摘    要:以Ti(OCH2CH2CH2CH3)4为钛源,脱脂棉花纤维为模板,利用浸渍-热转化两步法制备了具有中空结构的Sn4+掺杂TiO2光催化纤维材料(Sn4+/TiO2),利用X-射线衍射(XRD)、扫描电子显微镜(SEM)和紫外-可见光谱(UV-vis)等技术对其晶体结构、形貌、尺寸、光吸收特性等进行了表征.以亚甲基蓝(MB)溶液的脱色降解为模型反应,考察了样品Sn4+/TiO,在太阳光下的光催化性能.结果表明:利用该法制得的Sn4+/TiO2材料具有中空纤维结构;煅烧温度影响材料Sn4+/TiO2的相结构、组成、尺寸、形貌以及催化性能;Sn4+的掺入能够显著改善TiO2在太阳光条件下的催化性能,600℃煅烧2h所得的Sn4+掺杂量x=0.29%的TiO2中空纤维材料具有最佳的光催化活性,太阳光下2h即可使MB溶液的脱色降解率达97.28%;重复使用5次仍可使MB溶液的脱色降解率保持在90%以上,且该催化剂材料易于离心分离去除.

关 键 词:Sn4+/TiO2  中空纤维材料  棉花模板  两步法  光催化活性

Preparation and photocatalytic properties of Sn4+-doped TiO2 hollow fiber materials
ZHENG Tao , TIAN Ze , SUN Jia-xing , SU Bi-tao , LEI Zi-qiang. Preparation and photocatalytic properties of Sn4+-doped TiO2 hollow fiber materials[J]. Chemical Research and Application, 2012, 24(1): 79-83
Authors:ZHENG Tao    TIAN Ze    SUN Jia-xing    SU Bi-tao    LEI Zi-qiang
Affiliation:(Key Laboratory of Polymer Materials of Gansu Province,Key Laboratory of Eco-Environment-Related Polymer Materials Ministry of Education,College of Chemistry and Chemical Engineering,Northwest Normal University,Lanzhou,730070,China)
Abstract:Sn4+-doped TiO2 photocatalytic materials(Sn4+/TiO2) with hollow fiber structure were prepared by a two-steps(dipping-thermal conversion)method using tetrabutyl titanate as the source of titanium and absorbent cotton fiber as the template.X-ray diffraction(XRD),scanning electron microscopy(SEM)and ultraviolet-visible spectroscopy(UV-vis)techniques were employed to characterize the crystal structure,phase component,morphology,and optical absorption properties of the materials.Using the degradation of methylene blue(MB)as the model reaction,the photocatalytic properties of the samples were investigated under the solar light.Results showed that obtained materials(Sn4+/TiO2) have hollow fiber structure;the phase structure and component,size,morphology and photocatalytic activity of Sn4+/TiO2 were influenced by the calcining temperatures.Doping Sn4+ into TiO2 can significantly improved its photocatalytic activity under the solar light.Sn4+/TiO2 hollow fiber material of x=0.29%which obtained at 600 ℃ for 2 h has the optimum photocatalytic activity.On the material,the decolorizing efficiency of the MB solution reached 97.28%when the radiation time was 2 h and remained above 90%after being repeatedly used for 5 times.And the material was easily removed by centrifugal separation.
Keywords:Sn4+/TiO2  hollow fiber material  cotton template  two-steps method  photocatalytic activity