Specific swelling behaviors of poly(4-vinyl phenol) gels in tetraalkylammonium chloride solutions
Authors:Xu Ling  Yokoyama Eisuke  Watando Hiroko  Okuda-Fukui Rei  Kawauchi Susumu  Satoh Mitsuru
Institution:Department of Chemistry and Materials Science, Tokyo Institute of Technology, 2-12-1 Ookayama, Meguro-ku, Tokyo 152-0033, Japan.
Abstract:Swelling behaviors of poly(4-vinyl phenol) (P4VPh) gel in aqueous tetraalkylammonium chloride (TAACl) solutions were investigated to find a very specific swelling behavior. Especially for the tetrabutylammonium chloride (TBACl) system, P4VPh gel remarkably deswelled with increasing salt concentration (/= ca. 2.1 M). A similar swelling profile was also observed in the swelling time-course; upon immersion of a water-swollen P4VPh gel into 2.5 M TBACl solution, the gel first deswelled in an early stage (approximately 0.1 h) and then remarkably reswelled with time. Relative amounts (mol/mol) of TBA cation and water per monomer residue were estimated as ca. 1 and 0 for the deswollen state and 5 and 50 for the reswollen state, respectively. This result, together with those of attenuated total reflection Fourier transform infrared measurements performed for the gels swollen in various kinds of TAACl and inorganic salt solutions, suggested that in the highly deswollen and almost dehydrated state, phenol rings aggregated with intervening TBA cations, while the aggregation reswelled upon further binding with TBA cations.
Keywords:
本文献已被 PubMed 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号