1.
The crystal and magnetic structures of manganite Pr0.7Ba0.3MnO3 have been studied at high pressures of up to 5.1 GPa and temperatures from 10 to 300 K by means of the neutron diffraction. At normal pressure and a temperature T C = 200 K, a ferromagnetic state forms in Pr0.7Ba0.3MnO3. At high pressures P ≥ 1.9 GPa and T < T N ≈ 153 K, a new antiferromagnetic state of A-type have been observed. Under high pressure, the Curie temperature T C increases with the characteristic quantity dT C/dP ≈ 2.4 K/GPa. A possible reason for the appearance of an A-type antiferromagnetic phase in Pr0.7Ba0.3MnO3 at high pressures may be anisotropic uniaxial compression of oxygen octahedra along the b axis of the orthorhombic structure.  相似文献   

2.
The atomic and magnetic structures of La0.5Ca0.5CoO3 cobaltite have been studied by the neutron diffraction technique at high pressures of up to 4 GPa in the 10- to 300-K temperature range. The pressure dependences of the structural parameters have been obtained. The Curie temperature increases with the pressure with the coefficient dT C/dP = 1 K/GPa, demonstrating the stability of the ground ferromagnetic (FM) state. The pressure dependence of the ground FM state in La0.5Ca0.5CoO3 is in drastic contrast with that for La1 − x Ca x CoO3 at a lower calcium content (x < 0.3). For the latter compound, the pressure suppressed the ground FM state and a large negative pressure coefficient of the Curie temperature (dT C/dP ∼ −10 K/GPa) was observed. The nature of such a phenomenon is analyzed in the framework of the double exchange model also taking into account the changes in the electron configuration of Co3+ ions.  相似文献   

3.
The crystal structure and Raman spectra of Pr0.7Ca0.3MnO3 manganite at high pressures of up to 30 GPa and the magnetic structure at pressures of up to 1 GPa have been studied. A structural phase transition from the orthorhombic phase of the Pnma symmetry to the high-pressure orthorhombic phase of the Imma symmetry has been observed at P ∼ 15 GPa and room temperature. Anomalies of the pressure dependences of the bending and stretching vibrational modes have been observed in the region of the phase transition. A magnetic phase transition from the initial ferromagnetic ground state (T C = 120 K) to the A-type antiferromagnetic state (T N = 140 K) takes place at a relatively low pressure of P = 1 GPa in the low-temperature region. The structural mechanisms of the change of the character of the magnetic ordering have been discussed.  相似文献   

4.
The crystal and magnetic structures of Pr0.15Sr0.85MnO3 manganite have been studied by means of powder X-ray and neutron diffraction in the temperature range 10–400 K at high external pressures up to 55 and 4 GPa, respectively. A structural phase transition from cubic to tetragonal phase upon compression was observed, with large positive pressure coefficient of transition temperature dT ct /dP = 28(2) K/GPa. The C-type antiferromagnetic (AFM) ground state is formed below T N 260 K at ambient pressure. While at ambient pressure the structural and magnetic transition temperatures are close, T ct ~ T N , upon compression they become decoupled with T N T ct due to much weaker T N pressure dependence with coefficient dT N /dP = 3.8(1) K/GPa.  相似文献   

5.
The crystal and magnetic structures of La0.75Ca0.25MnO3 manganite are studied under high pressures up to 4.5 GPa in the temperature range 12–300 K by the neutron diffraction method. At normal pressure and temperature T C = 240 K, a ferromagnetic state is formed in La0.75Ca0.25MnO3. At high pressures P ≥ 1.5 GPa and at temperatures T < T N ≈ 150 K, a new A-type antiferromagnetic state appears. A further increase in pressure leads to an increase in the volume fraction of the antiferromagnetic phase, which coexists with the initial ferromagnetic phase. The effect of high pressure causes a considerable increase in T C with the slope dT C /dP ≈ 12 K/GPa. Calculations performed in the framework of the double exchange model with allowance for the electron-phonon interaction make it possible to explain this pressure dependence of T C on the basis of experimental data.  相似文献   

6.
The crystal structure of lead titanate PbTiO3 was investigated by energy dispersive X-ray diffraction at high pressures up to 4 GPa in a temperature range of 300–950 K. At the ambient conditions, the PbTiO3 structure is tetragonal with the space group P4mm (ferroelectric phase). A structural phase transition into the cubic phase with a space group Pm[`3]mPm\bar 3m is observed at T = 747 K. It was found that the phase transition temperature decreases upon applying the high pressure with the coefficient dT C /dP = -65 K/GPa. Dependences of parameters and volume of the unit cell on the pressure and temperature was found, and the bulk modulus and thermal expansion coefficients for the tetragonal and cubic phases of lead titanate have been calculated.  相似文献   

7.
The crystal and magnetic structures of the oxygen deficient manganites La0.7Sr0.3MnO3-d (d = 0.15, 0.20) have been studied by means of powder neutron diffraction over the 0–5.2 GPa pressure and 10–290 K temperature ranges. La0.7Sr0.3MnO2.85 exhibits a coexistence of rhombohedral and tetragonal (I4/mcm) crystal structures and below Tg ~ 50 K a spin glass state is formed. La0.7Sr0.3MnO2.80 exhibits a tetragonal (I4/mcm) crystal structure. Below Tg ~ 50 K a phase separated magnetic state is formed, involving coexistence of C-type AFM domains with spin glass domains. In both compounds the crystal structure and magnetic states remain stable upon compression. The factors leading to the formation of different magnetic states in La0.7Sr0.3MnO3-d (d = 0.15, 0.20) and their specific high pressure behavior, contrasting with that of the stoichiometric A0.5Ba0.5MnO3 (A = Nd, Sm) compounds showing pressure-induced suppression of the spin glass state and the appearance of the FM state, are analysed.  相似文献   

8.
High pressure evolution of structural, vibrational and magnetic properties of La0.75Ca0.25MnO3 was studied by means of X-ray diffraction and Raman spectroscopy up to 39 GPa, and neutron diffraction up to 7.5 GPa. The stability of different magnetic ground states, orbital configurations and structural modifications were investigated by LDA + U electronic structure calculations. A change of octahedral tilts corresponding to the transformation of orthorhombic crystal structure from the Pnma symmetry to the Immaone occurs above P ~ 6 GPa. At the same time, the evolution of the orthorhombic lattice distortion evidences an appearance of the e g d x² ? z² orbital polarization at high pressures. The magnetic order in La0.75Ca0.25MnO3 undergoes a continuous transition from the ferromagnetic 3D metallic (FM) ground state to the A-type antiferromagnetic (AFM) state of assumedly 2D pseudo-metallic character under pressure, that starts at about 1 GPa and extends possibly to 20–30 GPa.  相似文献   

9.
The crystal and magnetic structures and the vibrational spectra of Pr0.7Sr0.3MnO3 manganite are studied within the pressure range up to 25 GPa by methods of X-ray diffraction and Raman spectroscopy. Neutron diffraction studies have been performed at pressures up to 4.5 GPa. The magnetic phase transition from the ferromagnetic phase (T C = 273 K) to the A-type antiferromagnetic phase (T N = 153 K) is found at P ≈ 2 GPa. This transition is characterized by a broad pressure range corresponding to the phase separation. The Raman spectra of Pr0.7Sr0.3MnO3 measured under high pressures significantly differ from the corresponding spectra of the isostructural doped A1 ? x A′ x MnO3 manganites, (where A is a rare-earth ion and A′ is an alkaline-earth ion) with the smaller average ionic radius 〈r A〉 of A and A′ cations. Namely, the former spectra do not include clearly pronounced stretching phonon modes. At P ~ 7 GPa, there appears the structural phase transition from the orthorhombic phase with the Pnma space group to the orthorhombic high-pressure phase with the Imma symmetry. In the vicinity of the phase transition, anomalies in the pressure dependences of the lattice parameters, unit cell volume, and phonon frequencies corresponding to the characteristic lattice vibration modes are observed.  相似文献   

10.
The effect of hydrostatic pressure on the photoluminescence and Raman spectra of hydrofullerene C60H36 was investigated for pressures up to 12 GPa at room temperature. The samples were synthesized by means of high-pressure hydrogenation. The pressure coefficients of the phonon modes were found to be positive and demonstrate singularities at ~0.7 and ~6 GPa. The pressure shift of the luminescence spectrum is unusually small and increases slightly at P≥6 GPa. All observed features are reversible with pressure, and C60H36 is stable in the pressure region investigated.  相似文献   

11.
Pressure effects on magnetic properties of two La0.7Ca0.3MnO3 nanoparticle samples with different mean particle sizes were investigated. Both the samples were prepared by the glycine-nitrate method: sample S—as-prepared (10 nm), and sample S900—subsequently annealed at 900 °C for 2 h (50 nm). Magnetization measurements revealed remarkable differences in magnetic properties with the applied pressure up to 0.75 GPa: (i) for S sample, both transition temperatures, para-to-ferromagnetic T C = 120 K and spin-glass-like transition T f = 102 K, decrease with the pressure with the respective pressure coefficients dT C/dP = −2.9 K/GPa and dT f/dP = −4.4 K/GPa; (ii) for S900 sample, para-to-ferromagnetic transition temperature T C = 261 K increases with pressure with the pressure coefficient dT C/dP = 14.8 K/GPa. At the same time, saturation magnetization M S recorded at 10 K decreases/increases with pressure for S/S900 sample, respectively. Explanation of these unusual pressure effects on the magnetism of sample S is proposed within the scenario of the combined contributions of two types of disorders present in the system: surface disorder introduced by the particle shell, and structural disorder of the particle core caused by the prominent Jahn–Teller distortion. Both disorders tend to vanish with the annealing of the system (i.e., with the nanoparticle growth), and so the behavior of the sample S900 is similar to that previously observed for the bulk counterpart.  相似文献   

12.
Stability of the linear orthorhombic polymer of C60 under pressure and laser irradiation is studied by Raman scattering and X-ray diffraction measurements. The Raman spectrum at ambient pressure remains unchanged, in the time scale of the experiment, up to an intensity of 3200 W/cm2 of the 514.5 nm line of an Ar+ laser, but irreversible changes are observed at higher intensities. The Raman spectra recorded at increased pressure show similar irreversible changes even at the laser intensity as low as 470 W/cm2. The X-ray diffraction and Raman measurements of the pressure-treated samples, performed after pressure release, show that the nonirradiated material does not exhibit any changes in the crystal structure and phonon spectra. This behavior indicates a pressure-enhanced photo-induced transformation to a new polymeric phase characterized by a Raman spectrum that differs from those of the other known polymeric phases of C60. The Raman spectra of the phototransformed linear orthorhombic polymer of C60 were measured at a pressure of up to 29 GPa. The pressure dependence of the Raman mode frequencies show singularities near 4 GPa and 15 GPa, respectively, related to a reversible phase transition and an irreversible transformation to a metastable disordered phase. The diffuse Raman spectrum of the disordered phase does not exhibit substantial changes with an increase in pressure up to 29 GPa. The high-pressure phase transforms to a mixture of pristine and dimerized C60, after pressure release and exposure to ambient conditions for 30 h. The text was submitted by the authors in English.  相似文献   

13.
The behavior of the specific heat of MnS2 at high pressures has been studied. A significant increase in the transition temperature TN to an antiferromagnetic state with the pressure from 48.2 K at atmospheric pressure to 76 K at a pressure of 5.3 GPa has been revealed. The initial pressure derivative is dT N /dP = 4.83 K/GPa. It has been found that the parameter α = d(logT N )/d(logV ) = ?6.6 ± 0.1 is significantly different from the value α = ?10/3 ≈ ?3.3 (Bloch relation), which is typical of numerous antiferromagnetic insulators—transition- metal oxides and fluorides. The volume jump at the magnetic transition point has been estimated. The necessity of direct dilatometric measurements of the volume has been justified.  相似文献   

14.
We present the results from studying the magnetic properties (linear and nonlinear susceptibilities and the depolarization of polarized neutrons) of Nd1 − x Ba x MnO3 manganite, x = 0.3, with Curie temperature T C ≈ 140 K and dielectric-to-metal transition temperature T DM ≈ 129 K. Its critical behavior corresponds to that of an isotropic 3-D ferromagnet at temperatures above T*≈ 144 K, but a strong nonlinear response in weak magnetic fields and depolarization are observed at temperatures below T*. It is shown that this nontraditional behavior is related to the generation of ferromagnetic clusters in the paramagnetic matrix that form a conducting percolative network at temperatures near T DM.  相似文献   

15.
The structure and magnetic states of a crystal of lightly doped manganite La0.95Ba0.05MnO3 were studied using thermal-neutron diffraction, magnetic measurements, and electrical resistance data in a wide temperature range. It is shown that, in terms of its magnetic properties, the orthorhombic crystal is characterized by two order parameters, namely, antiferromagnetic (T N = 123.6 K) and ferromagnetic (T C = 136.7 K). The results obtained differ in detail from known information on the manganites La0.95Ca0.05MnO3 and La0.94Sr0.06MnO3. Two models of the magnetic state of the La0.95Ba0.05MnO3 crystal are discussed, one of which is a model of a canted antiferromagnetic spin system and another is associated with the phase separation of the manganite. Arguments are advanced in favor of the coexistence in this crystal of the antiferromagnetic phase (about 87%) with a Mn4+ ion concentration of 0.048 and the 1/16-type charge-ordered ferromagnetic phase (about 13%) with a Mn4+ ion concentration of 0.0625. The specific features of the manganite studied are due to self-organization of the La0.95Ba0.05MnO3 crystal lattice caused by the relatively large barium ion size.  相似文献   

16.
The temperature and magnetic-field dependences of the heat capacity, thermal conductivity, thermopower, and electrical resistivity of the Sm0.55Sr0.45MnO3.02 ceramic material are studied in the temperature range 77–300 K and in magnetic fields up to 26 kOe. It is revealed that the quantities under investigation exhibit anomalous behavior due to a magnetic phase transition at the Curie temperature TC. An increase in the magnetic field strength H leads to an increase in the Curie temperature TC and a jump in the heat capacity ΔCp at TC. The temperature dependences of the measured quantities are characterized by hystereses that are considerably suppressed in a magnetic field of 26 kOe and depend neither on the thermocycling range nor on the rate of change in the temperature. The thermal conductivity K at temperatures above TC shows unusual behavior for crystalline solids (dK/dT>0) and, upon the transition to a ferromagnetic state, drastically increases as a result of a decrease in the phonon scattering by Jahn-Teller distortions. It is demonstrated that the hystereses of the studied properties of the Sm0.55Sr0.45MnO3.02 manganite are caused by a jumpwise change in the critical temperature due to variations in the lattice parameters upon the magnetic phase transition.  相似文献   

17.
The low-temperature specific heat C p of La(Fe0.873Co0.007Al0.12)13 compound has been measured in two states: (i) antiferromagnetic (AFM) with a Néel temperature of T N = 192 K and (ii) ferromagnetic (FM). The FM order appears at T = 4.2 K in a sample exposed to an external magnetic field with induction B C ≥ 2.5 T and is retained for a long time in a zero field at temperatures up to T*C = 23 K. The coefficient γFM in the low-temperature specific heat C = γT + βT 3 in the FM state differs quite insignificantly from that (γAFM) in the AFM state. Contributions to the low-temperature specific heat, which are related to a change in the elastic and magnetoelastic energy caused by magnetostrictive deformations, are considered.  相似文献   

18.
The atomic and magnetic structures of the La0.7Sr0.3CoO3 cobaltite are investigated using neutron diffraction at high pressures up to 4.2 GPa in the temperature range 16–300 K. The structural parameters are determined as functions of the pressure. It is revealed that the effect of high pressure leads to a decrease in the Curie temperature: dT C/dP = −8.3(8) K/GPa. It is established that, under high pressure, the decrease in the Curie temperature T C is associated with the transition of a number of Co3+ ions from the intermediate-spin state (t 2g 5 e g 1 , S = 1) to the low-spin state (t 2g 6 , S = 0).  相似文献   

19.
The crystal and magnetic structure of Pr0.1Sr0.9MnO3 manganite has been studied by the neutron diffraction at high pressures up to 5 GPa in the temperature range 10?C295 K. At normal pressure and decreasing temperature the appearance of the C-type (T N = 220 K) and G-type (T N = 180 K) antiferromagnetic states occurs, which is accompanied by a structural phase transition from the cubic structure (Pm $ \bar 3 $ m space group) to the tetragonal structure (I4/mcm space group). It is shown that the temperature of the transition to the C-type antiferromagnetic phase increases with pressure with the pressure coefficient dT N/dP = 4.0(5) K/GPa and the temperature of the transition to the G-type antiferromagnetic phase weakly depends on pressure.  相似文献   

20.
An experimental study of the temperature behavior of longitudinal sound velocity, internal friction, electrical resistivity, and thermopower of single-crystal La0.75Ba0.25MnO3 is reported. A structural transition accompanied by a large jump (18%) in the sound velocity was found to occur at T S ≈170 K. Within the interval 156–350 K, the temperature dependences of the sound velocity and internal friction reveal a temperature hysteresis. An internal-friction peak due to relaxation processes was detected. The metallic and semiconducting regions are separated by a transition domain about 80 K wide lying below the Curie temperature T C =300 K.  相似文献   