Pyroxene inclusions in paleo-Christian mosaic tesserae: a new tool for constraining the glass manufacturing temperature
Authors:Tonietto  Serena  Nestola  Fabrizio  Redhammer  Gunther J  Silvestri  Alberta  Molin  Gianmario  Bruno  Marco
Institution:1.Dipartimento di Geoscienze, Università di Padova, Via Giotto 1, 35137, Padova, Italy
;2.Abteilung für Mineralogie, Fachbereich Materialwissenschaften & Physik, Universität Salzburg, Hellbrunnerstrasse 34, 5020, Salzburg, Austria
;3.Dipartimento di Scienze Mineralogiche e Petrologiche, Università di Torino, Via Valperga Caluso 35, 10125, Torino, Italy
;
Abstract:The mineral inclusions of two orange glass tesserae from paleo-Christian mosaics were investigated in order to derive the melting temperature reached during their production (sourced from Padua and Vicenza, Veneto region, Italy). In particular, clinopyroxene crystals were studied by single-crystal X-ray diffraction and electron microprobe WDS analysis. The crystals show C2/c symmetry, typical of disordered Ca/Na and Mg/Al distributions indicating high-temperature of formation (>700°C). The cation site populations were obtained by combining results from the two experimental techniques enabled us to derive the following stoichiometric formula:
lM2Ca0.819Na0.172Mn0.006K0.003]M1Mg0.765Fe3+0.210   Cu0.015Ti0.006Zn0.006]TSi1.933Al0.037Sn0.024]O6\begin{array}{l}{}^{M2}\mathrm{Ca}_{0.819}\mathrm{Na}_{0.172}\mathrm{Mn}_{0.006}\mathrm{K}_{0.003}]{}^{M1}\mathrm{Mg}_{0.765}\mathrm{Fe}^{3+}_{0.210}\\3pt]\quad{}\mathrm{Cu}_{0.015}\mathrm{Ti}_{0.006}\mathrm{Zn}_{0.006}]{}^{T}\mathrm{Si}_{1.933}\mathrm{Al}_{0.037}\mathrm{Sn}_{0.024}]\mathrm{O}_{6}\end{array}