首页 | 本学科首页   官方微博 | 高级检索  
     

在铜铁、铜钴复合氧化物上利用CO低温催化还原NO
作者单位:江南大学食品科学技术学院,无锡,214122;中国科学技术大学化学系,合肥,230026
摘    要:

关 键 词:CuO/Fe2O3  CuO/Co3O4  NO还原  催化活性  热稳定性

Low-temperature Catalytic Reduction of Nitrogen Monoxide with Carbon Monoxide on Copper Iron and Copper Cobalt Composite Oxides
Jun-sheng Shu,Wen-shui Xia,You-jin Zhang,Tao Cheng,Min-rui Gao. Low-temperature Catalytic Reduction of Nitrogen Monoxide with Carbon Monoxide on Copper Iron and Copper Cobalt Composite Oxides[J]. Chinese Journal of Chemical Physics, 2008, 21(4): 393-400. DOI: 10.1088/1674-0068/21/04/393-400
Authors:Jun-sheng Shu  Wen-shui Xia  You-jin Zhang  Tao Cheng  Min-rui Gao
Affiliation:{{each article.affiliations aff i}} {{if aff.addressEn && aff.addressEn != ""}} {{if aff.label && aff.label != "" && article.affiliations.length != 1}}{{@ aff.label}}.{{/if}}{{@ aff.addressEn}}{{/if}} {{/each}}
Abstract:Copper iron composite oxides (CuO/Fe2O3) and copper cobalt composite oxides (CuO/Co3O4) for the catalytic reduction of NO with CO at low temperature were prepared by co-precipitation. The catalytic activity and thermal stability of the catalysts were evaluated by a microreactor-GC system. The 100% conversion temperatures of NO are 80 oC for CuO/Fe2O3 and 90 oC for CuO/Co3O4. The catalysts possess high catalytic activity and favorable thermal stability for NO reduction with CO in a wide temperature range and long time range. A systematic study of the molar ratios of the reactants, the volume of NaOH, aging time, and calcination temperature/time was carried out to investigate the influence preparation conditions on the catalytic activity of the catalysts.
Keywords:CuO/Fe2O3   CuO/Co3O4   NO reduction   Catalytic activity   Thermal stability  
本文献已被 万方数据 等数据库收录!
点击此处可从《化学物理学报(中文版)》浏览原始摘要信息
点击此处可从《化学物理学报(中文版)》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号