摘    要:以典型蓝色发光材料-联苯乙烯衍生物(4,4’-bis(2,2’-diphenylvinyl) -1,1’-biphenyl,DPVBi)为发光层,采用MoO3为阳极缓冲层制备了结构简单的非掺杂型蓝色有机电致发光器件.在电流密度为20 mA/cm2、MoO3缓冲层厚度为0.5 nm对器件效率约为无缓冲层器件效率的18倍,...

关 键 词:有机电致发光  蓝色  阳极缓冲层  MoO3
收稿时间:2011-09-01

Highly Efficient Nondoped Blue Organic Light-emitting Diode Using MoO3 as Anode Buffer Layer
NI Wei-de,WU You-zhi,ZHANG Wen-lin,ZHANG Cai-rong,ZHANG Ding-jun.Highly Efficient Nondoped Blue Organic Light-emitting Diode Using MoO3 as Anode Buffer Layer[J].Chinese Journal of Luminescence,2011,32(12):1271-1275.
Authors:NI Wei-de  WU You-zhi  ZHANG Wen-lin  ZHANG Cai-rong  ZHANG Ding-jun
Institution:1. State Key Laboratory of Gansu Advanced Non-ferrous Metal Materials, School of Materials Science & Engineering, Lanzhou University of Technology, Lanzhou 730050, China; 2. Department of Applied Physics, Shcool of Science, Lanzhou University of Technology, Lanzhou 730050, China
Abstract:Contact properties between electrodes and organic layers play a key role for the performance of an organic device. Ohmic contacts at electrode/organic interfaces are required for an ideal device. In order to improve performance of 4,4'-bis(2,2'-diphenylvinyl)-1,1'-biphenyl (DPVBi, a typical blue organic luminescent material) based organic light-emitting diode, MoO3 was introduced at anode interface as a buffer layer and a highly efficient bright nondoped blue electroluminescent device with low driving voltage was fabricated. Luminescent efficiency of the device with a 0.5-nm-thick MoO3 buffer layer is 18 times higher than that of the device without buffer layer, and 1.2 times higher than that of the device with a conventional copper phthalocyanine (CuPc) buffer layer at a current density of 20 mA/cm2. Turn-on voltage, maximum external quantum efficiency and luminance of the device are 3.3 V, 3.1% and 16000 cd/m2, respectively. Commission Internationale de l'Eclairage (CIE) co-ordinates are (0.15, 0.15). Realization of excellent device performance is attributed to formation of ohmic contact between anode and organics by insertion of MoO3.
Keywords:luminescence  organic electroluminescence  blue  anode buffer layer  MoO3
本文献已被 CNKI 等数据库收录!
点击此处可从《发光学报》浏览原始摘要信息
点击此处可从《发光学报》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号