CO2 adsorption and dehydration behavior of LiNaX,KNaX, CaNaX and CeNaX zeolites |
| |
Authors: | Y. Erten A. Güneş-Yerkesikli A. E. Çetin F. Çakιcιoǧlu-Özkan |
| |
Affiliation: | (1) Department of Chemical Engineering, Izmir Institute of Technology, Urla, İzmir, Turkey |
| |
Abstract: | In this study, NaX synthetic zeolite was modified by following the conventional cation exchange method at 70°C. 82, 81, 79 and 48% of sodium were exchanged with Li+, K+, Ca2+ and Ce3+, respectively. Thermal analysis data obtained by TG/DSC was used to evaluate the dehydration behavior of the zeolites. The strongest interaction with water and the highest dehydration enthalpy (ΔH) value were found for Li-exchanged form and compared with the other forms. The temperature required for complete dehydration increased with decreasing cation size (cation size: K+>Ce3+>Ca2+>Na+>Li+). CO2 adsorption at 5 and 25°C was also studied and the virial model equation was used to analyze the experimental data to calculate the Henry’s law constant, K o and isosteric heat of adsorption at zero loading Q st. K o values decreased with increasing temperature and the highest Qst was obtained for K rich zeolite. It was observed that both dehydration and CO2 adsorption properties are related to cation introduced into zeolite structure. |
| |
Keywords: | cation exchange CO2 adsorption dehydration behavior NaX zeolite |
本文献已被 SpringerLink 等数据库收录! |
|