Fabrication and characterization of sputtered titanium dioxide films |
| |
Authors: | A.A. Akl H. Kamal |
| |
Affiliation: | a Faculty of Science, Physics Department, Minia University, El-Minia, Egypt b Faculty of Science, Physics Department, Ain Shams University, Abbassia, Cairo, Egypt |
| |
Abstract: | TiO2 thin films were prepared under various conditions by using a reactive RF sputtering technique. The structural, optical and electrical characteristics of the films have been investigated. All as-deposited films were amorphous. After annealing at T > 673 K, the crystallinity of the observed tetragonal anatase phase appeared improved. The optical band gap, determined by using Tauc plot, has been found to amount to 3.38 ± 0.03 and 3.21 ± 0.03 eV for the direct and indirect transition, respectively. Also the complex optical constants for the wavelength range 300-2500 nm are reported. Using the two-point probe technique, the dark resistivity has been measured as a function of the film thickness, d. The resistivity, ρ, of the samples has been found to decrease markedly with increasing thickness, but only for d < 100 nm. The behaviour of ρd versus d was found to fit properly with the Fuchs and Sondheimer relation with parameters ρo = 4.95 × 106 Ω cm and mean free path, l = 310 ± 2 nm. The log ρ versus 1/T curves show three distinct regions with values for the activation energy of 0.03 ± 0.01, 0.17 ± 0.01 and 0.50 ± 0.02 eV, respectively. |
| |
Keywords: | Titanium oxide Thin films and sputtering |
本文献已被 ScienceDirect 等数据库收录! |
|