Experimental study on the aging process of the LR 115 cellulose nitrate radon detector |
| |
Authors: | M. Siems, K. Freyer, H. -C. Treutler, G. J nsson,W. Enge |
| |
Affiliation: | a Institut für Experimentelle und Angewandte Physik, University Kiel, Olshausenstr. 40-60, D-24118 Kiel, Germany b Umweltforschungszentrum Leipzig-Halle, Permoserstr.15, D-04318 Leipzig, Germany c Lund Institute of Technology, Box 118, S-22100 Lund, Sweden |
| |
Abstract: | An experimental determination of the aging process of cellulose nitrate detector material was based on the examination of special properties of the LR 115 solid state nuclear track detectors (SSNTDs) of various ages up to 18 years. The examined relevant parameters are the bulk etching rate vb and the track etching rate vt. These parameters are responsible for the appearance, the size and the registration efficiency of tracks of -particles from radon gas in the detector. To find a correlation between these material parameters and the detector sensitivity an experimental calibration of indoor room and outdoor soil detector devices based on LR 115 took place at the Umweltforschungszentrum Leipzig-Halle (Germany). To avoid routine calibration work in external radon exposure facilities a correction of the age dependent calibration factors with the material parameters measured in one's own laboratory was targeted. In this study a general age dependence, however, was not found. The following statements for practical applications can be made. (i) the bulk etching rate vb for detectors of the same batch has a depth dependence and this dependence is constant over 2 years (LR 115 September 1994). (ii) detectors of different batches older than 5 years and stored at room temperature show an odd vb behaviour when vb is used for describing track shapes. (iii) the calibration factor of detectors of different batches that were stored at about +4°C is constant over 5 years (LR 115 September 1994 and February 1999, Table 2). The conclusion is that LR 115 detectors not older than 5 years and stored in a refrigerator at about +4°C should be preferred for radon measurements. Furthermore these detectors should be recalibrated every year and the microscope work of this calibrations should be performed by the same person who performs the measurements. In addition, a phenomenon related to fundamental track formation mechanisms was found, that the time straggling of the time tthrough when vertical tracks penetrate the 12 μm thick detector layer is independent of the age of the detectors and the energy of the -particle at the detector surface. |
| |
Keywords: | |
本文献已被 ScienceDirect 等数据库收录! |
|