Copolymers of PBT and nylon 4T
Authors:R J Gaymans  J L De Haan  O Van Nieuwenhuize
Abstract:Polybutylene terephthalate–nylon 4T copolymers (PBT–PA 4T) are synthesized from the diamide of diaminobutane and dimethyl terephthalate (DMT) with butane diol and more DMT in a concentration range of up to 50% PA 4T. The polymerization conditions were similar to those for PBT: first, a melt polymerization, followed by solid-state post-condensation. The materials were studied by differential scanning analysis (DSC) (melting and crystallization behavior) and dynamic mechanical thermal analysis (DMTA) (glass transitions and torsion moduli). The water absorptions were determined at 100% RH. By increasing the PA 4T content in the copolymers, melting temperatures increased strongly, heats of fusion decreased slightly, and glass transition temperatures increased linearly. The torsion moduli above the glass transition temperature were higher. © 1993 John Wiley & Sons, Inc.
Keywords:PBT copolymer  polyesteramide  diaminobutane  nylon 4T copolymer
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号