Abstract:A high-torque rheometer was used to facilitate the polycondensation of 4-5-amino-6-hydroxybenzoxazol-2-yl]benzoic acid (ABA) with trimesic acid and 1,3,5,7-tetrakis(4-carboxylatophenyl)adamantane to yield two- and three-dimensional benzobisoxazole polymers, respectively. Although the resultant polymer dopes exhibited improved homogeneity compared to polymer dopes previously prepared in glassware, improved polymer solution viscosities were not achieved. Fibers spun from the two- and three-dimensional polymers did not show a significant increase in compressive strength compared to fibers of the linear or one-dimensional benzobisoxazole polymer derived from the homopolymerization of ABA. Morphological studies of the polymer fibers and films by wide-angle X-ray scattering and scanning electron microscopy strongly indicated more lateral disorder and a more isotropic character for the three-dimensional structures compared to the one-dimensional structures. © 1997 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 35 : 3457–3466, 1997
Keywords:PBO  rigid-rod polymer  multidimensional polymer  compressive strength  fiber morphology
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号