Abstract: | A triblock copolymer of the ABA type in which both components were crystallizable was synthesized. The A block was poly(ethylene oxide), PEO, and the B block, poly(dimethyl siloxane), PDMS. Upon cooling from the melt to liquid nitrogen temperature, the PEO block crystallized at around 40°C. When the copolymer was heated from ?170°C after quenching, glass transition, crystallization and melting of the PDMS middle block were identified in the thermogram at ?117°C, ?74°C and ?42°C, respectively. The degree of crystallinity of the PDMS block was estimated from the heat of fusion to be about 27%. The growth rates of the PEO spherulites were reduced by the presence of the middle block. |