Contamination problems from glass beaker inner surface in low level 210Po analysis
Authors:J. Kameník  Z. Hölgye
Affiliation:(1) National Radiation Protection Institute, Bartoškova 28, 140 00 Prague, Czech Republic;(2) Nuclear Physics Institute, Academy of Sciences of the Czech Republic, 250 68 Řež near Prague, Czech Republic
Abstract:It was found that heating of diluted nitric or hydrochloric acids in many years stored glass beakers can result in mBq quantities of 210Po leached from beaker walls to the solution. In the case of freshly bought beakers acid leaching of 210Po was not observed. We suppose that acid leachable 210Po in old beakers is mainly due to implantation of radon progenies (from air) into superficial layers of glass beaker walls.