(1) Department of Inorganic Materials, School of Resources Processing and Bioengineering, Central South University, Changsha, 410083, China
Abstract:
CdO nanoparticles of 43 nm in crystal size were successfully synthesized by the mechanochemical reaction (CdCl2 + Na2CO3) with NaCl as a diluent and subsequent thermal treatment at 700°C for 2 h. The samples were characterized by differential thermal analysis (DTA), thermogravimetric analysis (TGA), X-ray diffraction (XRD) and transmission electron microscopy (TEM). Effect of calcination temperature on the crystal size of CdO nanoparticles was primarily investigated. The apparent activation energy of CdO nanoparticle formation during thermal treatment was calculated to be 12.2 kJ/mol.