CaS∶Eu~(2+),Sm~(3+)的制备与表征
引用本文:张希艳,姜薇薇,卢利平.CaS∶Eu~(2+),Sm~(3+)的制备与表征[J].光学技术,2004,30(3):296-298.
作者姓名:张希艳  姜薇薇  卢利平
作者单位:长春理工大学,长春,130022
摘    要:采用湿法工艺在还原气氛下制备了CaS∶Eu2+,Sm3+光存储材料。研究了灼烧温度和灼烧时间对样品性能的影响。XRD图谱表明,样品在700℃—1200℃均形成CaS晶格。光谱分析表明,在紫外光(295nm)激发后,用980nm半导体激光照射样品,具有光激励发光现象,发射光谱峰值波长为649nm。

关 键 词:CaS∶Eu2+  Sm3+  制备  光激励发光
文章编号:1002-1582(2004)03-0296-03
修稿时间:2003年9月22日

Preparation of CaS∶Eu2+,Sm3+ and characterization
ZHANG Xi-yan,JIANG Wei-wei,LU Li-ping.Preparation of CaS∶Eu2+,Sm3+ and characterization[J].Optical Technique,2004,30(3):296-298.
Authors:ZHANG Xi-yan  JIANG Wei-wei  LU Li-ping
Abstract:The CaS∶Eu~(2+), Sm~(3+) powders are prepared by the wet-method in a reducing atmosphere. The influences on properties of sample from temperature and fired-time are studied. XRD analysis shows crystal structure of CaS is formed at 700℃. Spectrum analysis results show that the sample which is stimulated by 980nm laser after excitated by ultraviolet lamp (295nm ) emits red luminescence which peaking at 649nm.
Keywords:CaS∶Eu~(2+)  Sm~(3+)    preparation    photo-stimulated luminescencei