首页 | 本学科首页   官方微博 | 高级检索  
     

Synthesis of Polyacrylaminothiourea Chelating Fiber and Properties of Concentration and Separation of Trace Noble Metal Ions from Samples
引用本文:GONG,Bo-Lin SUN,Yan-Pb 等. Synthesis of Polyacrylaminothiourea Chelating Fiber and Properties of Concentration and Separation of Trace Noble Metal Ions from Samples[J]. 中国化学, 2002, 20(1): 63-67. DOI: 10.1002/cjoc.20020200113
作者姓名:GONG,Bo-Lin SUN,Yan-Pb 等
作者单位:[1]InstituteofModernSeparationScience,NorthwestUniversity,Xi′an,Shannxi710069,China [2]DepartmentofChemistry,NingxiaUniversity,Yinchuan,Ningxia750021,China
基金项目:theNaturalScienceFoundationofNingxia ,China (No .199912 )andtheScienceCommitteeFoundationofNingx ia ,China
摘    要:A novel polyacrylaminothiourea chelating fiber was synthesized simply and rapidly from nitrilon (an acrylonitrile-based synthetic fiber), which was applied to preconcentrate and separate of trace amount of Au(Ⅲ),Pt(Ⅳ),Pd(Ⅳ) and Ir (Ⅳ) ions from solution of samples.The analyzed ions can be quantitatively concentrated by the fiber up to a flow rate of 20.0mL/min at pH2, and can also be desorbed with 15 mL of 4mol/L HCl 3% thiourea from the fiber column with recoveries of 96.5%-100%.The chelating fiber can be reused for ten times,the recoveries of these ions are still over 92%,and hundred to thousand times of excess of Fe(Ⅲ),Al(Ⅲ),Ca(Ⅱ),Mg(Ⅱ),Ni(Ⅱ),Mn(Ⅱ),Cu(Ⅱ),Zn(Ⅱ),and Cd(Ⅱ) cause no interference on the determination of the analyzed ions by inductively-coupled plasma atomic emission spectrometry (ICP-AES).The static saturation adsorption capacities of the fiber for the analytes are in the range of 1.15-2.80mmol/g.The relative standard deviations for the determination of 20.0ng/mL each of Au(Ⅲ),Pt(Ⅳ),Pd(Ⅳ)and Ir(Ⅳ) are in the range of 0.7%-3.0%.The recoveries for test from standard additions to real solution samples are between 96% and 100%.The concentration of each ion in powder sample detected by the method is in good agreement with the certified value.

关 键 词:合成 聚合烯氨基硫脲 螯合纤维 浓缩 分离 痕量贵金属离子

Synthesis of Polyacrylaminothiourea Chelating Fiber and Properties of Concentration and Separation of Trace Noble Metal Ions from Samples
GONG,Bo-Lin WANG,Yan SUN,Yan-Pu Zhao,Jian-Guo a a Institute of Modern Separation Science,Northwest University,Xi'an,Shannxi ,China b. Synthesis of Polyacrylaminothiourea Chelating Fiber and Properties of Concentration and Separation of Trace Noble Metal Ions from Samples[J]. Chinese Journal of Chemistry, 2002, 20(1): 63-67. DOI: 10.1002/cjoc.20020200113
Authors:GONG  Bo-Lin WANG  Yan SUN  Yan-Pu Zhao  Jian-Guo a a Institute of Modern Separation Science  Northwest University  Xi'an  Shannxi   China b
Affiliation:GONG,Bo-Lin WANG,Yan SUN,Yan-Pu Zhao,Jian-Guo a a Institute of Modern Separation Science,Northwest University,Xi'an,Shannxi 710069,China b Department of Chemistry,Ningxia University,Yinchuan,Ningxia 750021,China
Abstract:A novel polyacrylaminothiourea chelating fiber was synthesized simply and rapidly from nitrilon (an acrylonitrile-based synthetic fiber), which was applied to preconcentrate and separate of trace amount of Au(III), Pt(IV), Pd(IV) and Ir(IV) ions from solution of samples. The analyzed ions can be quantitatively concentrated by the fiber up to a flow rate of 20.0 mL/min at pH 2, and can also be desorbed with 15 mL of 4 mol/L HCl+3% thiourea from the fiber column with recoveries of 96.5%-100%. The chelating fiber can be reused for ten times, the recoveries of these ions are still over 92%, and hundred to thousand times of excess of Fe(III), Al(III), Ca(II), Mg(II), Ni(II), Mn(II), Cu(II), Zn(II), and Cd(II) cause no interference on the determination of the analyzed ions by inductively-coupled plasma atomic emission spectrometry (ICP-AES). The static saturation adsorption capacities of the fiber for the analytes are in the range of 1 15-2 80 mmol/g. The relative standard deviations for the determination of 20.0 ng/mL each of Au(III), Pt(IV), Pd(IV) and Ir(IV) are in the range of 0.7%-3.0%. The recoveries for test from standard additions to real solution samples are between 96% and 100%. The concentration of each ion in powder sample detected by the method is in good agreement with the certified value.
Keywords:concentration   separation   polyacrylacylamino~thiourea chelating fiber   gold   platinum   palladium   iridium