1.
Polymerizations of ethylene by the MgCl2/ethylbenzoate/p-cresol/AlEt3 TiCl4-AlEt3/methyl-p-toluate (CW-catalyst) have been studied. The initially formed active site concentration, [Ti] has a maximum value of 50% of total titanium at 50°C and lower values at other temperatures. The Ti decays rapidly to Ti sites with conc. ca. 10 mol %/mol Ti. The rate constants for four chain transfer processes have been obtained at 50°C: for transfer with AlEt3, k = 2.1 × 10?4 s?1 and k = 4.8 × 10?4 s?1; for transfer with monomer, k = 3.6 × 10?3 (M s)?1 and K = 8.3 × 10?3 (M s)?1; for β-hydride transfer, k = 7.2 × 10?4 s?1 and k = 4.9 × 10?4 s?1; and transfer with hydrogen, k = 4.0 × 10?3 torr1/2 s? and k = 5.1 × 10?3 torr1/2 s?1. The rate constants for the termination assisted by hydrogen is k = 1.7 (M1/2 torr1/2 S)?1. If monomer is assisting termination as was observed for propylene polymerization, then k = 7.8 (M3/2 s)?1. Values of all the rate constants can be higher or lower at other temperatures. Detailed comparisons were made with the results of propylene polymerizations. There are more than four times as many Ti active sites for ethylene polymerization than there are for stereospecific polymerization of propylene; the difference is more than a factor of two for the Ti sites. Certain rate constants are nearly the same for both monomers while others are markedly different. Some of the differences can be explained by stereoelectronic effects.  相似文献   

2.
Soluble microgels with several pendant vinyl groups were synthesised by radical copolymerization of methyl methacrylate (MMA) with p-divinyl benzene (p-DVB). The competitive reactions of intermolecular and intramolecular crosslinkings of these microgels were carried out at 40°C in the presence of 1-buten-3-ol as a degradative chain transfer agent. The rate constant of intermolecular crosslinking (k) was estimated by GPC (gel permeation chromatography) analysis on the polymer produced from intermolecular propagation between bimolecules. The k depended strongly on the internal structure of microgels. Network formation was discussd inclusive of informations for the rate constant of intramolecular crosslinking (k).  相似文献   

3.
Acrylamide was polymerized in acetonitrile at 82 °C with a perfluorinated azo‐derivative initiator. The polymerization proceeded heterogeneously. Varying amounts of initiator and monomer were used. The activation energy was deduced from three experiments carried out at 59, 71, and 82 °C. The following kinetic law, deviating a great deal from the classical law, was obtained: R ∼ [I2][M](0.05% < [I2]o/[M]o < 1.00%) and R ∼ [I2][M](1% < [I2]o/[M]o < 7%). These results can be interpreted in light of the contribution of primary radical termination and the emergence of occlusion. The development of a new kinetic relationship allowed us to confirm the existence of both of these termination reactions. The calculation of the kprt /ki · kp ratio was also achieved. © 2000 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 38: 1834–1843, 2000  相似文献   

4.
In carbocationic polymerization and copolymerization, a recent publication concluded that the substituent effect on carbocation reactivity is much larger than its effect on monomer reactivity, and this by a factor 106 in the case of the rate constant k12capp for p‐methylstyrene addition (monomer M2) on, respectively, poly(p‐methoxystyrene)± or poly(p‐methylstyrene)± (M). This conclusion is disputed, as well as the assumption that the rate constants of capping (k12capp) obtained in deactivation reactions of poly(p‐methoxystyrene)± are identical with cross propagation rate constants in copolymerization (k12copol). It is shown that the large calculated k12capp are based on propagation constant values for p‐methylstyrene (k ≈ 109) obtained by the diffusion‐clock method. They are 104 times smaller as found for all styrenes, that is, between 104 and 105 when they are based on the ionic species concentrations. In such a case, the available data are still in agreement with an approximate compensation between the reactivities of a monomer and of the corresponding carbocation. It is also shown that copolymerization data for styrenes are not compatible with k values near to diffusion control, and that variations of log k12capp and log k12copol with the nucleophilicity parameter N of the monomers indicate a much lower selectivity of the monomers in the case of copolymerization. © 2010 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 48: 2666–2680, 2010  相似文献   

5.
Three molecules of 5-(bromoacetyl)salicylate ( 1 ) complexed to uranyl UO ion were crosslinked with branchy poly(ethylenimine) (PEI) in DMSO by alkylation of amino groups of PEI with 1, leading to the formation of UO2(Sal) PEI. Upon demetalation of UO2(Sal) PEI with HCl, apo(Sal) PEI was obtained. Based on the pH dependence of log Kf for UO2(Sal) PEI, it was concluded that each uranyl binding site in UO2(Sal) PEI or apo(Sal) PEI contains three salicylate moieties. In terms of the equilibrium constant for formation of the uranyl complex, apo(Sal) PEI was found to be comparable to or better than the previously reported effective uranophiles. In terms of the rates for the formation of the uranyl complex, however, apo(Sal) PEI was far superior to those other uranophiles. © 1997 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 35 : 2935–2942, 1997  相似文献   

6.
The cationic ring-opening polymerization of oxepane was found to be initiated by carbon black having acylium perchlorate (CO+CIO) groups, which were introduced by the reaction of acyl chloride groups with silver perchlorate. It was confirmed that polyoxepane, i.e., poly(oxyhexamethylene), was propagated from CO+CIO groups on carbon black and effectively grafted on the surface. The rate of the polymerization and the percentage of grafting of poly(oxyhexamethylene) remarkably increased by the addition of epichlorohydrin (ECH) as a promoter: the percentage of grafting in the presence of ECH increased to about 100% with an increase in conversion. Furthermore, CO+CIO groups on carbon black have an ability to initiate the cationic ring-opening copolymerization of oxepane with ECH to give poly(oxepane-co-ECH) with various composition. The ring-opening copolymerization of oxepane with phthalic anhydride was also initiated by CO+CIO groups to give polyether ester, i.e., poly(hexamethylene phthalate) containing poly(oxyhexamethylene) sequence. In the copolymerization, polyether or polyether ester was effectively grafted from carbon black based on the propagation of these polymers from CO+CIO groups.  相似文献   

7.
8.
The effect of external Lewis base (Be) on the polymerization of ethylene by the MgCl2/ethyl benzoate/p-cresol/AlEt3/TiCl4 catalyst was studied by activation with AlEt3 alone without the use of methyl-p-toluate. The initially formed active site concentration, [Ti], is about doubled in the absence of Be; at 50°C about 93% of the total titanium became catalytic. The same increment of [Ti] was observed without Be. The rate constants of propagation are not appreciably affected by Be; the values are the same at 50° with and without Be. At other temperatures the kp values are somewhat smaller without Be. One major effect was the very large k values for chain transfer with aluminum alkyls in the absence of Be as compared to those with Be. This can be attributed to the greater monomeric AlEt3 concentration in the former, but in much smaller amounts in the presence of Be due to complexation. The rate constants of chain transfer with hydrogen are not much affected by Be. However, the termination rate constants are generally much smaller when Lewis base is not present.  相似文献   

9.
A well‐defined branched copolymer with PLLA‐b‐PS2 branches was prepared by combination of reversible addition‐fragmentation transfer (RAFT) polymerization, ring‐opening polymerization (ROP), and atom transfer radical polymerization (ATRP). The RAFT copolymerization of methyl acrylate (MA) and hydroxyethyl acrylate (HEA) yielded poly(MA‐co‐HEA), which was used as macro initiator in the successive ROP polymerization of LLA. After divergent reaction of poly(MA‐co‐HEA)‐g‐PLLAOH with divergent agent, the macro initiator, poly(MA‐co‐HEA)‐g‐PLLABr2 was formed in high conversion. The following ATRP of styrene (St) produced the target polymer, poly(MA‐co‐HEA)‐g‐(PLLA‐b‐PS2). The structures, molecular weight, and molecular weight distribution of the intermediates and the target polymers obtained from every step were confirmed by their 1H NMR and GPC measurements. DSC results show one T = 3 °C for the poly(MA‐co‐HEA), T = ?5 °C, T= 122 °C, and T = 157 °C for the branched copolymers (poly(MA‐co‐HEA)‐g‐PLLA), and T = 51 °C, T = 116 °C, and T = 162 °C for poly(MA‐co‐HEA)‐g‐(PLLA‐b‐PS2). © 2005 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 549–560, 2006  相似文献   

10.
Poly(2,5‐dimethoxyaniline) (PDMA)–Ag composites were successfully obtained through the oxidative polymerization of 2,5‐dimethoxyaniline in poly(styrene sulfonic acid) with CH3SO3Ag and AgNO3 as oxidants. In situ ultraviolet–visible spectroscopy results showed that the growth rate of PDMA was strongly affected by CH3SO and NO. The coupling reaction of PDMA and NO was proposed to explain the lower growth rate of PDMA with AgNO3 as the oxidant in comparison with CH3SO3Ag. X‐ray photoelectron spectroscopy and Fourier transform infrared spectroscopy were used to validate the proposed coupling reaction through the monitoring of the side products and oxidized state of PDMA. The results showed that there were more side products and lower oxidized states for the composite structure in the presence of NO than in the presence of CH3SO, and this agreed with the proposal. Transmission electron microscopy showed that the Ag nanoparticles had almost the same size, regardless of the anions. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 6624–6632, 2006  相似文献   

11.
Solvay type S –VCl3 catalyst has 7% of catalytically active vanadium sites ([C*]) with kp (rate constant of propagation) = 31 (M s)?1 for ethylene polymerization. Addition of a comonomer, propylene of 4-methylpentene-1 (4-MP) significantly raised the ethylene polymerization activity. S –VCI3 catalyst has very small amounts of catalytically active vanadium for propylene polymerizations: [C] = 0.19% with kp,i = 857 (M s)?1 and [C] = 0.45% with kp,a = 23 (M s)?1 for isospecific and nonspecific sites, respectively. Addition of a conomer, ethylene or 4-MP. lowered the propylene polymerization activity. S –VCI3 is more easily reduced to the divalent ion by AIR3 than S –TiCl3. Methyl-p-toluate moderates the reducting power of AIR3; it increase the productivity and stereoselectivity of the S –YiCl3 catalyst, VCI3 supported on MgCl2 (CW–V catalyst) has enhanced rate constant of propylene polymerization but has the opposite effects on the S –TiCl3 Catalyst. VCI3 supported on MgCl2 (CW–V catalyst) has enhances rate constant of propylene polymerization but only a minute fraction of the supported vanadiums are catalytically active: [C] = 0.019% and kp,i = 1580 (Ms)?1, [C] = 0.057% and kp,i = 58 (M s)?1. This is compared with far greater number of catalytically active titanium sites in the TiCl3 supported on MgCl2 catalyst: [C] = 6% and kp,i = 200 (M s)?1, [C] = 6% and kp,a = 16(M s)?1. Therefore, both the S –VCI3 and CW–V catalysts are highly stereoselective but low in efficiency with respect to the utilization of the vanadium ion in the catalysis.  相似文献   

12.
Multipulse pulsed laser polymerization coupled with size exclusion chromatography (MP‐PLP‐SEC) has been employed to study the depropagation kinetics of the sterically demanding 1,1‐disubstituted monomer di(4‐tert‐butylcyclohexyl) itaconate (DBCHI). The effective rate coefficient of propagation, k, was determined for a solution of monomer in anisole at concentrations, c, 0.72 and 0.88 mol L?1 in the temperature range 0 ≤ T ≤ 70 °C. The resulting Arrhenius plot (i.e., ln k vs. 1/RT) displayed a subtle curvature in the higher temperature regime and was analyzed in the linear part to yield the activation parameters of the forward reaction. In the temperature region where no depropagation was observed (0 ≤ T ≤ 50 °C), the following Arrhenius parameters for kp were obtained (DBCHI, Ep = 35.5 ± 1.2 kJ mol?1, ln Ap = 14.8 ± 0.5 L mol?1 s?1). In addition, the k data was analyzed in the depropagatation regime for DBCHI, resulting in estimates for the associated entropy (?ΔS = 150 J mol?1 K?1) of polymerization. With decreasing monomer concentration and increasing temperature, it is increasingly more difficult to obtain well structured molecular weight distributions. The Mark Houwink Kuhn Sakurada (MHKS) parameters for di‐n‐butyl itaconate (DBI) and DBCHI were determined using a triple detection GPC system incorporating online viscometry and multi‐angle laser light scattering in THF at 40 °C. The MHKS for poly‐DBI and poly‐DBCHI in the molecular weight range 35–256 kDa and 36.5–250 kDa, respectively, were determined to be KDBI = 24.9 (103 mL g?1), αDBI = 0.58, KDBCHI = 12.8 (103 mL g?1), and αDBCHI = 0.63. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 1931–1943, 2007  相似文献   

13.
A new kind of polymeric chemosensor containing chiral naphthaldimine moiety in the side chain was synthesized by the reversible addition‐fragmentation chain transfer polymerization of N‐{[2‐(4‐vinylbenzyloxy)‐1‐naphthyl]‐methylene}‐(S)‐2‐phenylglycinol (VNP). The resulting polymers (PVNP) showed high selectivity for hydrogen sulfate relative to other anions including F?, Cl?, Br?, H2PO, CH3CO, and NO in tetrahydrofuran (THF) solution as judged from UV?vis, fluorescence, and circular dichroism spectrophotometric titrations. Compared with its monomer, the polymer has proven to be more attractive for detection of HSO in terms of sensitivity and reproducibility. Upon addition of the anion it gives remarkable spectral responses concomitant with detectable color change from colorless to pale yellow. Furthermore, the HSO‐induced CD or fluorescence signal can be totally reversed with addition of base and eventually recovered the initial state, leading to a reproducible molecular switch with two distinguished “on” and “off” states. © 2012 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2012  相似文献   

14.
The free radical promoted cationic polymerization cyclohexene oxide (CHO), was achieved by visible light irradiation (λinc = 430–490 nm) of methylene chloride solutions containing thioxanthone‐fluorene carboxylic acid (TX‐FLCOOH) or thioxanthone‐carbazole (TX‐C) and cationic salts, such as diphenyliodonium hexafluorophosphate (Ph2I+PF) or silver hexafluorophosphate (Ag+PF) in the presence of hydrogen donors. A feasible initiation mechanism involves the photogeneration of ketyl radicals by hydrogen abstraction in the first step. Subsequent oxidation of ketyl radicals by the oxidizing salts yields Bronsted acids capable of initiating the polymerization of CHO. In agreement with the proposed mechanism, the polymerization was completely inhibited by 2,2,6,6‐tetramethylpiperidinyl‐1‐oxy and di‐2,6‐di‐tert‐butylpyridine as radical and acid scavengers, respectively. Additionally polymerization efficiency was directly related to the reduction potential of the cationic salts, that is, Ag+PF (E = +0.8 V) was found to be more efficient than Ph2I+PF (E = ?0.2 V). In addition to CHO, vinyl monomers such as isobutyl vinyl ether and N‐vinyl carbazole, and a bisepoxide such as 3,4‐epoxycyclohexyl‐3′,4′‐epoxycyclohexene carboxylate, were polymerized in the presence of TX‐FLCOOH or TX‐C and iodonium salt with high efficiency. © 2011 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2011  相似文献   

15.
The kinetic feature of the anionic polymerization of N-PMI was investigated in THF. The polymerization system initiated with lithium tert-butoxide was revealed to be so-called “slow-initiation” system. The rate constant of the initiation reaction, ki, was obtained to be 4.2 × 10?3 (L mol?1 s?1) at ?72°C. The apparent rate constants of the propagation reaction, k, at ?72°C were individually obtained from each slope of the first-order plots in the later stages of the polymerizations for four different initiator concentrations. Each k is fairly close to that of initiation rate around 10?3. The propagation reaction was concluded to be dominated by ion-pair mechanism from the analysis of the kinetic data and the results of the addition effects of crown ether and common salt.  相似文献   

16.
Following earlier suggestions the values for the rate coefficient of chain termination kt in the bulk polymerization of styrene at 25°C were formally calculated (a) from the second moment of the chainlength distribution (CLD) and (b) from the rate equation for laser-initiated pseudostationary polymerization (both expressions originally derived for chain-length independent termination) by inserting the appropriate experimental data including the rate constant of chain propagation kp. These values were treated as average values, k and k , respectively. They exhibited good mutual agreement, even the predicted gradation (k < k by about 20%) was recovered. The log-log plot of kt vs. the number-average degree of polymerization of the chains at the moment of their termination yielded exponents b of 0.16–0.18 in the power-law kt = A · Pn −b, A ranging from 2.3 × 108 to 2.7 × 108 L · mol−1 · s−1. These data are only slightly affected if termination is not assumed to occur by recombination only and a small contribution of disproportionation is allowed for.  相似文献   

17.
Novel poly(3,4‐ethylenedioxythiophene) (PEDOT) polymers bearing imidazolium‐ionic liquid moieties were synthesized by electrochemical polymerizations. For this purpose, new functional monomers were synthesized having an 3,4‐ethylenedioxythiophene (EDOT) unit and an imidazolium‐ionic liquid with different anions such as tetrafluoroborate (BF), bis(trifluoromethane)sulfonimide ((CF3SO2)2N?), and hexafluorophosphate (PF). Next, polymer films were obtained by electrochemical synthesis in dicholoromethane solutions. Obtained polymers were characterized, revealing the characteristics of PEDOT in terms of electrochemical and spectroelectrochemical properties, FTIR, 1H NMR, and AFM microscopy. Interestingly, the hydrophobic character of electropolymerized films could be modified depending on the anion type. The hydrophobicity followed the trend PF > (CF3SO2)2N? > BF > pure PEDOT as determined by water contact angle measurements. Furthermore, the polymers could be dissolved in a range of polar organic solvents such as dimethylformamide, propylene carbonate, and dimethyl sulfoxide making these polymers interesting candidates for wet processing methods. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 3010–3021, 2009  相似文献   

18.
Decene-1 was polymerized with the CW catalyst and fractionated by precipitation technique. Light-scattering and viscometric measurements on these fractions established the relationship [η] = 5.19 × 10?3 M . The unperturbed mean square end-to-end distance is (〈R〉/M)1/2 = (6.17 ± 0.34) × 10?9. Light-scattering data is consistent with a relatively stiff molecule with length of L = 1.75 × 10?5 cm for poly(decene-1) with MW = 397,000. Its mean square radius of gyration 〈R〉 is 2.79 × 10?11 cm.2 The ratio of L2/〈R〉 = 11 is close to the theoretical ratio of 12 for this kind of macromolecule.  相似文献   

19.
Poly(vinyl alcohol) (PVA)/poly(vinyl acetate) (PVAc) microspheres with a skin/core structure were prepared through the heterogeneous surface saponification of PVAc microspheres suspension‐polymerized. The PVA skin formed through the heterogeneous saponification was hydrogel swellable in water. In addition, to obtain monodisperse PVA/PVAc microspheres having various skin/core ratios and morphologies, the ion‐specificities to the heterogeneous saponification were investigated using SO, Cl?, NO, Br?, and I? for anions and Li+, Na+, and K+ for cations, respectively. The ions were not specific significantly to the rate of the heterogeneous saponification, while were related to the degree of saponification (DS). DSs had different values between by weight loss (DSw) and by proton nuclear magnetic resonance spectroscopy (DSNMR) measurements. The order of DSws was SO < Cl? < NO < Br? < I? for anions and K+ < Na+ < Li+ for cations, and that of DSNMRs, I? < Br? < NO < Cl? < SO for anions and Li+ < Na+ < K+ for cations. The differences in values between DSws and DSNMRs were caused by the dissolution of PVA skin and were significantly decreased for SO. The peaks at melting temperature of PVA were sharp and their areas were large for ions deswelling PVA skins.  相似文献   

20.
(S)‐1‐Cyano‐2‐methylpropyl‐4′‐{[4‐(8‐vinyloxyoctyloxy)benzoyl]oxy}biphenyl‐ 4‐carboxylate [ (S)‐11 ] and (R)‐1‐cyano‐2‐methylpropyl‐4′‐{[4‐(8‐vinyloxyoctyloxy)benzoyl]oxy}biphenyl‐4‐carboxylate [( R)‐11 ] enantiomers, both greater than 99% enantiomeric excess, and their corresponding homopolymers, poly[ (S)‐11 ] and poly[ (R)‐11 ], with well‐defined molecular weights and narrow molecular weight distributions were synthesized and characterized. The mesomorphic behaviors of (S)‐11 and poly[ (S)‐11 ] are identical to those of (R)‐11 and poly[ (R)‐11 ], respectively. Both (S)‐11 and (R)‐11 exhibit enantiotropic SA, S, and SX (unidentified smectic) phases. The corresponding homopolymers exhibit SA and S phases. The homopolymers with a degree of polymerization (DP) less than 6 also show a crystalline phase, whereas those with a DP greater than 10 exhibit a second SX phase. Phase diagrams were investigated for four different pairs of enantiomers, (S)‐11 /( R)‐11 , (S)‐11 /poly[ (R)‐11 ], and poly[ (S)‐11 ]/poly[ (R)‐11 ], with similar and dissimilar molecular weights. In all cases, the structural units derived from the enantiomeric components are miscible and, therefore, isomorphic in the SA and S phases over the entire range of enantiomeric composition. Chiral molecular recognition was observed in the SA and SX phases of the monomers but not in the SA phase of the polymers. In addition, a very unusual chiral molecular recognition effect was detected in the S phase of the monomers below their crystallization temperature and in the S phase of the polymers below their glass‐transition temperature. In the S phase of the monomers above the melting temperature and of the polymers above the glass‐transition temperature, nonideal solution behavior was observed. However, in the SA phase the monomer–polymer and polymer–polymer mixtures behave as an ideal solution. © 2000 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 38: 3631–3655, 2000  相似文献   