1,1‐Bis[4‐(4‐aminophenoxy)phenyl]‐1‐phenylethane (BAPPE) was prepared through nucleophilic substitution reaction of 1,1‐bis(4‐hydroxyphenyl)‐1‐phenylethane and p‐chloronitrobenzene in the presence of K2CO3 in N,N‐dimethylformamide, followed by catalytic reduction with hydrazine and Pd/C. Novel organosoluble polyimides and copolyimides were synthesized from BAPPE and six kinds of commercial dianhydrides, including pyromellitic dianhydride (PMDA, Ia ), 3,3′,4,4′‐benzophenonetetracarboxylic dianhydride (BTDA, Ib ), 3,3′,4,4′‐ biphenyltetracarboxylic dianhydride (BPDA, Ic ), 4,4′‐oxydiphthalic anhydride (ODPA, Id ), 3,3′,4,4′‐diphenylsulfonetetracarboxylic dianhydride (DSDA, Ie ) and 4,4′‐hexafluoroisopropylidenediphthalic anhydride (6FDA, If ). Differing with the conventional polyimide process by thermal cyclodehydration of poly(amic acid), when polyimides were prepared by chemical cyclodehydration with N‐methyl‐2‐pyrrolidone as used solvent, resulted polymers showed good solubility. Additional, Ia,b were mixed respectively with the rest of dianhydrides (Ic–f) and BAPPE at certain molar ratios to prepare copolyimides with arbitrary solubilities. These polyimides and copolyimides were characterized by good mechanical properties together with good thermal stability. © 2000 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 38: 2082–2090, 2000  相似文献   

2.
A series of organosoluble aromatic polyimides (PIs) was synthesized from 5,5′‐bis[4‐(4‐aminophenoxy)phenyl]‐4,7‐methanohexahydroindan (3) and commercial available aromatic dianhydrides such as 3,3′,4,4′‐biphenyltetracarboxylic dianhydride (BPDA), 4,4′‐oxydiphthalic anhydride (ODPA), 4,4′‐sulfonyl diphthalic anhydride (SDPA), or 2,2′‐bis(3,4‐dicarboxyphenyl) hexafluoropropanic dianhydride (6FDA). PIs (IIIc–f), which were synthesized by direct polymerization in m‐cresol, had inherent viscosities of 0.83–1.05 dL/g. These polymers could easily be dissolved in N,N′‐dimethylacetamide (DMAc), N‐methyl‐2‐pyrrolidone (NMP), N,N‐dimethylformamide (DMF), pyridine, m‐cresol, and dichloromethane. Whereas copolymerization was proceeded with equivalent molar ratios of pyromellitic dianhydride (PMDA)/6FDA, 3,3′,4,4′‐benzophenonetetracarboxylic dianhydride (BTDA)/6FDA, or BTDA/SDPA, or ½ for PMDA/SDPA, copolyimides (co‐PIs), derived from 3 and mixed dianhydrides, were soluble in NMP. All the soluble PIs could form transparent, flexible, and tough films, and they showed amorphous characteristics. These films had tensile strengths of 88–111 MPa, elongations at break of 5–10% and initial moduli of 2.01–2.67 GPa. The glass transition temperatures of these polymers were in the range of 252–311°C. Except for IIIe, the 10% weight loss temperatures (Td) of PIs were above 500°C, and the amount of carbonized residues of the PIs at 800°C in nitrogen atmosphere were above 50%. © 1999 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 37: 1681–1691, 1999  相似文献   

3.
A novel aromatic diamine monomer bearing tertbutyl and 4‐tertbutylphenyl groups, 3,3′‐ditertbutyl‐4,4′‐diaminodiphenyl‐4′′‐tertbutylphenylmethane (TADBP), was prepared and characterized. A series of non‐coplanar polyimides (PIs) were synthesized via a conventional one‐step polycondensation from TADBP and various aromatic dianhydrides including pyromellitic dianhydride (PMDA), 3,3′,4,4′‐biphenyltetracarboxylic dianhydride (BPDA), 4,4′‐oxydiphthalic anhydride (OPDA), 3,3′,4,4′‐benzophenone tetracarboxylic dianhydride (BTDA) and 4,4′‐(hexafluoroisopropylidene)dipthalic anhydride (6FDA). All PIs exhibit excellent solubility in common organic solvents such as N,N‐dimethylformamide (DMF), N,N‐dimethylacetamide (DMAc), N‐methyl‐2‐pyrrolidone (NMP), dimethyl sulfoxide (DMSO), chloroform (CHCl3), tetrahydrofuran (THF), and so on. Furthermore, the obtained transparent, strong and flexible polyimide films present good thermal stability and outstanding optical properties. Their glass transition temperatures (Tgs) are in the range of 298 to 347°C, and 10% weight loss temperatures are in excess of 490°C with more than 53% char yield at 800°C in nitrogen. All the polyimides can be cast into transparent and flexible films with tensile strength of 80.5–101 MPa, elongation at break of 8.4%–10.5%, and Young's modulus of 2.3–2.8 GPa. Meanwhile, the PIs show the cutoff wavelengths of 302–356 nm, as well as low moisture absorption (0.30% –0.55%) and low dielectric constant (2.78–3.12 at 1 MHz).  相似文献   

4.
A novel aromatic diamine monomer, 3,3′‐diisopropyl‐4,4′‐diaminodiphenyl‐3′′,4′′‐difluorophenylmethane (PAFM), was successfully synthesized by coupling of 2‐isopropylaniline and 3,4‐difluorobenzaldehyde. The aromatic diamine was adopted to synthesize a series of fluorinated polyimides by polycondensation with various dianhydrides: pyromellitic dianhydride (PMDA), 3,3′,4,4′‐biphenyltetracarboxylic dianhydride (BPDA), 4,4′‐oxydiphthalic anhydride (ODPA) and 3,3′,4,4′‐benzophenone tetracarboxylic dianhydride (BTDA) via the conventional one‐step method. These polyimides presented excellent solubility in common organic solvents, such as N,N‐dimethylformamide (DMF), N,N‐dimethyl acetamide (DMAc), dimethyl sulfoxide (DMSO), N‐methyl‐2‐pyrrolidone (NMP), chloroform (CHCl3), tetrahydrofuran (THF) and so on. The glass transition temperatures (Tg) of fluorinated polyimides were in the range of 260–306°C and the temperature at 10% weight loss in the range of 474–502°C. Their films showed the cut‐off wavelengths of 330–361 nm and higher than 80% transparency in a wavelength range of 385–463 nm. Moreover, polymer films exhibited low dielectric properties in the range of 2.76–2.96 at 1 MHz, as well as prominent mechanical properties with tensile strengths of 66.7–97.4 MPa, a tensile modulus of 1.7–2.1 GPa and elongation at break of 7.2%–12.9%. The polymer films also showed outstanding hydrophobicity with the contact angle in the range of 91.2°–97.9°.  相似文献   

5.
Four polyimides containing hexylene spacer and a fluorostilbene unit in the side chains were prepared in thin‐film form by two‐step condensation of 3,3′‐bis[(4′‐fluoro‐4‐stilbenyl)oxyhexyloxy]‐4,4′‐biphenyldiamine (FS6B) with pyromellitic dianhydride (PMDA), benzophenone‐3,3′,4,4′‐tetracarboxylic dianydride (BTDA), 4,4′‐oxydi(phthalic anhydride) (ODPA), and 4,4′‐hexafluoroisopropylidenedi(phthalic anhydride) (6FDA), respectively, and their controllability of liquid crystal (LC) alignment on rubbed surfaces was investigated. Pretilt angles of LCs were achieved in the 2–9° range, depending on the rubbing density and backbone structures. The effect of the mesogenic stilbene group on the pretilting of LCs was distinctive in FS6B‐PMDA. Contact‐angle measurements on thin films annealed at 120 °C revealed that FS6B‐PMDA potentially had the better alignment stability than FS6B‐6FDA. © 2001 John Wiley & Sons, Inc. J Polym Sci Part A: Polym Chem 39: 3622–3632, 2001  相似文献   

6.
The sorption of compressed carbon dioxide and methane in a series of all‐aromatic poly(etherimide) (PEI) thin films is presented. The polymer films are derived from the reactions between an arylether diamine (P1) and four different dianhydrides [3,3′,4,4′‐oxydiphthalic dianhydride (ODPA), 3,3′,4,4′ biphenyltetra‐carboxylic dianhydride (BPDA), 3,3′,4,4′‐benzo‐phenonetetracarboxylic dianhydride (BTDA), and pyromellitic dianhydride (PMDA)] that have been selected to systematically change the flexibility of the polymer backbone, the segmental mobility, and the nonequilibrium excess free volume (EFV) of the polymer. The EFV, gas sorption capacities, and sorption‐ and temperature‐induced dynamic changes in film thickness and refractive index have been investigated by spectroscopic ellipsometry. The sorption capacity depends to a great extent on the PEI backbone composition. PMDA‐P1 shows the highest carbon dioxide sorption, combined with the lowest sorption selectivity because of the predominant sorption of methane in the EFV. For ODPA‐P1, the highest sorption selectivity is obtained, while it shows little long‐term relaxations at carbon dioxide pressures up to 25 bar. © 2016 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2016 , 54, 986–993  相似文献   

7.
A novel diamine, bis‐(3‐aminophenyl)‐4‐(trifluoromethyl)phenyl phosphine oxide (mDA3FPPO), containing phosphine oxide and fluorine moieties was prepared via the Grignard reaction from an intermediate, 4‐(trifluoromethyl)phenyl diphenyl phosphine oxide, that was synthesized from diphenylphosphinic chloride and 4‐(trifluoromethyl)bromobenzene, followed by nitration and reduction. The monomer was characterized by Fourier transform infrared (FTIR), 1H NMR, 31P NMR, 19F NMR spectroscopies; elemental analysis; melting point measurements; and titration and was used to prepare polyimides with a number of dianhydrides such as pyromellitic dianhydride (PMDA), 5,5′‐[2,2,2‐trifluoro‐1‐(trifluoromethyl)ethyliden]‐bis‐1,3‐isobenzofuranedione (6FDA), 3,3′,4,4′‐benzophenone tetracarboxylic dianhydride (BTDA), and 4,4′‐oxydiphthalic dianhydride (ODPA). Polyimides were synthesized via a conventional two‐step route; preparation of polyamic acids, followed by solution imidization, and the molecular weight were controlled to 20,000 g/mol. Resulting polyimides were characterized by FTIR, NMR, DSC, and intrinsic viscosity measurements. Refractive‐index, dielectric constant, and adhesive properties were also determined. The properties of polyimides were compared with those of polyimides prepared from 1,1‐bis‐(4‐aminophenyl)‐1‐phenyl‐2,2,2‐trifluoroethane (3FDAm) and bis‐(3‐aminophenyl) phenyl phosphine oxide (mDAPPO). The polyimides prepared from mDA3FPPO provided high glass‐transition temperatures (248–311 °C), good thermal stability, excellent solubility, low birefringence (0.0030–0.0036), low dielectric constants (2.9–3.1), and excellent adhesive properties with Cu foils (107 g/mm). © 2001 John Wiley & Sons, Inc. J Polym Sci Part A: Polym Chem 39: 3335–3347, 2001  相似文献   

8.
A novel fluorinated aromatic diamine, 1,1‐bis(4‐amino‐3,5‐dimethylphenyl)‐1‐(3,5‐ditrifluoromethylphenyl)‐2,2,2‐trifluoroethane (9FMA), was synthesized by the coupling reaction of 3′,5′‐ditrifluoromethyl‐2,2,2‐trifluoroacetophenone with 2,6‐dimethylaniline under the catalysis of 2,6‐dimethylaniline hydrochloride. A series of fluorinated aromatic polyimides were synthesized from 9FMA and various aromatic dianhydrides, including pyromellitic dianhydride, 3,3′4,4′‐biphenyl tetracarboxylic dianhydride, 4,4′‐oxydiphthalic anhydride, 3,3′,4,4′‐benzophenone tetracarboxylic dianhydride (BTDA), and 4,4′‐hexafluoroisopropylidene diphthalic anhydride, via a high‐temperature, one‐stage imidization process. The inherent viscosities of the polyimides ranged from 0.37 to 0.74 dL/g. All the polyimides were quickly soluble in many low‐boiling‐point organic solvents such as tetrahydrofuran, chloroform, and acetone as well as some polar organic solvents such as N‐methyl‐2‐pyrrolidinone, N,N′‐dimethylacetamide, and N,N′‐dimethylformamide. Freestanding fluorinated polyimide films could be prepared and exhibited good thermal stability with glass‐transition temperatures of 298–334 °C and outstanding mechanical properties with tensile strengths of 69–102 MPa and elongations at break of 3.3–9.9%. Moreover, the polyimide films possessed low dielectric constants of 2.70–3.09 and low moisture absorption (<0.58%). The films also exhibited good optical transparency with a cutoff wavelength of 303–351 nm. One polyimide (9FMA/BTDA) also exhibited an intrinsic negative photosensitivity, and a fine pattern could be obtained with a resolution of 5 μm after exposure at the i‐line (365‐nm) wavelength. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 2665–2674, 2006  相似文献   

9.
We have synthesized a novel dianhydride, 2,2′-dichloro-4,4′,5,5′-benzophenone tetracarboxylic dianhydride (DCBTDA). Polyimides were synthesized with DCBTDA or 3,3′,4,4′-benzophenone tetracarboxylic dianhydride (BTDA) and several relatively rigid meta- and para- substituted mononuclear diamines. The BTDA based systems were insoluble in dipolar, aprotic solvents whereas the DCBTDA based polymers displayed enhanced solubility in these solvents. The thermal stability of these polyimides was excellent as measured by 5% weight loss decomposition. The Tg's of the polymers were all above 290°C.  相似文献   

10.
The isomeric diamine monomer 5(6)‐amino‐1‐(4‐aminophenyl)‐1,3,3‐trimethylindane (DAPI) was successfully synthesized via the dimerization of α‐methylstyrene followed by nitration and reduction. High molecular weight, soluble polyimides were synthesized via ester–acid solution imidization techniques and had glass‐transition temperature values ranging from 247 to 369 °C. The polymers were soluble in common organic solvents because of the asymmetric and nonplanar nature of DAPI and displayed good short‐term thermal stability by thermogravimetric analysis, as shown by their 5% weight‐loss values above 500 °C in air. The DAPI/(3,4‐dicarboxyphenyl) hexafluoropropane dianhydride (6FDA) polyimide also showed 2‐h thermal stability at 400 °C under nitrogen, despite the partial aliphatic character. Refractive index values as low as 1.571 were observed for DAPI/6FDA, which allows an estimated dielectric constant of 2.47 to be derived. The permeation of O2 and N2 was conducted on thin dense films. The bulky, bent, and isomeric nature of DAPI imparted film‐forming membranes that permitted high O2 permeability. In combination with 3,3′,4,4′‐benzophenone tetracarboxylic dianhydride (BTDA), DAPI had a good combination of O2 permeability and O2/N2 selectivity values of 2.8 Ba and 7.3, respectively. The polymerization method utilized to facilitate the cyclization of DAPI/BTDA to the polyimide affected the final thermal properties of the resulting polymer. The chemical imidization of DAPI/BTDA generated a polyimide with a glass‐transition temperature value of 311 °C and a 5% weight‐loss value in air of 457 °C. However, thermal and ester–acid imidization routes yielded an increase in the thermal properties. The ester–acid solution imidization of DAPI/BTDA produced a polymer glass‐transition temperature value of 333 °C and a 5% weight‐loss value of 525 °C in air. © 2000 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 38: 2840–2854, 2000  相似文献   

11.
A series of new polyimides were prepared via the polycondensation of (3‐amino‐2,4,6‐trimethylphenyl)‐(3′‐aminophenyl)methanone and aromatic dianhydrides, that is, 3,3′,4,4′‐biphenyltetracarboxylic dianhydride (BPDA), 4,4′‐oxydiphthalic anhydride, 3,3′,4,4′‐benzophenone tetracarboxylic dianhydride, and 2,2′‐bis(3,4‐dicarboxyphenyl) hexafluoropropane dianhydride. The structures of the polyimides were characterized by Fourier transform infrared and NMR measurements. The properties were evaluated by solubility tests, ultraviolet–visible analysis, differential scanning calorimetry, and thermogravimetric analysis. The two different meta‐position‐located amino groups with respect to the carbonyl bridge in the diamine monomer provided it with an unsymmetrical structure. This led to a restriction on the close packing of the resulting polymer chains and reduced interchain interactions, which contributed to the solubility increase. All the polyimides except that derived from BPDA had good solubility in strong aprotic solvents, such as N‐methyl‐2‐pyrrolidinone, N,N′‐dimethylacetamide, N,N‐dimethylformamide, and dimethyl sulfone, and in common organic solvents, such as cyclohexanone and chloroform. In addition, these polyimides exhibited high glass‐transition values and excellent thermal properties, with an initial thermal decomposition temperature above 470 °C and glass‐transition temperatures in the range of 280–320 °C. The polyimide films also exhibited good transparency in the visible‐light region, with transmittance higher than 80% at 450 nm and a cutoff wavelength lower than 370 nm. © 2005 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 1291–1298, 2006  相似文献   

12.
Two ternary miscible fluoro-polyimide blends have been identified. They are 6FDA-3,3′-6F-diamine/6FDA-4,4′- F - diamine/BTDA - 4,4′ - 6FDA blend and 6FDA - 3,3′ - 6F - diamine/6FDA - 4,4′ - 6F - diamine/ODPA - PMDA - 4,4′-6F-diamine blend (6FDA is 2,2′-bis(3,4′-dicarboxy- phenyl)hexafluoro propane dianhydride, 6F-diamine is 2,2′-bis(3-aminophenyl) hexafluoro propane). Their miscibility probably arises from the fact that their diamine parts have hexafluoro isopropylidene groups, their dianhydride parts have similar bond angle, space, rigidity and length. Several 6FDA-polyimides and PCTG 5445 (glycol-modified polycyclohexanedimethanolterephthalate) form- ing miscible blends have also been discovered. These surprising results suggest that hexafluoro-isopropylidene-group containing polyimides are quite intermolecular active and the 1,4-cyclohexane dimethanol component in PCTG 5445 may also offer unique miscibility capability. © 1997 John Wiley & Sons, Ltd.  相似文献   

13.
2,2,′3,3′‐Biphenyltetracarboxylic dianhydride (2,2,′3,3′‐BPDA) was prepared by a coupling reaction of dimethyl 3‐iodophthalate. The X‐ray single‐crystal structure determination showed that this dianhydride had a bent and noncopolanar structure, presenting a striking contrast to its isomer, 3,3,′4,4′‐BPDA. This dianhydride was reacted with aromatic diamines in a polar aprotic solvent such as N,N‐dimethylacetamide (DMAc) to form polyamic acid intermediates, which imidized chemically to polyimides with inherent viscosities of 0.34–0.55 dL/g, depending on the diamine used. The polyimides from 2,2,′3,3′‐BPDA exhibited a good solubility and were dissolved in polar aprotic solvents and polychlorocarbons. These polyimides have high glass transition temperatures above 283°C. Thermogravimetric analyses indicated that these polyimides were fairly stable up to 500°C, and the 5% weight loss temperatures were recorded in the range of 534–583°C in nitrogen atmosphere and 537–561°C in air atmosphere. All polyimides were amorphous according to X‐ray determination. © 1999 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 37: 1425–1433, 1999  相似文献   

14.
3,3′,4,4′‐Diphenylthioether dianhydride (4,4′‐TDPA), 2,3,3′,4′‐diphenylthioether dianhydride (3,4′‐TDPA), and 2,2′,3,3′‐diphenylthioether dianhydride (3,3′‐TDPA) were synthesized from 3‐chlorophthalic anhydride and 4‐chlorophthalic anhydride. A series of polyimides derived from the isomeric diphenylthioether dianhydrides with several diamines were prepared. The properties, such as the solubility, thermal and mechanical behavior, dynamic mechanical behavior, wide‐angle X‐ray diffraction, and permeability to some gases, were compared among the isomeric polyimides. Both 3,3′‐TDPA‐ and 3,4′‐TDPA‐based polyimides had good solubility in polar aprotic solvents and phenols. The 5% weight loss temperatures of all the obtained polyimides was near 500 °C in nitrogen. The glass‐transition temperatures decreased according to the order of the polyimides based on 3,3′‐TDPA, 3,4′‐TDPA, and 4,4′‐TDPA. The 3,4′‐TDPA‐based polyimides had the best permeability and lowest permselectivity, whereas the 4,4′‐TDPA‐based polyimides had the highest permselectivity and the lowest permeability of the three isomers. Furthermore, the rheological properties of thermoplastic polyimide resins based on the isomeric diphenylthioether dianhydrides were investigated, and they showed that polyimide 3,4′‐TDPA/4,4‐oxydianiline had the lowest melt viscosity among the isomers; this indicated that the melt processibility had been greatly improved. © 2005 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 959–967, 2006  相似文献   

15.
The proper combination of material (i.e. fluorinated polyimides) and processing technique (electrospinning) could lead to the formation of polyimides with low dielectric constant, high thermo‐oxidative stability and glass transition temperature, and high hydrophobicity. The polyimides in this work were based on 4, 4‐bis [3′‐trifluoromethyl‐4′ (4′‐amino benzoxy) benzyl] biphenyl (Q) and various fluorinated and non‐fluorinated dianhydrides namely benzene‐1,2,4,5‐tetracarboxylic dianhydride, 3,3′,4,4′‐biphenyltetracarboxylic dianhydride, benzophenone‐3,3′,4,4′‐tetracarboxylic dianhydride, and 4,4′‐(hexafluoroisopropylidene)diphthalic anhydride (6FDA). Processing of the polyimides was carried out in poly(amic acid) stage by two different methods—electrospinning and solution casting for comparison purposes. The processing of polyimides by electrospinning led to enhancement in mechanical properties (dianhydride‐structure dependent) and hydrophobicity without sacrificing thermo‐oxidative stability and glass transition temperatures significantly. Also, low dielectric constants (as low as 1.43) could be attained by suitable combination of dianhydride (6FDA) with 4, 4‐bis [3′‐trifluoromethyl‐4′ (4′‐amino benzoxy) benzyl] biphenyl diamine. Copyright © 2011 John Wiley & Sons, Ltd.  相似文献   

16.
A series of sulfonated polyimides (SPIs) were synthesized from a sulfonated diamine of 4,4′‐bis(4‐aminophenoxy) biphenyl‐3,3′‐disulfonic acid (BAPBDS), common nonsulfonated diamines, and various tetracarboxylic dianhydrides including 1,4,5,8‐naphthalene tetracarboxylic dianhydride (NTDA), 3,4,9,10‐perylene tetracarboxylic dianhydride (PTDA), 4,4′‐binaphthyl‐1,1′,8,8′‐tetracarboxylic dianhydride (BTDA), 4,4′‐ketone dinaphthalene 1,1′,8,8′‐tetracarboxylic dianhydride (KDNTDA), and isophthatic dinaphthalene 1,1′,8,8′‐tetracarboxylic dianhydride (IPNTDA). Their membrane properties were investigated to clarify the effects of the dianhydrides. They displayed reasonably high mechanical properties, thermal stability, and proton conductivity. The dianhydrides with flexible and non‐coplanar structure (IPNTDA > KDNTDA > BTDA) led to the better solubility of the SPIs than those with rigid and coplanar one (NTDA, PTDA). The dianhydride with the smaller molecular weight led to the larger value of the number of sorbed water molecules per sulfonic acid group (λ) in membrane, that is, NTDA (λ: 17) > PTDA (15) > BTDA (14) > KDNTDA (12) > IPNTDA (10), and as a result let to the larger proton conductivity in water. All of the BAPBDS‐based SPIs showed the anisotropy in membrane swelling and in proton conductivity, of which the degree hardly depended on the dianhydride moieties. The water stability of SPI membranes against the aging in water at 130 °C for 192 h was in the order, PTDA = NTDA ≧ BTDA > KDNTDA > IPNTDA. The hydrolysis stability of polymer chain was similar between the BTDA‐ and KDNTDA‐based SPIs. These results are discussed. © 2010 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 48: 905–915, 2010  相似文献   

17.
For polyimide thin films, the dielectric properties were investigated with the capacitance and optical methods. The dielectric constants of the 4,4′‐oxydianiline (ODA)‐based polyimide thin films varied from 2.49 to 3.10 and were in the following decreasing order: 3,3′,4,4′‐biphenyltetracarboxylic dianhydride (BPDA)–ODA > 1,2,4,5‐benzenetetracarboxylic dianhydride (PMDA)–ODA > 4,4′‐hexafluoroisopropylidene diphthalic dianhydride (6FDA)–ODA. According to the absorption of water, the diffusion coefficients in the films varied from 4.8 × 10?10 to 7.2 × 10?10 cm2/s and were in the following increasing order: BPDA–ODA < PMDA–ODA < 6FDA–ODA. The dielectric constants and diffusion coefficients of the polyimides were affected by the morphological structures, including the molecular packing order. However, because of the water uptake, the changes in the dielectric constants in the polyimide thin films varied from 0.49 to 1.01 and were in the following increasing order: BPDA–ODA < 6FDA–ODA < PMDA–ODA. Surprisingly, 6FDA–ODA with bulky hexafluoroisopropylidene groups showed less of a change in its dielectric constant than PMDA–ODA. The total water uptake for the polyimide thin films varied from 1.43 to 3.19 wt % and was in the following increasing order: BPDA–ODA < 6FDA–ODA < PMDA–ODA. This means that the changes in the dielectric constants in the polyimide thin films were significantly related to the morphological structure and hydrophobicity of hexafluoroisopropylidene groups. Therefore, the morphological structure and chemical affinity in the polyimide thin films were important factors in controlling the dielectric properties. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 2190–2198, 2002  相似文献   

18.
A triamine monomer, 1,3,5‐tris(4‐aminophenoxy)benzene (TAPOB), was synthesized from phloroglucinol and 4‐chloronitrobenzene, and it was successfully polymerized into soluble hyperbranched polyimides (HB PIs) with commercially available dianhydrides: 4,4′‐(hexafluoroisopropylidene)diphthalic anhydride (6FDA), 4,4′‐oxydiphthalic anhydride (ODPA), and 3,3′,4,4′‐benzophenonetetracarboxylic dianhydride (BTDA). Different monomer addition methods and different monomer molar ratios resulted in HB PIs with amino or anhydride end groups. From 1H NMR spectra, the degrees of branching of the amino‐terminated polymers were estimated to be 0.65, 0.62, and 0.67 for 6FDA–TAPOB, ODPA–TAPOB, and BTDA–TAPOB, respectively. All polymers showed good thermal properties with 10% weight‐loss temperatures (T10's) above 505 °C and glass‐transition temperatures (Tg's) of 208–282 °C for various dianhydrides. The anhydride‐terminated HB PIs showed lower T10 and Tg values than their amino‐terminated counterparts. The chemical conversion of the terminal amino or anhydride groups of the 6FDA‐based polyimides into an aromatic imido structure improved their thermal stability, decreased their Tg, and improved their solubility. The HB PIs had moderate molecular weights with broad distributions. The 6FDA‐based HB PIs exhibited good solubility even in common low‐boiling‐point solvents such as chloroform, tetrahydrofuran, and acetone. © 2002 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 40: 3804–3814, 2002  相似文献   

19.
A series of hyperbranched polyimides (HBPIs) were synthesized by reacting a triamine monomer N ,N ′,N ″‐tris(4‐methoxyphenyl)‐N ,N ′,N ″‐tris(4‐phenylamino)?1,3,5‐benzenetriamine with various dianhydrides such as oxydiphthalic dianhydride (ODPA), 3,3′,4,4′‐diphenylsulfonetetracarboxylic dianhydride (DSDA), 3,3′,4,4′‐benzophenonetetracarboxylic dianhydride (BTDA), and pyromellitic dianhydride (PMDA). The hyperbranched polyimide (6FHBPI) using 4,4′‐(hexafluoroisopropylidene)diphthalic anhydride (6FDA) as dianhydride monomer was also added into the discussion. All the hyperbranched polyimides exhibited excellent organo‐solubility and high thermal stability. Memory devices with a sandwiched structure of indium tin oxide (ITO)/HBPI/Al were constructed by using these HBPIs as the active layers. All these HBPIs based memory devices exhibited favorable memory performances, with switching voltages between ?1.3 V and ?2.5 V, ON/OFF current ratios up to 107 and retention times long to 104 s. Tunable memory characteristics from electrical insulator to volatile memory, and then to nonvolatile memory were obtained by adjusting the electron acceptors of these HBPIs. Molecular simulation results suggested that the electron affinity and the dipole moment of these HBPIs were responsible for the conversion of the memory characteristics. With the electron affinity and dipole moment of these HBPIs increasing, the memory characteristics turned from volatile to nonvolatile. The present study suggested that tunable memory performance could be achieved through adjusting the acceptor moieties of the hyperbranched polyimides. © 2017 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2017 , 55 , 2281–2288  相似文献   

20.
A new diamine monomer, 4,4″‐bis(aminophenoxy)‐3,3″‐trifluoromethyl terphenyl (ATFT) was synthesized that led to a number of novel fluorinated polyimides by solution as well as thermal imidization routes when reacted with different commercially available dianhydrides like pyromellatic dianhydride (PMDA), benzophenone tetracarboxylic acid dianhydride (BTDA), or 2,2‐bis(3,4‐dicarboxyphenyl) hexafluoropropane (6FDA). The polyimides ATFT/BTDA and ATFT/6FDA derived from both routes were soluble in several organic solvents such as N,N‐dimethylformamide, N,N‐dimethylacetamide, and dimethyl sulfoxide. The polyimide ATFT/PMDA was only soluble in N‐methylpyrollidone. The polyimide films had low water absorption of 0.3–0.7%, low dielectric constants of 2.72–3.3 at 1 Hz, refractive indices of 1.594–1.647 at 589.3 nm, and optical transparency >85%. These polyimides showed very high thermal stability with decomposition temperatures (5% weight loss) up to 532 °C in air and good isothermal stability; only 7% weight loss occurred at 400 °C after 7 h, and less than 0.6% weight loss was observed at 315 °C for 5 h. Transparent thin films of these polyimides exhibited tensile strengths up to 112 MPa, a modulus of elasticity up to 3.05 GPa, and elongation at break up to 21% depending on the repeating unit structure. © 2002 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 40: 1016–1027, 2002  相似文献   