Isotactic sequence lengths by ozonation of poly(propylene oxide)
Authors:Charles C Price  Anthony L Tumolo
Abstract:Ozonation followed by lithium aluminum hydride reduction cleaved high molecular weight isotactic poly(propylene oxide) to crystalline polyglycols. From the melting point and molecular weight of the latter, the molar freezing point depression produced by end groups is found to be ca. 18°C./mole, as compared to that estimated for poly(ethylene glycols), Kf = 12°C./mole, from earlier data. By assuming syndiotactic placements (or other irregularities) would produce the same molar depression, the melting point of isotactic poly(propylene oxides) produced by various catalysts has been used to estimate the isotactic sequence lengths.