Pd-Si Binary Bulk Metallic Glass Prepared at Low Cooling Rate |
| |
作者姓名: | 姚可夫 阮芳 |
| |
作者单位: | DivisionofEngineeringMaterials,DepartmentofMechanicalEngineering,TsinghuaUniversity,Beijing100084 |
| |
摘 要: | We report that binary bulk metallic glasses can be made up to 6ram in diameter in a Pd Si ahoy system by air cooling at slow cooling rate (about 8 K/s). The high stability of the undercooled liquid and the large glass-forming ability (GFA) of the binary alloy are contributed to the removing of heterogeneous impurities in the alloy melt by employing the fluxing technique. It has been found that decreasing cooling rate can increase the supercooled liquid region and thermal stability of the glassy alloy. After fluxing, a wider supercooled liquid region (△T = 58 K) and higher glass-forming ability have been obtained in a Pd81Si19 binary glassy alloy prepared by slow cooling rate.
|
关 键 词: | 钯-硅金属玻璃 低冷却率 热稳定性 稀释工艺 |