首页 | 本学科首页   官方微博 | 高级检索  
     


Thermal degradation of polystyrene—4. Decomposition of oxygen-containing polymers
Authors:G. Gordon Cameron  I.T. McWalter
Affiliation:Department of Chemistry, University of Aberdeen Aberdeen, Scotland;School of Chemistry, Robert Gordon''s Institute of Technology, Aberdeen, Scotland
Abstract:The thermal decomposition of two polystyrene samples prepared by radical polymerisation in the presence of oxygen was studied in the temperature range 280–300°C where volatile formation is negligible. The energy of activation for chain scission of the oxygen-containing polymers was lower than that of a reference sample prepared under vacuum. All three polymers contained the same proportion of weak bonds and it was therefore concluded that these structures are not copolymerised peroxide groups.
Keywords:
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏