钛合金的六角密堆α相中微量氢所引起的内耗峰
引用本文:杜家驹.钛合金的六角密堆α相中微量氢所引起的内耗峰[J].物理学报,1982,31(6):801-806.
作者姓名:杜家驹
作者单位:中国科学院金属研究所
摘    要:在100K到350K温度范围内,测量了含氢的Ti,Ti-6Al-4V,Ti-5Al-2.5Sn和Ti-50Nb合金的内耗。发现,除了存在已知的溶于Ti合金的体心立方β相中的氢snoek峰以外,还存在一个新的由溶于其六角密堆α-相中的微量氢所引起的弛豫内耗峰。对产生此峰的机制提出了一个初步的原子模型。 关键词

收稿时间:1981-03-16

A INTERNAL FRICTION PEAK DUE TO TRACE HYDROGEN IN H.C.P. LATTICE α-PHASE OF TITANIUM ALLOYS
DU JIA-JU.A INTERNAL FRICTION PEAK DUE TO TRACE HYDROGEN IN H.C.P. LATTICE α-PHASE OF TITANIUM ALLOYS[J].Acta Physica Sinica,1982,31(6):801-806.
Authors:DU JIA-JU
Abstract:Internal friction of hydrogenated Ti, Ti-6A1-4V, Ti-5Al-2.5Sn and Ti-50Nb alloys in the range of 100 K to 350 K was measured. It was found that there was not only a known Snoek peak of hydrogen atoms in the β-phase, but also a new relaxation peak caused by the small amount of hydrogen atoms in the h.c.p. lattice α-phase. The mechanism, by which this new peak is produced, is suggested.