC only on heating scans for the polymers with long tails (n ≥ 7). © 2003 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 41: 1454–1464, 2003  相似文献   

11.
A series of new polyimides containing alicyclic units and alkyloxy side chains were prepared from 9,10‐dialkyloxy‐1,2,3,4,5,6,7,8‐octahydro‐2,3,6,7‐anthracenetetracarboxylic 2,3:6,7‐dianhydrides and various aromatic diamines. Their physical properties and structures were investigated. Polymers were obtained with inherent viscosities of 0.24–0.53 dL/g. In comparison with the aromatic polyimides, most polymers were readily soluble in common organic solvent such as N‐methylpyrrolidone and m‐cresol. These polymers had glass‐transition temperatures between 111 and 296 °C depending on the structure of the repeating unit and 10% weight‐loss temperatures of 418–477 °C in nitrogen. Wide‐angle X‐ray diffractometry for as‐polymerized samples revealed very low crystallinity and layered structures, which were better developed in the polymers with longer side chains. © 2002 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 40: 1764–1774, 2002  相似文献   

12.
A series of rigid‐rod polyamides and polyimides containing p‐terphenyl or p‐quinquephenyl moieties in backbone as well as naphthyl pendent groups were synthesized from two new aromatic diamines. The polymers were characterized by inherent viscosity, elemental analysis, FT‐IR, 1H‐NMR, 13C‐NMR, X‐ray, differential scanning calorimetry (DSC), thermomechanical analysis (TMA), thermal gravimetric analysis (TGA), isothermal gravimetric analysis, and moisture absorption. All polymers were amorphous and displayed Tg values at 304–337°C. Polyamides dissolved upon heating in polar aprotic solvents containing LiCl as well as CCl3COOH, whereas polyimides were partially soluble in these solvents. No weight loss was observed up to 377–422°C in N2 and 355–397°C in air. The anaerobic char yields were 57–69% at 800°C. © 1999 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 37: 15–24, 1999  相似文献   

13.
In an effort to design efficient low‐cost polymers for use in organic photovoltaic cells the easily prepared donor–acceptor–donor triad of a either cis‐benzobisoxazole, trans‐benzobisoxazole or trans‐benzobisthiazole flanked by two thiophene rings was combined with the electron‐rich 4,8‐bis(5‐(2‐ethylhexyl)‐thien‐2‐yl)‐benzo[1,2‐b:4,5‐b′]dithiophene. The electrochemical, optical, morphological, charge transport, and photovoltaic properties of the resulting terpolymers were investigated. Although the polymers differed in the arrangement and/or nature of the chalcogens, they all had similar highest occupied molecular orbital energy levels (?5.2 to ?5.3 eV) and optical band gaps (2.1–2.2 eV). However, the lowest unoccupied molecular orbital energy levels ranged from ?3.1 to ?3.5 eV. When the polymers were used as electron donors in bulk heterojunction photovoltaic devices with PC71BM ([6,6]‐phenyl C71‐butyric acid methyl ester) as the acceptor, the trans‐benzobisoxazole polymer had the best performance with a power conversion efficiency of 2.8%. © 2015 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2016 , 54, 316–324  相似文献   

14.
We have synthesized novel σπ conjugated polymers with an alternating organosilanylene and π‐electron system, intending to utilize them for hole‐transporting materials of electroluminescent (EL) devices. 3,6‐Di(lithioethynyl)carbazoles were co‐polymerized with organodichlorosilanes to give the corresponding polymers with molecular weights of MW = 2000–5000. Another type of polymer with a thienylene unit was also synthesized by the nickel‐catalyzed reaction of the di‐Grignard reagent of 1,2‐bis[2‐(5‐bromothienyl)]tetraethyldisilane with 3,6‐dibromocarbazole, the molecular weight being Mn = 3100. The EL devices with a double‐layer system composed of tris(8‐quinolinolato)aluminum(III) and the present polymers as the emitting‐electron‐transporting and hole‐transporting layers, respectively, emit green EL with a maximum intensity of the order of 103 cd m?2. Of these, the device with the thienylene–carbazole polymers exhibited the highest luminance of 1480 cd m?2. Copyright © 2001 John Wiley & Sons, Ltd.  相似文献   

15.
A modular and facile route has been developed to synthesize functionalized 2,5‐di(thiophen‐2‐yl)‐1‐H‐arylpyrroles from readily available starting materials. These units are compatible with various polymerization conditions and are versatile building blocks for conjugated polymers. The polymers show high thermal stability and solubility in a number of solvents. Characterization of the polymers reveals a correlation between molecular packing, controllable by polymer design, and charge carrier mobility. © 2018 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2018 , 56, 1133–1139  相似文献   

16.
We have synthesized novel σ–π conjugated polymers with N,N‐bis(p‐ethynylphenyl)‐N‐(p‐tolyl)amine as the π‐unit. The electroluminescent devices, with a double‐layer system composed of Alq and the present polymers as the emitting‐electron‐transporting and hole‐transporting layers respectively, emit green electroluminescence with a maximum intensity of 760 cd m?2. Copyright © 2001 John Wiley & Sons, Ltd.  相似文献   

17.
(2→5)‐1,4‐Anhydro‐3‐O‐methyl‐pentitol, which is a novel carbohydrate polymer without an anomeric linkage, was synthesized by cationic cyclopolymerization of 1,2 : 4,5‐dianhydro‐3‐O‐methyl‐xylitol. When BF3·OEt2 was used as the initiator, soluble polymers were obtained in 28 to 50% yield. These polymers have number‐average molecular weights of 1 150 to 2 340 corresponding to an average degree of polymerization of 8.8 to 18.0. It was confirmed by 13C NMR that the resulting polymer mainly consists of 1,4‐anhydro‐3‐O‐methyl‐D L ‐arabinitol units.  相似文献   

18.
The synthesis, characterization, and ring‐opening polymerization of a new cyclic carbonate monomer containing an allyl ester moiety, 5‐methyl‐5‐allyloxycarbonyl‐1,3‐dioxan‐2‐one (MAC), was performed for the first time. MAC was synthesized in five steps in good yield beginning from the starting material, 2,2‐bis(hydroxymethyl)propionic acid. Subsequent polymerization and copolymerizations of the new cyclic carbonate with rac‐lactide (rac‐LA) and ?‐caprolactone (CL) were attempted. Rac‐LA copolymerized well with MAC, but CL copolymerizations produced insoluble products. Oligomeric macroinitiators of MAC and rac‐LA were synthesized from stannous ethoxide, and both macroinitiators were used for the controlled ring‐opening polymerization of rac‐LA. The polymerization kinetics were examined by monitoring the disappearance of the characteristic C? O ring stretch of the monomer at 1240 cm?1 with real‐time in situ Fourier transform infrared spectroscopy. Postpolymerization oxidation reactions were conducted to epoxidize the unsaturated bonds of the MAC‐functionalized polymers. Epoxide‐containing polymers may allow further organic transformations with various nucleophiles, such as amines, alcohols, and carboxylic acids. NMR was used for microstructure identification of the polymers, and size exclusion chromatography and differential scanning calorimetry were used to characterize the new functionalized poly(ester‐carbonates). © 2003 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 41: 1978–1991, 2003  相似文献   

19.
(E)‐1,3‐Pentadiene (EP) and (E)‐2‐methyl‐1,3‐pentadiene (2MP) were polymerized to cis‐1,4 polymers with homogeneous and heterogeneous neodymium catalysts to examine the influence of the physical state of the catalyst on the polymerization stereoselectivity. Data on the polymerization of (E)‐1,3‐hexadiene (EH) are also reported. EP and EH gave cis‐1,4 isotactic polymers both with the homogeneous and with the heterogeneous system, whereas 2MP gave an isotactic cis‐1,4 polymer with the heterogeneous catalyst and a syndiotactic cis‐1,4 polymer, never reported earlier, with the homogeneous one. For comparison, the results obtained with the soluble CpTiCl3‐based catalyst (Cp = cyclopentadienyl), which gives cis‐1,4 isotactic poly(2MP), are examined. A tentative interpretation is given for the mechanism of the formation of the stereoregular polymers obtained and a complete NMR characterization of the cis‐1,4‐syndiotactic poly(2MP) is reported. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2013, 51, 3227–3232  相似文献   

20.
A series of π‐conjugated polymers and copolymers containing 1,4‐dioxo‐3,6‐diphenylpyrrolo[3,4‐c]pyrrole (also known as 2,5‐dihydro‐3,6‐diphenylpyrrolo[3,4‐c]pyrrole‐1,4‐dione) (DPP) and 1,4‐phenylene units in the main chain is described. The polymers are synthesised using the palladium‐catalysed aryl‐aryl coupling reaction (Suzuki coupling) of 2,5‐dihexylbenzene‐1,4‐diboronic acid with 1,4‐dioxo‐2,5‐dihexyl‐3,6‐di(4‐bromophenyl)pyrrolo[3,4‐c]pyrrole and 1,4‐dibromo‐2,5‐dihexylbenzene in different molar ratios. Soluble hairy rod‐type polymers with molecular weights up to 21 000 are obtained. Polymer solutions in common organic solvents such as chloroform or xylene are of orange colour (λmax = 488 nm) and show strong photoluminescence (λmax = 544 nm). The photochemical stability is found to be higher than for corresponding saturated polymers containing isolated DPP units in the main chain. Good solubility and processability into thin films render the compounds suitable for electronic applications.  相似文献   