 共查询到20条相似文献,搜索用时 78 毫秒
1.
An anti-Stokes luminescence band with λmax = 515 nm of microcrystals of solid AgCl0.95I0.05 solutions excited by a radiation flux of density 1013–1015 quanta/cm2·sec in the range 600–800 nm at 77 K was detected. It is shown that the intensity of this luminescence and the frequency of its excitation depend on the prior UV-irradiation of samples. Analysis of the stimulated-photoluminescence spectra and the anti-Stokes luminescence excitation spectra of the indicated microcrystals has shown that to the centers of anti-Stokes luminescence excitation correspond local levels in the forbidden band of the crystals. These states are apparently due to the atomic and molecular disperse silver particles that can be inherent in character or formed as a result of a low-temperature photochemical process. __________ Translated from Zhurnal Prikladnoi Spektroskopii, Vol. 72, No. 6, pp. 738–742, November–December, 2005.  相似文献   

2.
The photoluminescence and photoexcitation spectra as well as the luminescence decay kinetics of Er3+ ions in the visible ultraviolet and vacuum ultraviolet (VUV) regions have been studied by the method of low-temperature, time-resolved VUV-spectroscopy on excitation by synchrotron radiation. In the VUV spectral region of the luminescence of SrF2:1% Er3+, the 146.5-nm band with a time of decay of less than 0.6 nsec was revealed together with the well-known emission band at 164.3 nm (decay constant in the microsecond range). Its possible nature is discussed. The specific features of the formation of photoexcitation spectra of the f-f and f-d transitions in the Er3+ ion are considered. Competition between the processes of excitation of f-f and d-f luminescence has been revealed. It manifests itself in the inverse relationship of their photoexcitation spectra in a range of energies of incident photons that are close to the position of the 4fn−15d configuration levels. __________ Translated from Zhurnal Prikladnoi Spektroskopii, Vol. 72, No. 4, pp. 519–523, July–August, 2005.  相似文献   

3.
It has been shown using atomic-force microscopy that the PbI2 impurity is embedded in the CdI2 crystal lattice in the form of nanocrystalline inclusions. The model of a high-energy cation exciton related to the 3 P 2 state of a free Pb2+ ion has been considered for the impurity absorption (excitation) band at 3.23 eV. The resonance narrow photoluminescence bands with the split absorption band at 3.12 and 3.20 eV have been compared with the emission of a free Frenkel exciton. It has been demonstrated that, in the temperature range 25–45 K, there arises a self-trapped exciton state, and the main role in its formation is played by the bending vibrations of the CdI2 crystal lattice. The potential barrier separating the self-trapped state from the free exciton is 23 meV. The photoluminescence band at 2.4 eV is assigned to the emission of the self-trapped high-energy cation exciton of PbI2 in the CdI2 crystal lattice.  相似文献   

4.
We present the characteristics of an optical parametric oscillator based on a KTP crystal, pumped with noncritical phase matching by a pulsed Ti3+:Al2O3 laser, tunable in the range 677–970 nm. Tunable generation of signal and idler waves is obtained in the ranges 1030–1390 nm and 2690–3050 nm respectively. The efficiency of conversion of the pump to the signal wave is ≈23%, which for pulses of duration ≈8 nsec ensures an energy in the range 1.0–11.5 mJ. The width of the emission spectrum for the signal wave is within the range 0.8–1.8 nm and is predominantly determined by the linewidth of the Ti3+:Al2O3 pump laser. __________ Translated from Zhurnal Prikladnoi Spektroskopii, Vol. 74, No. 3, pp. 351–356, May–June, 2007.  相似文献   

5.
The luminescence and thermally stimulated recombination processes in lithium borate crystals Li6Gd(BO3)3 and Li6Gd(BO3)3:Ce have been studied. The steady-state luminescence spectra under X-ray excitation (X-ray luminescence), temperature dependences of the intensity of steady-state X-ray luminescence (XL), and thermally stimulated luminescence (TSL) spectra of these compounds have been investigated in the temperature range of 90–500 K. The intrinsic-luminescence 312-nm band, which is due to the 6 P J 8 S 7/2 transitions in Gd3+ matrix ions, dominates in the X-ray luminescence spectra of these crystals; in addition, there is a wide complex band at 400–420 nm, which is due to the d → f transitions in Ce3+ impurity ions. It is found that the steady-state XL intensity in these bands increases several times upon heating from 100 to 400 K. The possible mechanisms of the observed temperature dependence of the steady-state XL intensity and their correlation with the features of electronic-excitation energy transfer in these crystals are discussed. The main complex TSL peak at 110–160 K and a number of minor peaks, whose composition and structure depend on the crystal type, have been found in all crystals studied. The nature of the shallow traps that are responsible for TSL at temperatures below room temperature and their relation with defects in the lithium cation sublattice are discussed.  相似文献   

6.
Single crystals of gadolinium orthosilicate Gd2SiO5 containing 0.5 at% and 5 at% of Sm3+ were grown by the Czochralski method. Optical absorption spectra, luminescence spectra and luminescence decay curves were recorded for these systems at 10 K and at room temperature. Comparison of optical spectra recorded in polarized light revealed that the anisotropy of this optically biaxial host affects the intensity distribution within absorption and emission bands related to transitions between multiplets rather than the overall band intensity. It has been found that among four bands of luminescence related to the 4G5/26HJ (J=5/2–11/2) transitions of Sm3+ in the visible and near infrared region the 4G5/26H7/2 one has the highest intensity with a peak emission cross section of 3.54×10−21 cm2 at 601 nm for light polarized parallel to the crystallographic axis c of the crystal. The luminescence decay curve recorded for Gd2SiO5:0.5 at% Sm3+ follows a single exponential time dependence with a lifetime 1.74 ms, in good agreement with the 4G5/2 radiative lifetime τ rad=1.78 ms calculated in the framework of Judd-Ofelt theory. Considerably faster and non-exponential luminescence decay recorded for Gd2SiO5:5 at% Sm3+ sample was fitted to that predicted by the Inokuti-Hirayama theory yielding the microparameter of Sm3+–Sm3+ energy transfer C da=1.264×10−52 cm6×s−1.  相似文献   

7.
The absorption spectra and photo-and dark conductivity of the CdI2-PbI2 system are investigated in the temperature range 4.2–300 K. The temperature dependence of the photoluminescence and the IR stimulation spectra of luminescence and induced photoconductivity at 4.2 K are also studied. The results are interpreted by considering microphase inclusions of PbI2 into the CdI2 crystal lattice as activator centers. An energy-level diagram in which the narrow band of the PbI2 microphase genetically related to the metastable 3P0 level of lead plays a significant role is presented for this crystal system.  相似文献   

8.
We present the results of studying the luminescence properties of transparent ceramics Y3Al5O12:Yb obtained by the vacuum sintering and nanocrystalline technology. In the course of research, we measured the luminescence and luminescence excitation spectra, as well as the temperature and kinetic behavior of luminescence. Our results are analyzed in comparison with the characteristics of corresponding single crystals. We revealed that processes of generation and relaxation of electronic excitations that occur in ceramics, in particular, in the charge transfer state, are similar to processes occurring in crystals. The behavior of two charge-transfer luminescence bands at 340 and 490 nm is studied. In the range 300–600 nm, we revealed a broad emission band of radiation of other type, which is also observed in spectra of undoped ceramics. This broad band is attributed to F+ centers. Emission and excitation spectra of charge transfer luminescence at a maximum of the temperature dependence of 100 K are measured for the first time. We found that, upon excitation in the charge transfer band, luminescence in ceramics is more intense than in single crystals with similar concentrations of Yb and has a higher quenching temperature.  相似文献   

9.
This paper reports on a study of the dynamics of electronic excitations in KBe2BO3F2 (KBBF) crystals by low-temperature luminescent vacuum ultraviolet spectroscopy with nanosecond time resolution under photoexcitation by synchrotron radiation. The first data have been obtained on the kinetics of photoluminescence (PL) decay, time-resolved PL spectra, time-resolved PL excitation spectra, and reflection spectra at 7 K; the estimation has been performed for the band gap E g = 10.6−11.0 eV; the predominantly excitonic mechanism for PL excitation at 3.88 eV has been identified; and defect luminescence bands at 3.03 and 4.30 eV have been revealed. The channels of generation and decay of electronic excitations in KBBF crystals have been discussed.  相似文献   

10.
Results of comprehensive research into optical and luminescent-kinetic characteristics of europium-doped cadmium iodide crystals excited by nitrogen laser radiation, α-particles, and x-rays are presented. Crystals under study have been grown by the Bridgman–Stockbarger method. The doping EuCl3 admixture was introduced into the charge in quantities of about 0.05 and 1.0 mol%. Impurity absorption detected in the near-edge region of the crystals is interpreted as part of the Eu2+ ion long-wavelength band associated with fd-transitions. The cation impurity and matrix defects in CdI2:Eu2+ crystals create complex centers responsible for emission with a maximum in the 580–600-nm region. The short component in the luminescence decay kinetics of weakly-doped crystal excited by α-particles and x-ray photons is due to the exciton emission characteristic of CdI2. The slow component in the scintillation pulse results from recombination of charge carriers followed by creation of exciton-like states on the defect-impurity centers. Laser or x-ray excitation induces light-sum accumulation on the trapping levels at a depth of 0.2–0.6 eV that is mainly related to matrix microdefects. Trapping centers associated with the chlorine impurity are observed in the heavily-doped crystal. Photostimulated luminescence at 85 K arising at the electron stage of the recombination process is caused by recombination of electrons released from F-type centers with holes localized near the activator. Translated from Zhurnal Prikladnoi Spektroskopii, Vol. 76, No. 3, pp. 358–364, May–June, 2009.  相似文献   

11.
Thin films of M2CdI4 ferroelectrics (M=Cs, Rb) of orthorhombic structure were synthesized, and their electronic optical spectrum was studied. It was established that both compounds belong to direct-gap dielectrics and that their low-frequency excitons are localized on a sublattice made up of (CdI4)2? tetrahedra. The temperature dependence of the exciton band parameters was studied for Cs2CdI4 within the temperature interval 90–420 K. The phase transitions occurring in this interval manifest themselves as breaks in the temperature behavior of the band spectral positions and weak peaks in the halfwidth and oscillator strength.  相似文献   

12.
The exciton absorption spectra of thin films of (Cs1 − x Rb x )2CdI4 solid solutions have been investigated and the refractive index n(λ) in their transparency window in the concentration range of 0 ≤ x ≤ 1 has been measured. The exciton-band parameters and optical permittivity ɛ(x) have been found to linearly depend on the concentration. It is established that excitons are incorporated into the CdI2 sublattice of the solid solutions and belong to intermediate-coupling ones. The characteristics of excitons in ferroelastics are compared with the corresponding parameters for CdI2, RbI, and CsI, which are used as components to synthesize ternary compounds.  相似文献   

13.
The thermally stimulated recombination processes and luminescence in crystals of the lithium borate family Li6(Y,Gd,Eu)(BO3)3 have been investigated. The steady-state luminescence spectra under X-ray excitation (X-ray luminescence spectra), the temperature dependences of the X-ray luminescence intensity, and the glow curves for the Li6Gd(BO3)3, Li6Eu(BO3)3, Li6Y0.5Gd0.5(BO3)3: Eu, and Li6Gd(BO3)3: Eu compounds have been measured in the temperature range 90–500 K. In the X-ray luminescence spectra, the band at 312 nm corresponding to the 6 P J 8 S 7/2 transitions in the Gd3+ ion and the group of lines at 580–700 nm due to the 5 D 07 F J transitions (J = 0–4) in the Eu3+ ion are dominant. For undoped crystals, the X-ray luminescence intensity of these bands increases by a factor of 15 with a change in the temperature from 100 to 400 K. The possible mechanisms providing the observed temperature dependence of the intensity and their relation to the specific features of energy transfer of electronic excitations in these crystals have been discussed. It has been revealed that the glow curves for all the crystals under investigation exhibit the main complex peak with the maximum at a temperature of 110–160 K and a number of weaker peaks with the composition and structure dependent on the crystal type. The nature of shallow trapping centers responsible for the thermally stimulated luminescence in the range below room temperature and their relation to defects in the lithium cation sublattice have been analyzed.  相似文献   

14.
The luminescence of excitons and antisite defects (ADs) was investigated, as well as the specific features of the excitation energy transfer from excitons and ADs to the activator (Ce3+ ion) in phosphors based on Lu3Al5O12:Ce (LuAG:Ce) single crystals and single-crystalline films, which are characterized by significantly different concentrations of ADs of the Lu Al 3+ type and vacancy-type defects. The luminescence band with λmax = 249 nm in LuAG:Ce single-crystal films is due to the luminescence of self-trapped excitons (STEs) at regular sites of the garnet lattice. The excited state of STEs is characterized by the presence of two radiative levels with significantly different transition probabilities, which is responsible for the presence of two excitation bands with λmax = 160 and 167 nm and two components (fast and slow) in the decay kinetics of the STE luminescence. In LuAG:Ce single crystals, in contrast to single-crystal films, the radiative relaxation of STEs in the band with λmax = 253.5 nm occurs predominantly near Lu Al 3+ ADs. The intrinsic luminescence of LuAG:Ce single crystals at 300 K in the band with λmax = 325 nm (τ = 540 ns), which is excited in the band with λmax = 175 nm, is due to the radiative recombination of electrons with holes localized near Lu Al 3+ ADs. In LuAG:Ce single crystals, the excitation of the luminescence of Ce3+ ions occurs to a large extent with the participation of ADs. As a result, slow components are present in the luminescence decay of Ce3+ ions in LuAG:Ce single crystals due to both the reabsorption of the UV AD luminescence in the 4f-5d absorption band of Ce3+ ions with λmax = 340 nm and the intermediate localization of charge carriers at ADs and vacancy-type defects. In contrast to single crystals, in phosphors based on LuAG:Ce single-crystal films, the contribution of slow components to the luminescence of Ce3+ ions is significantly smaller due to a low concentration of these types of defects.  相似文献   

15.
A method has been proposed to analyze the dynamics of interband two-photon absorption in a nonlinear medium excited by a sequence of picosecond laser pulses of variable intensity and continuous probe radiation. Induced absorption leading both to hysteresis in the dependence of the absorption on the intensity of laser pump radiation and to the opacity of crystals at the pump wavelength has been revealed in initially transparent ZnWO4 and PbWO4 crystals irradiated by a train of 523.5-nm pulses with a duration of 20 ps at pump intensities of 5 to 140 GW/cm2. The kinetics of an increase in absorption and its subsequent relaxation at a 523.5-nm picosecond excitation of the crystals have been measured with continuous 633-nm probe radiation. An exponential component of the increase in absorption with the time constant τ = 2−3.5 and 8–9.5 μs depending on the direction of the linear polarization of pump radiation has been revealed at 300 K in ZnWO4 and PbWO4 crystals, respectively. The absorption relaxation kinetics in the crystals are complicated and approach an exponential at a late stage with the constant τ = 40−130 and 12–80 ms for the ZnWO4 and PbWO4 crystals, respectively.  相似文献   

16.
The effect of a strong magnetic field (induction up to 10 T) on free and bound excitons in CuInS2 single crystals is studied. A diamagnetic shift to higher energies is observed in the luminescence and reflectance spectra for free-exciton lines ALPB ≈ 1.5348 eV, AUPB ≈ 1.5361 eV, and BC ≈ 1.557 eV. The diamagnetic shifts of free-exciton lines ALPB, AUPB, and BC provide a basis for estimating the exciton reduced masses = 0.131m0, = 0.13 4m0, and μBC = 0.111m0, respectively. Bound-exciton lines in luminescence spectra are split under the influence of the magnetic field. The magnitude of the Zeeman effect (g-factor of the magnetic splitting) is estimated. __________ Translated from Zhurnal Prikladnoi Spektroskopii Vol. 74, No. 3, pp. 373–377, May–June, 2007.  相似文献   

17.
We have studied photoluminescence and thermoluminescence (PL and TL) in CaGa2Se4:Eu crystals in the temperature range 77–400 K. We have established that broadband photoluminescence with maximum at 571 nm is due to intracenter transitions 4f6 5d–4f7 (8S7/2) of the Eu2+ ions. From the temperature dependence of the intensity (log I–103/T), we determined the activation energy (E a = 0.04 eV) for thermal quenching of photoluminescence. From the thermoluminescence spectra, we determined the trap depths: 0.31, 0.44, 0.53, 0.59 eV. The lifetime of the excited state 4f6 5d of the Eu2+ ions in the CaGa2Se4 crystal found from the luminescence decay kinetics is 3.8 μsec. Translated from Zhurnal Prikladnoi Spektroskopii, Vol. 76, No. 1, pp. 112–116, January–February, 2009.  相似文献   

18.
This paper reports on a study of the luminescence emitted by Li6Gd(BO3)3: Ce3+ crystals under selective photoexcitation to lower excited states of the host ion Gd3+ and impurity ion Ce3+ within the 100–500-K temperature interval, where the mechanisms of migration and relaxation of electronic excitation energy have been shown to undergo noticeable changes. The monotonic 10–15-fold increase in intensity of the luminescence band at 3.97 eV has been explained within a model describing two competing processes, namely, migration of electronic excitation energy over chains of Gd3+ ions and vibrational energy relaxation between the 6 I j and 6 P j levels. It has been shown that radiative transitions in Ce3+ ions from the lower excited state 5d 1 to 2 F 5/2 and 2 F 7/2 levels of the ground state produce two photoluminescence bands, at 2.08 and 2.38 eV (Ce1 center) and 2.88 and 3.13 eV (Ce2 center). Possible models of the Ce1 and Ce2 luminescence centers have been discussed.  相似文献   

19.
This paper reports on the results of the comprehensive study of the dynamics of electronic excitations in K2Al2B2O7 (KABO) crystals, obtained by low-temperature luminescence vacuum ultraviolet spectroscopy with nanosecond time resolution upon photoexcitation by synchrotron radiation. For the first time, the data have been obtained on the photoluminescence (PL) decay kinetics, PL spectra with time resolution, PL excitation spectra with time resolution, and reflection spectra at 7 K; the intrinsic nature of PL at 3.28 eV has been established; luminescence bands of defects have been separated in the visible and ultraviolet spectral regions; an intense long-wavelength PL band has been detected at 1.72 eV; channels of the formation and decay of electronic excitations in K2Al2B2O7 crystals have been discussed.  相似文献   

20.
The absorption spectrum of thin films of a new compound, K2CdI4, was studied. It was established that this compound belongs to direct-bandgap dielectrics and that its low-frequency electronic and excitonic excitations are localized in CdI 4 2? structural blocks of the crystal lattice. It was found that, in M2CdI4 compounds (M = K, Rb, Cs), the bandgap width E g grows and the spin-orbit splitting of the valence band top decreases with increasing ionic radius of the alkali metal.  相似文献   