首页 | 本学科首页   官方微博 | 高级检索  
     检索      


Rearrangement of the main-chain and subsequent thermal degradation of polyphenylene-ether
Authors:Shigeki Takayama  Nozomu Mathubara  Tsuyoshi Arai  Kunihiko Takeda
Institution:

a Asahi Chemical Ind. Co. Ltd., Tokyo, Japan

b Department of Materials Sciences, Shibaura Institute of Technology, Tokyo 108, Japan

Abstract:Studies of the thermal rearrangement and degradation of polyphenylene-ether (PPE) have been carried out by TGA (thermo-gravimetric analysis), GC-MS (gas chromatography-mass spectroscopy) and 1H-NMR. 2,6-Xylenol was a major scission product in the temperature range 420–700 °C, and 3,5-xylenol, as a scission product, decreased with increasing temperature. Four monomeric and eight dimeric scission products were observed at relatively high temperatures. The distribution of the scission products, which changed with increasing temperature, led to the suggestion that rearrangement of the PPE main-chain occurred to form diphenyl methylene groups, followed by thermal degradation.
Keywords:
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号