Abstract: | Blends of poly(ethylene- co-5.4 mol% 3,5,5-trimethylhexyl methacrylate) (PE-TMHM) with poly(dimethylsiloxane) (PDMS) were prepared in the PDMS content range from 0 to 20%. The miscibility was studied for PE-TMHM–PDMS blends by DSC, dynamic mechanical and microscopic spectroscopy, and the gas permeability was measured for O2, N2 and CO2 as function of PDMS content. PE-TMHM and PDMS were partially miscible with each other below 20 wt% of PDMS content. The permeability coefficients (P) for O2, N2 and CO2 were increased by the blending of PDMS to PE-TMHM. The change of P for O2 with PDMS content well reflected the partially miscible phase separation behavior. Received: 10 June 1996 Accepted: 14 August 1996 |
| |
Keywords: | Poly(ethylene-co-5.4 mol% 3 5 5-trimethylhexyl methacrythlate) poly(dimethyl-siloxane) miscibility permeability dynamic elastic measurement DSC |
本文献已被 SpringerLink 等数据库收录! |
|