Abstract: | A novel ABn-type dendrimer/linear polymer block copolymer, i.e., poly(trimethyleneimine) dendrimer-block-(polysarcosine)64 ( 1 ), was synthesized by ring-opening polymerization of sarcosine N-carboxyanhydride initiated with the 64-NH2-terminal poly(trimethyleneimine) dendrimer as a macroinitiator. 1 has narrow molecular weight distributions (Mw/Mn = 1.01–1.03, by size exclusion chromatography) and controlled polysarcosine chain lengths (by varying the monomer/dendrimer feed molar ratios). Small-angle neutron scattering (SANS) data obtained in D2O solution of 1 (DP's of polysarcosine = 2.0 and 24) fitted well with a Guinier plot of a spherical particle, and gave diameters of 44 and 100 Å, respectively. |