Synthesis and characterization of oligo-4-[(pyridin-3-ylimino)methyl]phenol |
| |
Authors: | İ. Kaya S. Çulhaoğlu D. Şenol |
| |
Affiliation: | 1.Department of Chemistry, Faculty of Sciences and Arts,?anakkale Onsekiz Mart University,?anakkale,Turkey |
| |
Abstract: | The oxidative polycondensation of 4-[(pyridin-3-ylimino)methyl]phenol (4-PIMP) with O2, H2O2, and NaOCl was studied in an aqueous alkaline medium between 50°C and 90°C. Oligo-4-[(pyridin-3-ylimino)methyl]phenol (O-4-PIMP) prepared was characterized by 1H-NMR, 13C-NMR, FT-IR, UV-VIS, size-exclusion chromatography, and elemental and thermal analyses techniques. At the optimum reaction conditions, the yield of O-4-PIMP was 18.9%, 39.4%, and 46.8% using H2O2, O2, and NaOCl oxidant, respectively. According to the TG analysis, the initial degradation temperature of O-4-PIMP was 218°C, which was by 50°C higher than that of 4-PIMP. Thermal analyses of 4-PIMP and O-4-PIMP were carried out in N2 atmosphere at 15–1000°C. The highest occupied molecular orbital, the lowest unoccupied molecular orbital, and electrochemical energy gaps of 4-PIMP and O-4-PIMP were determined from the onset potentials for n-doping and p-doping, respectively. Also, optical band gaps of 4-PIMP and O-4-PIMP were determined according to UV-VIS measurements. |
| |
Keywords: | oxygen hydrogen peroxide NaOCl oligo-4-[(pyridin-3-ylimino)methyl]phenol oxidative polycondensation thermal analysis electrical conductivity |
本文献已被 SpringerLink 等数据库收录! |
|