Production of Granulated NaP Zeolite without Binder
Authors:N E Gordina  V Yu Prokof’ev  T N Borisova  A M Elizarova
Institution:1.Ivanovo State University of Chemistry and Technology,Ivanovo,Russia
Abstract:Possibility was examined of synthesizing zeolites granulated without a binder with the use of a preliminary ultrasonic treatment of the suspension at a frequency of 22 kHz from mixtures of sodium metasilicate and aluminum and silicon oxides with various Si: Al ratios. It was found that, after the preliminary treatment, extrusion of grains, and calcination at 650°C, crystalline phases Na6Al4Si4O17, Na8Al4Si4O18, Na2Al2O4, and Na2SiO3 phases are formed in the sample with Si: Al = 1. These phases are precursors for synthesis of NaA and NaP zeolites and sodalite via hydrothermal crystallization in a NaOH solution with concentration of 2 M. Upon a similar treatment of a sample with Si: Al = 2, there are crystalline phases α- and β-Na2Si2O5, from which only NaP zeolite is formed in the course of crystallization. The hydrothermal crystallization in a 6 M alkali solution yields sodalite, irrespective of the Si: Al ratio. It was shown that an ultrasonic treatment gives a gel-like system at Si: Al = 1 and a powdered material at Si: Al = 2, which yields by the end of synthesis samples with cactus-like or wool-like morphology, respectively.
Keywords:
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号