Synthesis and surface characterization of heparin-immobilized polyetherurethanes
Authors:Inn-Kyu Kang  Dong Ki Baek  Young Moo Lee  Yong Kiel Sung
Abstract:Novel poly(ether urethanes) containing diester groups in the side chains (PU) were synthesized from 4,4′-diphenylmethyl diisocyanate, polytetramethylene glycol, and diethyl bis(hydroxymethyl)malonate as a chain extender. The surface modification of the PU film was carried out by a hydrolysis reaction, poly(ethylene oxide) (PEO) grafting, and heparin immobilization, and the surface-modified PUs were then characterized by attenuated total reflection Fourier transform infrared (ATR-FTIR) spectroscopy, electron spectroscopy for chemical analysis (ESCA), and a contact angle goniometer. The concentration of carboxylic acid groups introduced on the PU surfaces as determined by the rhodamine interaction method was 61 nmol/cm2 when treated with 4N NaOH/methanol (1 : 2 v/v) for 30 min and subsequently with a citric acid–methanolic aqueous solution. The amounts of heparin coupled to the carboxyl groups on the PU surfaces and to the terminus amino groups on the PU-PEO were 0.92 and 0.84 μ g/cm2, respectively. There was almost no heparin released from the immobilized surface of a physiological solution for 100 h, thereby indicating the strong stability of immobilized heparin. © 1998 John Wiley & Sons, Inc. J. Polym. Sci. A Polym. Chem. 36: 2331–2338, 1998
Keywords:poly(ether urethane)  surface modification  heparin immobilization
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号