Vinyl addition polymerization of norbornene using cyclopentadienylzirconium trichloride activated by isobutyl‐modified methylaluminoxane |
| |
Authors: | Osamu Nishizawa Hideki Misaka Toyoji Kakuchi Toshifumi Satoh |
| |
Affiliation: | 1. Mitsubishi Chemical Corporation, 14‐1, Shiba 4‐Chome, Minato‐ku, Tokyo 108‐0014, Japan;2. Division of Biotechnology and Macromolecular Chemistry, Graduate School of Engineering, Hokkaido University, Sapporo 060‐8628, Japan |
| |
Abstract: | Norbornene polymerization using the commercially available and inexpensive catalyst system, cyclopentadienylzirconium trichloride (CpZrCl3) and isobutyl‐modified methylaluminoxane (MMAO), were carried out over a wide range of polymerization temperatures and monomer concentrations. For the CpZrCl3 catalyst system activated by aluminoxane with a 40 mol % methyl group and a 60 mol % isobutyl group (MMAO40/60), the polymerization temperature and monomer concentration significantly affected the molecular weight (Mn) of the obtained polymer and the catalytic activity. With an increase in the polymerization temperature from 0 to 27 °C, the catalytic activity and Mn increased, but these values dramatically decreased with the increasing polymerization temperature from 27 to 70 °C, meaning that the most suitable temperature was 27 °C. The CpZrCl3/MMAO40/60 ([Al]/[Zr] = 1000) catalyst system with the [NB] of 2.76 mol L?1 at 27 °C showed the highest activity of 145 kg molZr?1 h?1 and molecular weight of 211,000 g mol?1. The polymerization using the CpZrCl3/MMAO40/60 catalyst system proceeds through the vinyl addition mechanism to produce atactic polynorbornene, which was soluble in chloroform, toluene, and 1,2‐dichlorobenzene, but insoluble in methanol. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 1185–1191, 2008 |
| |
Keywords: | addition polymerization metallocene catalysts polyolefins norbornene polymerization vinyl‐type polynorbornene |
|
|