Thermal explosion simulation and incompatible reaction of dicumyl peroxide by calorimetric technique
Authors:Sun-Ju Shen  Sheng-Hung Wu  Jen-Hao Chi  Yih-Wen Wang  Chi-Min Shu
Institution:(1) Department of Occupational Safety and Health, Chia Nan University of Pharmacy and Science, 60, Erh-Jen Rd., Sec. 1, Jente, Tainan, 71710, Taiwan, ROC;(2) Department of Fire Science, WuFeng Institute of Technology, 117, Chian-Kuo Rd., Sec. 2, Min-Hsiung, Chiayi, 62153, Taiwan, ROC;(3) Department of Occupational Safety and Health, Jen-Teh Junior College of Medicine, Nursing and Management, 1, Jen-Teh Rd., Houlong, Miaoli, 65601, Taiwan, ROC;(4) Graduate School of Engineering Science and Technology, National Yunlin University of Science and Technology (NYUST), 123, University Rd., Sec. 3, Douliou, Yunlin, 64002, Taiwan, ROC;
Abstract:Dicumyl peroxide (DCPO) is usually employed as an initiator for polymerization, a source of free radicals, a hardener, and a linking agent. In Asia, due to its unstable reactive nature, DCPO has caused many thermal explosions and runaway reaction incidents in the manufacturing process. This study was conducted to elucidate its essentially thermal hazard characteristics. In order to analyze the runaway behavior of DCPO in a batch reactor, thermokinetic parameters, such as heat of decomposition (ΔH d) and exothermic onset temperature (T 0), were measured via differential scanning calorimetry (DSC). Thermal runaway phenomena were then thoroughly investigated by DSC. The thermokinetics of DCPO mixed with acids or bases were determined by DSC, and the experimental data were compared with kinetics-based curve fitting of thermal safety software (TSS). Solid thermal explosion (STE) and liquid thermal explosion (LTE) simulations of TSS were applied to determine the fundamental thermal explosion behavior in large tanks or drums. Results from curve fitting indicated that all of the acids or bases could induce exothermic reactions at even an earlier stage of the experiments. In order to diminish the extent of hazard, hazard information must be provided to the manufacturing process. Thermal hazard of DCPO mixed with nitric acid (HNO3) was more dangerous than with other acids including sulfuric acid (H2SO4), phosphoric acid (H3PO4), and hydrochloric acid (HCl). By DSC, T 0, heat of decomposition (ΔH d), and activation energy (E a) of DCPO mixed with HNO3 were calculated to be 70 °C, 911 J g−1, and 33 kJ mol−1, respectively.
Keywords:
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号