首页 | 本学科首页   官方微博 | 高级检索  
     


Thermomechanical and shape memory properties of SCF/SBS/LLDPE composites
Authors:Yong-kun Wang  Wen-chao Tian  Guang-ming Zhu  Jian-qiang Xie
Affiliation:1. Key Laboratory of Ministry of Education for Electronic Equipment Structure Design, Xidian University, Xi'an 710071, China;2. Department of Applied Chemistry, Northwestern Polytehnical University, Xi'an 710129, China;3. Department of Polymer materials and Engineering, College of Material Science and Engineering, North China University of Science and Technology, Tangshan 063009, China
Abstract:A thermally triggered shape memory polymer composite was prepared by blending short carbon fiber (SCF) into a blend of poly(styrene-b-butadiene-b-styrene) triblock copolymer (SBS)/linear low density polyethylene (LLDPE) prior to curing. These composites have excellent processability compared with other thermosets. The dynamic mechanical analysis (DMA) and differential scanning calorimetry (DSC) were investigated to assess the thermomechanical properties of the SCF/SBS/LLDPE composite. Scanning electron microscope (SEM) imaging of the samples was performed to show the distribution of the SCF in the composite. The study specifically focused on the effect of SCF on the shape memory behavior of the SCF/SBS/LLDPE composite. The results indicated that the large amount of SCF significantly improved the mechanical property of the polymer composites while not damaging the shape memory performance. The SCF/SBS/LLDPE composites exhibited excellent shape memory behavior when the SCF content was less than 15.0 wt%. Moreover, the shape fixity ratio and shape recovery time of the SCF/SBS/LLDPE composites increased with the SCF content.
Keywords:Short carbon fiber  SCF/SBS/LLDPE composite  Mechanical properties  Shape memory behavior
本文献已被 CNKI 万方数据 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号