Tensile film stress of parylene deposited on liquid
Authors:Nguyen Binh-Khiem  Matsumoto Kiyoshi  Shimoyama Isao
Institution:Department of Mechano-Informatics, Graduate School of Information Science and Technology, the University of Tokyo, 7-3-1 Hongo Bunkyo-ku, Tokyo 113-8656, Japan. khiem@leopard.t.u-tokyo.ac.jp
Abstract:We found that liquid droplets encapsulated by Parylene deposited directly on a liquid surface deformed toward spherical shapes during Parylene deposition. This deformation suggested that the film stress was tensile. We calculated the film stress of such Parylene films by studying the surface mean curvature of the droplet shape and found the film stress measured about 0.7-0.9 MPa tensile. This film stress is of opposite type to that of as-deposited Parylene films deposited on solid substrates, which was compressive. This difference might indicate a profound change of the Parylene polymer due to the use of liquid surface as deposition substrate. The tensile film stress and its effect on the droplet shape also have implications in the fabrication and operation of Parylene microdevices that have encapsulated liquid structures such as microlens or micropumps.
Keywords:
本文献已被 PubMed 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号