Identification of A- and B-site cation vacancy defects in perovskite oxide thin films
Authors:Keeble D J  Wicklein S  Dittmann R  Ravelli L  Mackie R A  Egger W
Institution:Carnegie Laboratory of Physics, School of Engineering, Physics, and Mathematics, University of Dundee, Dundee DD1 4HN, United Kingdom. d.j.keeble@dundee.ac.uk
Abstract:Cation vacancies on both sublattices (V(Ti), V(Sr)) have been identified in homoepitaxial pulsed laser deposited SrTiO3 films using high intensity variable energy positron annihilation lifetime spectroscopy (PALS) measurements. Film nonstoichiometry was varied by varying laser fluence. PALS showed that on increasing the fluence above the Ti/Sr~1 value, the concentration ratio V(Sr)]/V(Ti)] systematically increased. Reducing the fluence into the Ti-poor region below resulted in additional vacancy cluster defect formation. Vacancy concentrations greater than ~50 ppm were observed in all films.
Keywords:
本文献已被 PubMed 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号