1.
We report an available approach for quickly fabricating CdS QD‐polymer nanocomposites via frontal polymerization (FP). First, we synthesized (3‐mercaptopropyl)‐1‐trimethoxysilane (MPS)‐capped CdS quantum dots (QDs). With these MPS‐capped CdS QDs containing mercapto groups, MPS‐capped CdS QDs can be easily incorporated into a poly(N‐methylolacrylamide) (PNMA) matrix via FP. A variety of features for preparing QD‐polymer nanocomposites, such as initiator concentration and CdS concentration, were thoroughly investigated. The fluorescence properties of QD‐polymer nanocomposites prepared via FP are comparatively investigated on the basis of ultraviolet–visible (UV–vis) spectra and photoluminescence (PL) spectra. Results show that the PL intensity of QD‐polymer nanocomposites prepared via the FP method is superior to that obtained by the traditional batch polymerization (BP) method. In addition, by measuring the changes of PL intensity of the samples immersed in different concentrations of copper acetate solution, we found the QD‐polymer nanocomposites can be ultrasensitive to copper ions. This FP process can be exploited as a facile and rapid way for synthesis QD‐polymer nanocomposites on a large scale, avoiding the fluorescence quenching of nanocrystals during incorporation nanocrystals into polymer matrices. © 2010 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 48: 2170–2177, 2010  相似文献   

2.
A series of A3‐type star poly(methylmethacrylate)/clay nanocomposites is prepared by in situ atom transfer radical polymerization (ATRP) initiated from organomodified montmorillonite containing quaternary trifunctional ATRP initiator. The first order kinetic plot shows a linear behavior, indicating the controlled character of the polymerization. The resulting nanocomposites are characterized by spectroscopic (XRD), thermal (DSC and TGA), and microscopic (TEM) analyses. The exfoliated nanocomposite has been obtained when polymerization was conducted with 1% of organic clay loading. Thermal analyses show that all nanocomposites have higher glass transition values and thermal stabilities compared to neat polymer. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2013 , 51, 5257–5262  相似文献   

3.
Polystyrene (PS)/clay nanocomposites were prepared with two different new intercalation organophilic clays, the phosphonium salt (APP) and the ammonium 4‐(4‐adamantylphenoxy)‐1‐butanamine (APB) salts, by emulsion polymerization technique. X‐ray diffraction and transmission electron microscopy were performed to characterize the layered structures of APB‐ and APP‐treated polymer–clay nanocomposites, and both resulted in exfoliated structures. Molecular weights of PS obtained from these nanocomposites are slightly lower than the virgin PS formed under similar polymerization conditions. Coefficient of thermal expansion showed approximately a 44–55% decrease for APB‐ and APP‐intercalated clay nanocomposites relative to the pure PS. Both Tg and thermal decomposition temperature of the PS component in the nanocomposite are higher than the virgin PS, implying that the presence of clay is able to enhance thermal stabilities of the PS. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 45: 1781–1787, 2007  相似文献   

4.
We report the first synthesis of poly (N‐methylolacrylamide) (PNMA) via free‐radical frontal polymerization (FP) with solid monomers at ambient pressure. The appropriate amounts of reactants (N‐methylolacrylamide) (NMA) and initiator (ammonium persulfate) were mixed together at ambient temperature without solvent. FP was initiated by heating the wall of the tube with a soldering iron, and the resultant hot fronts were allowed to self‐propagate throughout the reaction vessel. Once initiated, no further energy was required for polymerization to occur. To suppress the fingers of molten monomer, a small amount of nanosilica was added. We also produced PNMA with dimethyl sulfoxide (DMSO) or N‐methyl‐2‐pyrrolidone, as solvent by FP, to study the macrokinetics in FP of PNMA without fillers. The front velocity and front temperature dependence on the ammonium persulfate and N‐methyl‐2‐pyrrolidone concentration were investigated. The polymer was analyzed by thermogravimetric analysis. Results show that without postpolymerization solvent removal, waste production can be reduced. Solvent‐free FP could be exploited as a means for preparation of PNMA with the potential advantage of higher throughput than solvent‐based methods. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 4322–4330, 2007  相似文献   

5.
In this work, the synthesis of polypropylene (PP)/graphene nanosheet (GNS) nanocomposites by in situ polymerization using metallocene catalysts was studied. Initial reactions were performed using rac‐Et(Ind)2ZrCl2 and rac‐Me2Si(Ind)2ZrCl2 catalysts to select the best one to obtain good molecular weight, thermal properties, and tacticity. Subsequently, PP nanocomposites with different loadings of GNS were obtained. GNS from two different sources [Graphite Nacional (GN) and Graphite Aldrich (GA)] have been used, and the differences between the obtained nanocomposites were evaluated. The GNS and nanocomposites were studied by scanning electronic microcopy, transmission electronic microcopy, and X‐ray diffraction. They showed that the GN nanosheets had lower crystal size and diameter than the GA nanosheets and dispersed better in the PP matrix. Differential scanning calorimetry analyses of both types of nanocomposites showed an increase in the crystallization temperature with increasing graphite loading. The polymeric materials were also characterized by GPC, thermogravimetric analysis, and 13C NMR. © 2012 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2012  相似文献   

6.
We report on a new strategy for fabricating well‐defined POSS‐based polymeric materials with and without solvent by frontal polymerization (FP) at ambient pressure. First, we functionalize polyhedral oligomeric silsesquioxane (POSS) with isophorone diisocyanate (IPDI). With these functionalized POSS‐containing isocyanate groups, POSS can be easily incorporated into a poly(N‐methylolacrylamide) (PNMA) matrix via FP in situ. Constant velocity FP is observed without significant bulk polymerization. The morphology and thermal properties of POSS‐based hybrid polymers prepared via FP are comparatively investigated on the basis of scanning electronic microscopy (SEM) and thermogravimetric analysis (TGA). Results show that the as‐prepared POSS‐based polymeric materials exhibit a higher glass transition temperature than that of pure PNMA, ascribing to modified POSS well‐dispersed in these hybrid polymers. Also, the products with different microstructures display different thermal properties. The pure PNMA exhibits a featureless morphology, whereas a hierarchical morphology is obtained for the POSS‐based polymeric materials. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 1136–1147, 2009  相似文献   

7.
A metal complex, cobalt(II) 2‐ethylhexanoate (CEH), was added to the system of thermal‐initiated reversible addition‐fragmentation chain transfer (RAFT) polymerization of methyl methacrylate (MMA) with 2‐cyanoprop‐2‐yl 1‐dithionaphthalate (CPDN) as the RAFT agent at 115 °C. The polymerization rate was remarkably enhanced in the presence of CEH in comparison with that in the absence of CEH, and the increase of the CPDN concentration also accelerated the rate of polymerization. The polymerization in the concurrence of CPDN and CEH demonstrated the characters of “living”/controlled free radical polymerization: the number‐average molecular weights (Mn) increasing linearly with monomer conversion, narrow molecular weight distributions (Mw/Mn) and obtained PMMA end‐capped with the CPDN moieties. Meanwhile, CEH can also accelerate the rate of RAFT polymerization of MMA using the PMMA as macro‐RAFT agent instead of CPDN. Similar polymerization profiles were obtained when copper (I) bromide (CuBr)/N,N,N′,N′′,N′′‐pentamethyldiethylenetriamine was used instead of CEH. Extensive experiments in the presence of butyl methacrylate, bis(cyclopentadienyl) cobalt(II) and cumyl dithionaphthalenoate were also conducted; similar results as those of MMA/CPDN/CEH system were obtained. A transition of the polymerization mechanism, from RAFT process without CEH addition to atom transfer radical polymerization in the presence of CEH, was possibly responsible for polymerization profiles. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 5722–5730, 2007  相似文献   

8.
9.
Highly exfoliated isotactic‐polypropylene/alkyl‐imidazolium modified montmorillonite (PP/IMMT) nanocomposites have been prepared via in situ intercalative polymerization. TEM and XRD results indicated that the obtained composites were highly exfoliated PP/IMMT nanocomposites and the average thickness of IMMT in PP matrix was less than 10 nm, and the distance between adjacent IMMT particles was in the range of 20–200 nm. The isothermal crystallization kinetics of highly exfoliated PP/IMMT nanocomposites were investigated by using differential scanning calorimeter(DSC) and polarized optical microscope (POM). The crystallization half‐time t1/2, crystallization peak time tmax, and the Avrami crystallization rate constant Kn showed that the nanosilicate layers accelerate the overall crystallization rate greatly due to the nucleation effect, and the crystallization rate was increased with the increase in MMT content. Meanwhile, the crystallinity of PP in nanocomposites decreased with the increase in clay content which indicated the PP chains were confined by the nanosilicate layers during the crystallization process. Although the well‐dispersed silicate layers did not have much influence on spherulites growth rate, the nucleation rate and the nuclei density increased significantly. Accordingly, the spherulite size decreased with the increase in MMT content. © 2009 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 47: 2215–2225, 2009  相似文献   

10.
Triblock copolymers of poly(styrenesulfonate)‐b‐poly(ethylene glycol)‐b‐poly(styrenesulfonate) with narrow molecular weight distribution (Mw/Mn = 1.28–1.40) and well‐defined structure have been synthesized in aqueous solution at 70 °C via reversible addition‐fragmentation chain transfer polymerization. Poly(ethylene glycol) (PEG) capped with 4‐cyanopentanoic acid dithiobenzoate end groups was used as the macro chain transfer agent (PEG macro‐CTA) for sole monomer sodium 4‐styrenesulfonate. The reaction was controllable and displayed living polymerization characteristics and the triblock copolymer had designed molecular weight. The reaction rate depended strongly on the CTA and initiator concentration ratio [CTA]0/[ACPA]0: an increase in [CTA]0/[ACPA]0 from 1.0 to 5.0 slowed down the polymerization rate and improved the molecular weight distribution with a prolonged induction time. The polymerization proceeded, following first‐order kinetics when [CTA]0/[ACPA]0 = 2.5 and 5.0. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 3698–3706, 2007  相似文献   

11.
The soluble poly(methyl methacrylate‐co‐octavinyl‐polyhedral oligomeric silsesquioxane) (PMMA–POSS) hybrid nanocomposites with improved Tg and high thermal stability were synthesized by common free radical polymerization and characterized using FTIR, high‐resolution 1H NMR, 29Si NMR, GPC, DSC, and TGA. The POSS contents in the nanocomposites were determined based on FTIR spectrum, revealing that it can be effectively adjusted by varying the feed ratio of POSS in the hybrid composites. On the basis of the 1H NMR analysis, the number of the reacted vinyl groups on each POSS molecules was determined to be about 6–8. The DSC and TGA measurements indicated that the hybrid nanocomposites had higher Tg and better thermal properties than the pure PMMA homopolymer. The Tg increase mechanism was investigated using FTIR, displaying that the dipole–dipole interaction between PMMA and POSS also plays very important role to the Tg improvement besides the molecular motion hindrance from the hybrid structure. The thermal stability enhances with increase of POSS content, which is mainly attributed to the incorporation of nanoscale inorganic POSS uniformly dispersed at molecular level. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 5308–5317, 2007  相似文献   

12.
Graphene‐based nanocomposites with conducting polymers have attracted increasing interest due to the enhanced synergistic properties, which can potentiate and broaden applications. In this context, covalent functionalization stands out as a strategic designing tool, which optimizes the interaction between the nanocomposites components. Herein, covalently linked polymeric nanocomposites were obtained between graphene derivatives and polypyrrole (Ppy) under mild routes (i.e., aqueous, room temperature). First, pyrrole was covalently functionalized on graphene oxide (GO) through stable amide bonds and further polymerization with FeCl3 led to the polymeric nanocomposites. Finally, to improve conductivity, GO was reduced using NaBH4. Similarly, analogous non‐covalent nanocomposites were obtained for comparison purposes. All samples were thoroughly characterized by thermogravimetric analysis, scanning electron microscopy, and infrared and Raman spectroscopy, confirming the targeted functionalization, polymerization, and reduction processes. Moreover, the covalent link effectively enhances the interaction of the nanocomposite's components as evidenced by its improved electrochemical stability (300 cycles), compared to the non‐covalent composites which loses conductivity in the initial stages. Indeed, Ppy is known for its low stability, limiting its applications. Overall, the results herein evidence that covalently linked nanocomposites can be successfully obtained with optimized electrochemical response, promising for applications as supercapacitors and artificial muscles. © 2018 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2018 , 56, 579–588  相似文献   

13.
A new family of thermoplastic nanocomposites based on isotactic polypropylene (iPP) and inorganic fullerene‐like tungsten disulfide (IF‐WS2) has been successfully prepared. A very efficient dispersion of IF‐WS2 material was obtained by mixing in the melted polymer without using modifiers or surfactants. The addition of IF‐WS2 nanoparticles induces a remarkable enhancement of the thermal stability of iPP, as well as an increase in the crystallization rate of the matrix when compared with pure iPP. The nucleating efficiency of IF‐WS2 solid lubricant nanoparticles on the α‐phase of iPP reaches very high values (60–70%), the highest values observed hitherto for polypropylene nanocomposites. The incorporation of IF‐WS2 has also been observed to increase the size and stability of the crystals formed. The melting behavior of the nanocomposites indicates the formation of more perfect crystals as determined by differential scanning calorimetry and time‐resolved synchrotron X‐ray scattering experiments. The new nanocomposites show an increase in the storage modulus with respect to pure iPP measured by dynamic mechanical analysis. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 45: 2309–2321, 2007  相似文献   

14.
Pyrrolyl‐capped poly(N‐isopropylacrylamide) macromonomers (Py‐PNIPAM) were prepared through reversible addition‐fragmentation‐transfer polymerization with benzyl 1‐pyrrolylcarbodithioate as chain‐transfer agent. Polymerizations of Py‐PNIPAM with/without pyrrole using AgNO3 as oxidizing agent and dimethylforamide as solvent resulted in graft copolymers of polypyrrole‐graft‐poly(N‐isopropylacrylamide) (PPy‐g‐PNIPAM) as well as silver nanoparticles, leading to the formation of PPy‐g‐PNIPAM/silver nanocomposites. The resulting nanocomposites were soluble in water when the content of PPy was low, and when the molar ratio of Py/Py‐PNIPAM increased to 30, the resulting products became insoluble in water. The resulting nanocomposites had special optical properties because of PPy as well as the temperature‐responsible PNIPAM. The chemical structure and composition of nanocomposite were characterized by 1H nuclear magnetic resonance spectroscopy, gel permeation chromatograms, fourier transform infrared spectroscopy, and X‐ray diffraction. Their optical properties were characterized by UV–vis and fluorescence spectroscopy. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 6950–6960, 2008  相似文献   

15.
This work deals with the preparation of poly(urethane acrylates) by using two different polymerization techniques. Namely, the classical batch procedure has been compared with frontal polymerization (FP). A thorough study on the effect of initiator type, concentration, and on the velocity of the front and its maximum temperature has been carried out. Moreover, two different synthetic ways have been studied: the one step poly(urethane acrylate) preparation starting directly from 1,6 diisocyanato hexane and 2‐hydroxyethyl acrylate, and the two step procedure consisting of the synthesis of the corresponding diurethane diacrylate and of its subsequent polymerization. The first method has the advantage of being faster but some caution is necessary due to the excessive heat that is generated if the reaction conditions are not properly chosen. The second approach requires a further step but has the advantage of being more controlled. DSC analysis did not show any significant difference by comparing the thermal properties of the materials obtained by the two techniques (batch and FP). However, since FP runs are very easy and fast to be performed, FP should be seriously taken into proper account when these materials have to be prepared. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 3344–3352, 2008  相似文献   

16.
The reaction of phenyl propynyl ether and diphenyl disulfide in the presence of 1 mol % tetrakis(triphenylphosphine)palladium as a model reaction of the polymerization of bis(4‐prop‐2‐ynyloxyphenyl) disulfide ( 1a ) gave a Z‐substituted dithioalkene. No E‐substituted dithioalkene was formed in this reaction. The palladium‐catalyzed bisthiolation polymerization of a diethynyl disulfide derivative, 1a , in benzene, was carried out to give a hyperbranched polymer ( 5a ) containing a Z‐substituted dithioalkene unit after reaction for 4 h at 70 °C. From the gel permeation chromatography analysis (chloroform, PSt standards), the number‐average and weight‐average molecular weights of 5a were found to be 8,100 and 57,000, respectively. The structure of 5a was confirmed by 1H and 13C NMR spectra. The obtained polymer was soluble in common organic solvents such as benzene, acetone, and CHCl3. Polymerization for more than 5 h gave insoluble products. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 3580–3587, 2007  相似文献   

17.
Double‐hydrophilic in‐chain functionalized macromonomers consisting of poly(N‐isopropylacrylamide) (PNIPAM) and poly(ethylene oxide) were prepared by a multistep procedure including esterification of PNIPAM monoester of maleic acid with α‐methoxy‐ω‐hydroxypolyoxyethylene or its amidation with α‐methoxy‐ω‐aminopolyoxyethylene. The polymerization of the macromonomers was carried out in aqueous solutions. The temperature was the key parameter controlling the polymerization process that was performed in the organized domains formed by the macromonomers below and above the phase transition temperature (Ttr). Polymacromonomers with higher degrees of polymerization were prepared at temperatures just below the Ttr. Static light scattering measurements on dilute aqueous solutions of thermally‐responsive macromonomers and their polymerization products demonstrated that they formed aggregates below the Ttr. Supramolecular structures with low density cores, formed by the polymacromonomers at room temperature, were imaged by SEM. Morphological tuning was achieved by varying both the composition of the copolymer and the concentration of the aqueous solution. The rheological behavior of the polymacromonomers in 25 wt % aqueous solution was compared to that of the respective macromonomers. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 4720–4732, 2007  相似文献   

18.
This study describes the preparation of nanocomposites fabricated from monodispersed iron oxide (Fe3O4) and polypyrrole (PPy) by in situ chemical oxidative polymerization. The monodispersed 4 nm Fe3O4 nanoparticles which served as cores were synthesized using the thermal decomposition of a mixture of Iron (III) acetylacetonate and oleic acid in the presence of high boiling point solvents. The resulting nanoparticles were further dispersed in an aqueous solution with anionic surfactant sodium bis(2‐ethylhexyl) sulfosuccinate to form micelle/Fe3O4 spherical templates that avoid the aggregation of Fe3O4 nanoparticles during the further preparation of the nanocomposites. The Fe3O4/PPy nanocomposites were then synthesized via in situ chemical oxidative polymerization on the surface of the spherical templates. Both field‐emission scanning electron microscopy (FESEM) and high‐resolution transmission electron microscopy (HRTEM) images indicate that the resulting Fe3O4 nanoparticles are close to spherical dots with a particle size of about 4 nm and a standard deviation of less than 5% (4 ± 0.2 nm). Structural and morphological analysis using FESEM and HRTEM showed that the fabricated Fe3O4/PPy nanocomposites are core (Fe3O4)‐shell (PPy) structures. Morphology of the nanocomposites shows a remarkable change from spherical to tube‐like structures as the content of monodispersed Fe3O4 nanoparticles increases from 9% up to 24 wt %. The conductivities of these Fe3O4/PPy nanocomposites are about six times higher than those of PPy without Fe3O4. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 4647–4655, 2007  相似文献   

19.
Frontal polymerization (FP) has been used as an alternative technique for the preparation of poly(N,N‐dimethylacrylamide) hydrogels. Samples were synthesized in bulk, water, or dimethyl sulfoxide (DMSO), and the obtained materials were characterized and compared in terms of their yield, swelling behavior, thermal properties, and morphology. It was found that their features are dependent on the presence and type of the solvent used. Samples prepared in bulk are characterized by the lowest yields and the highest front temperatures (Tmax) and velocities (Vf), whereas those synthesized in water have the highest yields and the lowest values of Tmax and Vf. No significant differences have been found in terms of Tg among the three series of samples. By contrast, the reaction conditions influenced the porous morphology of the samples and, consequently, their swelling capability in water. The swelling ratio ranges from about 670–700% for some samples prepared in water up to 3500% for a sample obtained in DMSO, thus indicating that this parameter can be properly tuned by using the most suitable FP conditions. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 1422–1428, 2009  相似文献   

20.
Combination of coordination polymerization and atom transfer radical polymerization (ATRP) was applied to a novel synthesis of rod‐coil block copolymers. The procedure included the following steps: (1) monoesterification reaction of ethylene glycol with 2‐bromoisobutyryl bromide yielded a α‐bromo, ω‐hydroxy bifunctional initiator, (2) CpTiCl3 (bifunctional initiator) catalyst was prepared from a mixture of trichlorocyclopentadienyl titanium (CpTiCl3) and bifunctional initiator. Coordination polymerization of n‐butyl isocyanate initiated by such catalyst provided a well‐defined macroinitiator, poly(n‐butyl isocyanate)‐Br (PBIC‐Br), and (3) ATRP method of vinyl monomers using PBIC‐Br provided rod (PBIC)‐coil block copolymers. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 4037–4042, 2007  相似文献   