Abstract: | Measurements of thermal diffusivities of peroxide-cured and sulfur-cured rubbers, over the range 0–100°C and 0–75 phr of carbon, are described. They are based on the asymptotic time dependences of heating and cooling curves, recorded following quenching of the samples into baths at various temperatures. The diffusivities are shown to depend linearly on both temperature and carbon content, to reasonable accuracies over the ranges studied. Some theory bearing on measurement techniques is presented. |